Stress Sensing in Polycaprolactone Films via an Embedded Photochromic Compound
Source abstract
Abstract
A photochromic polymer exhibiting mechanochromic behavior is prepared by means of ring-opening polymerization (ROP) of epsilon-caprolactone by utilizing a difunctional indolinospiropyran as an initiator. The configuration of having the photochromic initiating species within the polymer backbone leads to a mechanochromic effect with deformation of polymer films leading to ring-opening of the spiro C-O bond to form the colored merocyanine. Active stress monitoring by dynamic mechanical analysis (DMA) in tension mode was used to probe the effects of UV irradiation on polymer films held under constant strain. Irradiation with UV light induces a negative change in the polymer stress of approximately 50 kPa. Finally, a model of the mechanochromic effect was performed using density functional theory (DFT) and time-dependent DFT (TDDFT) calculations. A sharp increase in the relative molecular energy and the absorption wavelength as well as a drastic decrease in the spiro-oxygen atom charge occurred at a molecular elongation of >39%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Photochromic and Fluorescence Chemistry · Polydiacetylene-based materials and applications · Polymer composites and self-healing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Sandia National Laboratories, P.O. Box 969, Livermore, California 94551, and Sandia National Laboratories, P.O. Box 5900, Albuquerque, New Mexico 87185
References (31)
Show source-provided references
1. Behl M. · Mater. Today · 2007 · 10 · 2010.1016/S1369-7021(07)70047-0 ↗
2. Kim S. J. · Polym. Bull. · 1993 · 31 · 36710.1007/BF00692965 ↗
3. Bauer, S. and Bauer, F.InPiezoelectricity;Heywang, W., Wersing, W., and Lubitz, K., Eds.Springer Series in Materials Science;Springer:Berlin, 2008; Vol. 114, pp157−177.
4. O’Halloran A. · J. Appl. Phys. · 2008 · 104 · 071101−110.1063/1.2981642 ↗
5. Koemer H. · Mater. Today · 2008 · 11 · 3410.1016/S1369-7021(08)70147-0 ↗
6. Smets G. · Pure Appl. Chem. · 1974 · 39 · 22510.1351/pac197439010225 ↗
7. Irie M. · Adv. Polym. Sci. · 1990 · 94 · 2710.1007/BFb0043060 ↗
8. Tamai N. · Chem. Rev. · 2000 · 100 · 187510.1021/cr9800816 ↗
9. Ichimura, K.InOrganic Photochromic and Thermochromic Compounds;Crano, J. C. and Guglielmetti, R. J., Eds.Topics in Applied Chemistry;Springer:New York, 2002; Vol. 2, pp9−63.10.1007/0-306-46912-X_2 ↗
10. Minkin V. I. · Chem. Rev. · 2004 · 104 · 275110.1021/cr020088u ↗
11. Ikeda T. · Angew. Chem., Int. Ed. · 2007 · 46 · 50610.1002/anie.200602372 ↗
12. Zhou W. · Org. Lett. · 2007 · 9 · 392910.1021/ol7015862 ↗
13. Shiraishi Y. · Org. Lett. · 2009 · 11 · 348210.1021/ol901399a ↗
14. Guo X. · J. Org. Chem. · 2003 · 68 · 568110.1021/jo034243w ↗
15. Matyjaszewski K. · Angew. Chem., Int. Ed. · 2007 · 46 · 245310.1002/anie.200604278 ↗
16. Drummond C. J. · J. Chem. Soc., Faraday Trans · 1990 · 86 · 361310.1039/FT9908603613 ↗
17. Tipkin D. S. · Russ. J. Phys. Chem. · 2001 · 75 · 1720
18. Potisek S. L. · J. Am. Chem. Soc. · 2007 · 129 · 1380810.1021/ja076189x ↗
19. Davis D. A. · Nature · 2009 · 459 · 6810.1038/nature07970 ↗
20. Raymo F. M. · J. Am. Chem. Soc. · 2001 · 123 · 465110.1021/ja005699n ↗
21. Rodriguez M. A. · Acta Crystallogr., Sect. E · 2009 · 65 · 190610.1107/S1600536809027238 ↗
22. Bertelson, R. C.InOrganic Photochromic and Thermochromic Compounds;Crano, J. C. and Guglielmetti, R. J., Eds.Topics in Applied Chemistry;Springer:New York, 2002; Vol. 1, p11−83.
23. The concentration of6in solution was diluted until the absorbance value at λ580nearly matched with the absorbance of5in solution to ensure concentration-dependant variables were maintained consistently.
24. Raymo F. M. · J. Am. Chem. Soc. · 2001 · 123 · 465110.1021/ja005699n ↗
25. Evans R. A. · Nat. Mater. · 2005 · 4 · 24910.1038/nmat1326 ↗
26. Blair H. S. · Polymer · 1982 · 23 · 77910.1016/0032-3861(82)90070-2 ↗
27. Iikura H. · J. Chem. Phys. · 2001 · 115 · 354010.1063/1.1383587 ↗
28. Tawada Y. · J. Chem. Phys. · 2004 · 120 · 842510.1063/1.1688752 ↗
29. Wong B. M. · J. Chem. Phys. · 2008 · 129 · 21470310.1063/1.3025924 ↗
30. Wong B. M. · Phys. Chem. Chem. Phys. · 2009 · 11 · 449810.1039/b901743g ↗
31. Color change in PCL films was observed experimentally between 35 and 40% elongation during deformation studies. Video of the film deformation can be found in the theSupporting Information.