A Si−O−C Composite Anode: High Capability and Proposed Mechanism of Lithium Storage Associated with Microstructural Characteristics
Source abstract
Abstract
A blend of phenyl-substituted, branched polysilane, (Ph(2)Si)(0.85)(PhSi)(0.15), and polystyrene (1:1 in weight) has been transformed into a composite material consisting of graphene layers, Si-O-C glasses, and micropores through a pyrolytic polymer-to-ceramic conversion. Several analytical techniques have been employed to characterize the Si-O-C composite material, demonstrating the presence of the three components in its host framework. The Si-O-C composite material performs well in electrochemical operations with a characteristic voltage plateau, offering a capacity of more than 600 mA h g(-1). When polystyrene is not blended, the resulting comparative material is even less porous and shows a shorter voltage plateau in electrochemical operations. A broad resonance in the (7)Li NMR spectrum recorded at low temperature can be deconvoluted into three components in the fully lithiated state of the Si-O-C composite material derived from the polymer blend. This result indicates that the Si-O-C composite material electrochemically stores lithium species in interstitial spaces or edges of the graphene layers, directly or indirectly the Si-O-C glass phase, and the micropores. However, both the Si-O-C glass phase and micropores are minor as electrochemically active sites for lithium storage, and interstitial spaces or edges of the graphene layers act as major electrochemically active sites in this composite material. Despite the excellent cyclability of the Si-O-C composite material, the voltage plateau disappeared over cycling. This phenomenon suggests that the microstructure is delicate for repetitive lithium insertion and extraction and that newly formed sites must generate the nearly equal capacity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Chemical Synthesis and Characterization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Dow Corning Toray Company, Ltd., Chigusa-Kaigan, Ichihara 299-0108, Japan, and Department of Applied Chemistry, Graduate School of Urban Environmental Sciences, Tokyo Metropolitan University, Hachioji, Tokyo 192-0397, Japan
References (57)
Show source-provided references
1. Tarascon J.-M. · Nature · 2001 · 414 · 35910.1038/35104644 ↗
2. Xing W. · Solid State Ionics · 1997 · 93 · 23910.1016/S0167-2738(96)00512-7 ↗
3. Xing W. · J. Electrochem. Soc. · 1997 · 144 · 241010.1149/1.1837828 ↗
4. Wilson A. M. · Chem. Mater. · 1997 · 9 · 160110.1021/cm970002r ↗
5. Tamai H. · J. Mater. Sci. Lett. · 2000 · 19 · 5310.1023/A:1006703931974 ↗
6. Mukai S. R. · Kagaku Kogaku Ronbunshu · 2003 · 29 · 22110.1252/kakoronbunshu.29.221 ↗
7. Ning L. J. · J. Solid State Electrochem. · 2005 · 9 · 52010.1007/s10008-004-0616-8 ↗
8. Konno H. · Carbon · 2005 · 43 · 111110.1016/j.carbon.2004.12.005 ↗
9. Wilson A. M. · Solid State Ionics · 1997 · 100 · 25910.1016/S0167-2738(97)00409-8 ↗
10. Wilson A. M. · J. Power Sources · 1997 · 68 · 19510.1016/S0378-7753(96)02551-7 ↗
11. Wilson A. M. · Chem. Mater. · 1997 · 9 · 213910.1021/cm970224p ↗
12. Larcher D. · Solid State Ionics · 1999 · 122 · 7110.1016/S0167-2738(98)00557-8 ↗
13. Dahn J. R. · Science · 1995 · 270 · 59010.1126/science.270.5236.590 ↗
14. Babonneau F. · Chem. Mater. · 1989 · 1 · 55410.1021/cm00005a017 ↗
15. Zhang H. · J. Am. Ceram. Soc. · 1990 · 73 · 95810.1111/j.1151-2916.1990.tb05143.x ↗
