journal article·2009-05-27

Development and Testing of Hierarchically Wrinkled Coatings for Marine Antifouling

Kirill Efimenko, John Finlay, Maureen E. Callow, James A. Callow, Jan Genzer

Publisher page

Abstract

We report on the formation and testing of novel marine coatings comprising hierarchically wrinkled surface topographies (HWTS) having wrinkles of different length scales (generations) ranging from tens of nanometers to a fraction of a millimeter. The individual wrinkle generations are arranged in nested patterns, where each larger wrinkle resides underneath and represents a scaled-up version of the smaller wrinkle. We present and discuss results from field tests in seawater and laboratory experiments. The results of our field tests reveal that while coatings with flat topographies foul after relatively short time periods (4-15 weeks), the HWST coatings with the same chemistries as flat coatings remain relatively free of biofouling even after prolonged exposure to seawater (18 months). In contrast to flat coatings, the HWST substrates are not colonized by barnacles. These observations suggest that surface topography plays a dominant role in governing the coating defense against barnacle fouling even without fine-tuning the chemical composition of the overcoat. Laboratory experiments indicate that settlement of zoospores of the green alga Ulva and the strength of attachment of sporelings (young plants) depend on the chemical composition of the coating as well as surface topography.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Marine Biology and Environmental Chemistry · Surface Modification and Superhydrophobicity · Microplastics and Plastic Pollution

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemical & Biomolecular Engineering, North Carolina State University, Raleigh, North Carolina 27695-7905, and School of Biosciences, University of Birmingham, Birmingham B15 2TT, U.K.

References (40)

Show source-provided references
1. Genzer J. · Biofouling · 2006 · 22 · 33910.1080/08927010600980223 ↗
2. Krishnan S. · J. Mater. Chem. · 2008 · 18 · 340510.1039/b801491d ↗
3. Kavanagh C. J. · J. Adhesion · 2005 · 81 · 84310.1080/00218460500189331 ↗
4. Hills J. M. · Biofouling · 1998 · 12 · 5710.1080/08927019809378346 ↗
5. Hills J. M. · Biofouling · 1998 · 13 · 3110.1080/08927019809378369 ↗
6. Thomason J. C. · Biofouling · 2002 · 18 · 29310.1080/0892701021000034409 ↗
7. Prendergast G. S. · Biofouling · 2008 · 24 · 44910.1080/08927010802340135 ↗
8. Prendergast G. S. · : Biofouling · 2009 · 25 · 3510.1080/08927010802444267 ↗
9. Callow M. E. · Biofouling · 2002 · 18 · 23710.1080/08927010290014908 ↗
10. Feinberg, A. W., Gibson, A. L., Wilkerson, W. R., Seegert, C. A., Wilson, L. H., Zhao, L. C., Baney, R. H., Callow, J. A., Callow, M. E., Brennan, A. B., Clarson, S. J., Fitzgerald, J. J., Owen, M. F., Smith, S. D., and van Dyke, M. E.Synthesis & Properties of Silicones and Silicon-Modified Materials;American Chemical Society:Washington, DC, 2003; ACS Symposium Series838, pp196−211.10.1021/bk-2003-0838.ch018 ↗
11. Hoipkemeirer-Wilson L. · Biofouling · 2004 · 20 · 5310.1080/08927010410001662689 ↗
12. Carman M. L. · Biofouling · 2006 · 22 · 1110.1080/08927010500484854 ↗
13. Schumacher J. F. · Biofouling · 2007 · 23 · 5510.1080/08927010601136957 ↗
14. Schumacher J. F. · Biofouling · 2007 · 23 · 30710.1080/08927010701393276 ↗
15. Bers A. V. · Biofouling · 2004 · 20 · 4310.1080/08927010410001655533 ↗
16. Scardino A. J. · Biofouling · 2004 · 20 · 24910.1080/08927010400016608 ↗
17. Scardino A. J. · Biofouling · 2006 · 22 · 5510.1080/08927010500506094 ↗
18. Howell D. · Biofouling · 2006 · 22 · 40110.1080/08927010601035738 ↗
19. Chung K. K. · Biointerphases · 2007 · 2 · 8910.1116/1.2751405 ↗
20. Guenther J. · Biofouling · 2007 · 23 · 41910.1080/08927010701570071 ↗
21. Scardino A. J. · Biofouling · 2008 · 24 · 4510.1080/08927010701784391 ↗
22. Scardino A. J. · Biofouling · 2009 · 25 · 8310.1080/08927010802538480 ↗
23. Efimenko K. · J. Colloid Interface Sci. · 2002 · 254 · 30610.1006/jcis.2002.8594 ↗
24. Efimenko K. · Nat. Mater. · 2005 · 4 · 29310.1038/nmat1342 ↗
25. Chen X. · Scr. Mater. · 2004 · 50 · 79710.1016/j.scriptamat.2003.11.035 ↗
26. Mahadevan L. · Science · 2005 · 307 · 174010.1126/science.1105169 ↗
27. Callow M. E. · J. Phycol. · 1997 · 33 · 93810.1111/j.0022-3646.1997.00938.x ↗
28. Finlay J. A. · Biofouling · 2002 · 18 · 25110.1080/08927010290029010 ↗
29. Finlay J. A. · Biofouling · 2008 · 24 · 21910.1080/08927010802040693 ↗
30. Schultz M. P. · Biofouling · 2000 · 15 · 24310.1080/08927010009386315 ↗
31. Schultz M. P. · Biofouling · 2003 · 19 · 1710.1080/0892701031000089516 ↗
32. Chaudhury M. K. · Biofouling · 2005 · 21 · 4110.1080/08927010500044377 ↗
33. Cassé F. · Biofouling · 2007 · 23 · 26710.1080/08927010701288336 ↗
34. Aldred N. · Biofouling · 2008 · 24 · 35110.1080/08927010802256117 ↗
35. Swain G. W. · Biofouling · 1998 · 12 · 25710.1080/08927019809378358 ↗
36. Bhat R. R. · Adv. Mater. · 2005 · 17 · 280210.1002/adma.200500858 ↗
37. Guidipati C. S. · Langmuir · 2005 · 21 · 304410.1021/la048015o ↗
38. Krishnan S. · Langmuir · 2006 · 22 · 507510.1021/la052978l ↗
39. Arifuzzaman, S. Özçam, A. E., Efimenko, K., and Genzer, J.,Work in progress (2009) .
40. Spange S. · Macromol. Symp. · 1998 · 126 · 22310.1002/masy.19981260118 ↗