journal article·2026-07-16

Study on the advancement process of surface slurry argillisation layer corrosion caused by concrete sulfate attack

Zhongzhe Zhang, Jun Li, Shuai Hao, Chao Niu, Linglei Zhang, Furong Gao, Luyuan Wang, Boyan Li

Magazine of Concrete Research· Volume 78· Issue 11-12
Publisher page

Abstract

Sulfate attack significantly compromises the durability of cement-based materials, yet the quantitative evolution of eroded layers remains inadequately understood. The degradation mechanisms of cement pastes with water/cement ratios (w/c) of 0.4 and 0.6 under long-term sodium sulfate immersion were investigated in this study. A multi-scale approach – combining microhardness profiling, elemental analysis (energy-dispersive spectroscopy and X-ray fluorescence) and three-dimensional pore characterisation based on micro-computed tomography (μ-XCT) – was employed to quantify the deterioration process. The results indicated that sulfate attack initiates with a prolonged incubation period, followed by non-uniform, layer-by-layer degradation. The eroded region can be spatially categorised into wetting, yellowing and argillised zones, leading to progressive surface disintegration. Notably, the w/c = 0.6 specimens exhibited a sharp increase in penetration depth from negligible levels at 10 months to 3.9 mm at 30 months, whereas the penetration depths of the w/c = 0.4 specimens remained below 1.0 mm. Microhardness analysis revealed mechanical stratification, with surface zones retaining only 50% of the core hardness. μ-XCT data suggest that sulfate ingress is primarily governed by surface-open pores rather than isolated internal voids. The transition of the paste into an argillised state exposes new substrate surfaces, creating a feedback loop that accelerates inward chemical penetration and structural decay.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Microbial Applications in Construction Materials · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Inner Mongolia University Institute of Transportation, , Hohhot, ; Key Laboratory of Green Resource Utilization of Civil Engineering Waste, Universities of Inner Mongolia Autonomous Region, Hohhot, China

Kaifeng University School of Civil Engineering and Architecture, , Kaifeng,

Inner Mongolia University of Technology School of Civil Engineering, , Hohhot,

The Third Construction Co Ltd of China Construction Eighth Engineering Division , Xuzhou,

Jiangsu Collaborative Innovation Center for Building Energy Saving and Construct Technolog Jiangsu Vocational Institute of Architectural Technology, y, Xuzhou,

Xuzhou College of Industrial Technology School of Architecture Engineering, , Xuzhou,

Inner Mongolia University Institute of Transportation, , Hohhot,

Funding

Natural Science Foundation of Inner Mongolia Autonomous Region · Natural Science Foundation of Jiangsu Province · Research Initiation Program for Young Academic Talents of Inner Mongolia University · Basic Scientific Research Expenses Program of Universities Directly Under Inner Mongolia Autonomous Region · Research Starting Grants Project of Inner Mongolia University of Technology · Jiangsu Collaborative Innovation Center for Building Energy Saving and Construct Technology Industrial Fund Program

References (27)

Show source-provided references
1. The effects of nano- and micro-particle additives on the durability and mechanical properties of mortars exposed to internal and external sulfate attacks10.1016/j.rinp.2017.02.009 ↗
2. Internal sulfate attack in mortars containing contaminated fine recycled concrete aggregates10.1016/j.conbuildmat.2020.121851 ↗
3. Pore structure evolution and sulfate attack of high-volume slag blended mortars under standard curing and steam curing10.1016/j.conbuildmat.2022.129878 ↗
4. Long-term erosion resistance of grouting curtain in coastal karst fracture area10.1016/j.jobe.2024.108721 ↗
5. Ultrasonic and impact spectroscopy monitoring on internal sulphate attack of cement-based materials10.1016/j.matdes.2017.03.068 ↗
6. Impact of sulfate attack on flexural behaviour of CFRP strengthened concrete beams10.1680/jmacr.23.00019 ↗
7. Durability of coral aggregate concrete under coupling action of sulfate, chloride and drying-wetting cycles10.1016/j.cscm.2022.e01003 ↗
8. The role of porosity in external sulphate attack10.1016/j.cemconcomp.2018.12.016 ↗
9. Effect of physical and chemical sulfate attack on performance degradation of concrete under different conditions10.1016/j.cplett.2020.137254 ↗
10. Effect of multi-walled carbon nanotube on reactive powder concrete (RPC) performance in sulfate dry-wet cycling environment10.1016/j.conbuildmat.2022.128075 ↗
11. In-situ assessment of the water-penetration resistance of polymer modified cement mortars by μ-XCT, SEM and EDS10.1016/j.cemconcomp.2020.103821 ↗
12. Deterioration assessment model for splash zone of marine concrete structures10.1016/j.cscm.2022.e01731 ↗
13. Evaluation of molybdenum tailings as replacement for fine aggregate in concrete: Mechanical, corrosion resistance, and pore microstructural characteristics10.1016/j.conbuildmat.2022.127982 ↗
14. Studies on the performance of alkali-activated aluminosilicate geopolymer mortar against exposure to acid, sulfate, and elevated temperature
15. Effect of external sulfate attack on the tensile properties of fiber-reinforced sprayed concrete10.1680/jmacr.23.00251 ↗
16. Behavior of self-compacting concrete made with marble and tile wastes exposed to external sulfate attack10.1016/j.conbuildmat.2016.12.193 ↗
17. Does gypsum formation during sulfate attack on concrete lead to expansion10.1016/S0008-8846(99)00211-2 ↗
18. Influential role of alkaline earth activators on durability and deterioration of GGBS binder in saline environments10.1680/jmacr.24.00395 ↗
19. A study of variables that affect the process of sulfate attack of cement-based materials subjected to stray current10.1002/suco.202100071 ↗
20. Experimental study on performance of cast-in-situ recycled aggregate concrete under different sulfate attack exposures10.1016/j.conbuildmat.2020.119144 ↗
21. Nondestructive monitoring the deterioration process of cement paste exposed to sodium sulfate solution by X-ray computed tomography10.1016/j.conbuildmat.2018.07.145 ↗
22. Damage evolution of cement mortar with high volume slag exposed to sulfate attack10.1016/j.conbuildmat.2020.118626 ↗
23. An integrated macro-microscopic model for concrete deterioration under external sulfate attack10.1016/j.engfracmech.2020.107345 ↗
24. Study on the deterioration mechanism of alkali dissolution of concrete mixed with Na2SO4 in external water sources10.1016/j.conbuildmat.2022.129283 ↗
25. Deterioration of fire resistance of ultra-high-performance polypropylene-fibre-reinforced concrete (UHPPFRC) under long-term acid rain corrosion action10.1016/j.jobe.2024.111064 ↗
26. The deterioration mechanisms of hardened cement paste exposed to combined action of cyclic wetting–drying, salt attack and carbonation10.1016/j.conbuildmat.2022.130148 ↗
27. Experimental and numerical study of the effects of solution concentration and temperature on concrete under external sulfate attack10.1016/j.cemconres.2020.106284 ↗