16. Belot V. · J. Non-Cryst. Solids · 1992 · 144 · 28710.1016/S0022-3093(05)80412-0 ↗
17. Babonneau F. · J. Non-Cryst. Solids · 1992 · 147 · 28010.1016/S0022-3093(05)80630-1 ↗
18. Babonneau F. · Chem. Mater. · 1994 · 6 · 5110.1021/cm00037a012 ↗
19. Bois L. · Chem. Mater. · 1994 · 6 · 79610.1021/cm00042a016 ↗
20. Sorarù G. D. · J. Am. Ceram. Soc. · 1995 · 78 · 37910.1111/j.1151-2916.1995.tb08811.x ↗
21. Campostrini R. · J. Mater. Chem. · 1996 · 6 · 58510.1039/JM9960600585 ↗
22. Liu Q. · Chem. Mater. · 1997 · 9 · 243410.1021/cm970316e ↗
23. Corriu R. J. P. · J. Mater. Sci. · 1995 · 30 · 231310.1007/BF01184579 ↗
24. Wild M. J. · J. Mater. Sci. · 1998 · 33 · 544110.1023/A:1004414820662 ↗
25. Schiavon M. A. · J. Non-Cryst. Solids · 2002 · 304 · 9210.1016/S0022-3093(02)01009-8 ↗
26. Kolář F. · Mater. Chem. Phys. · 2004 · 86 · 8810.1016/j.matchemphys.2004.02.011 ↗
27. Yajima S. · Nature · 1976 · 261 · 68310.1038/261683a0 ↗
28. Carlsson D. J. · J. Am. Ceram. Soc. · 1990 · 73 · 23710.1111/j.1151-2916.1990.tb06499.x ↗
29. Schmidt W. R. · Chem. Mater. · 1991 · 3 · 257−10.1021/cm00014a011 ↗
30. White D. A. · Adv. Ceram. Mater. · 1987 · 2 · 5310.1111/j.1551-2916.1987.tb00053.x ↗
31. Burns G. T. · Chem. Mater. · 1992 · 4 · 131310.1021/cm00024a035 ↗
32. Babonneau F. · Mater. Res. Soc. Symp. Proc. · 1992 · 271 · 78910.1557/PROC-271-789 ↗
33. Singh A. K. · Mater. Res. Soc. Symp. Proc. · 1992 · 271 · 79510.1557/PROC-271-795 ↗
34. Fukui H. · Chem. Lett. · 2009 · 8610.1246/cl.2009.86 ↗
35. Matthews M. J. · Phys. Rev. B · 1999 · 59 · 658510.1103/PhysRevB.59.R6585 ↗
36. From an electrochemical aspect (potential SEI formation accompanied by irreversible lithium consumption), less open pores would be favored.
37. Rouquerol F. · 1999
38. Fukuyama K. · Carbon · 2001 · 39 · 28710.1016/S0008-6223(00)00159-7 ↗
39. Omote K. · Appl. Phys. Lett. · 2003 · 82 · 54410.1063/1.1539546 ↗
40. NANO-Solveron the websitehttp://www.rigaku.com/software/nanosolver.html.
41. Amaratunga G. A. J. · Nature · 1996 · 383 · 32110.1038/383321a0 ↗
42. Carlino E. · Phys. Rev. B · 2005 · 71 · 23530310.1103/PhysRevB.71.235303 ↗
43. Alcántara R. · Chem. Mater. · 2006 · 18 · 229310.1021/cm060060p ↗
44. Nagao M. · J. Electrochem. Soc. · 2006 · 153 · A91410.1149/1.2184908 ↗
45. Letellier M. · J. Phys. Chem. Solids · 2004 · 65 · 24510.1016/j.jpcs.2003.10.022 ↗
46. Xing W. · J. Electrochem. Soc. · 1996 · 143 · 348210.1149/1.1837241 ↗
47. Peled E. · J. Power Sources · 1998 · 76 · 15310.1016/S0378-7753(98)00148-7 ↗
48. Buiel E. · J. Electrochem. Soc. · 1998 · 145 · 225210.1149/1.1838629 ↗
49. Guérin K. · Solid State Ionics · 2000 · 127 · 18710.1016/S0167-2738(99)00290-8 ↗
50. Azuma H. · J. Power Sources · 1999 · 81 · 110.1016/S0378-7753(99)00122-6 ↗
51. Tatsumi K. · Chem. Commun. · 1997 · 68710.1039/a700221a ↗
52. Tatsumi K. · J. Power Sources · 1999 · 81 · 39710.1016/S0378-7753(99)00114-7 ↗
53. Tatsumi K. · J. Electrochem. Soc. · 1996 · 143 · 192310.1149/1.1836926 ↗
54. Dai Y. · J. Electrochem. Soc. · 1998 · 145 · 117910.1149/1.1838435 ↗
55. Key B. · J. Am. Chem. Soc. · 2009 · 131 · 923910.1021/ja8086278 ↗
56. Tatsumi K. · J. Power Sources · 1997 · 68 · 26310.1016/S0378-7753(96)02560-8 ↗
57. We need to see which application is best suited to PB. Considering the energy density of rechargeable lithium-ion batteries, this composite material may be awkward to use in consumer applications such as portable devices. Because the rate capability of PB is likely to be high, it may meet the needs of specific applications such as hybrid electric vehicles.