journal article·2008-12-30Open access

Corrosion rate of steel embedded in blended Portland and fluid catalytic cracking catalyst residue (FC3R) cement mortars

E. Zornoza, P. Garcés, J. Payá

Materiales de Construcción· Volume 58· Issue 292

Abstract

This paper reports on a study of the corrosion levels in steel bars embedded in mortars made with a blend of Portland cement and (0-20%) spent fluid catalytic cracking catalyst residue (FC3R), with a variable (0.3-0.7) water/binder (w/b) ratio. The specimens were stored in the following conditions: relative humidity of 40, 80 or 100% and CO2 concentrations of 5 and 100%. The steel corrosion rate was measured with polarization resistance techniques. In the absence of aggressive agents, the steel was found to remain duly passivated in mortars with an FC3R content of up to 15% under all the conditions of relative humidity tested. The reinforcement corrosion level in mortars with a w/b ratio of 0.3 and 15% FC3R subjected to accelerated carbonation was similar to the level observed in the unblended Portland cement control mortar.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete Corrosion and Durability · Concrete and Cement Materials Research · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Influence of cement type and temperature on the rate of corrosion of steel in concrete exposed to carbonation10.5006/1.3278306 ↗
2. Pathak. “Corrosion behavior of reinforcement in slag concrete
3. 10.1007/BF0248616210.1007/BF02486162 ↗
4. A study of carbonation-induced corrosion10.1680/macr.1994.46.166.23 ↗
5. 10.1016/j.cemconcomp.2004.02.04110.1016/j.cemconcomp.2004.02.041 ↗
6. 10.1016/j.cemconres.2003.12.02910.1016/j.cemconres.2003.12.029 ↗
7. 10.1016/S0958-9465(01)00025-710.1016/S0958-9465(01)00025-7 ↗
8. 10.1016/S0008-8846(02)01026-810.1016/S0008-8846(02)01026-8 ↗
9. 10.1016/S0008-8846(03)00014-010.1016/S0008-8846(03)00014-0 ↗
10. 10.1016/S0008-8846(99)00164-710.1016/S0008-8846(99)00164-7 ↗
11. 10.1002/jctb.58310.1002/jctb.583 ↗
12. 10.1016/S0008-8846(00)00401-410.1016/S0008-8846(00)00401-4 ↗
13. Effect of sewage sludge ash (SSA) on the mechanical performance and corrosion levels of reinforced Portland cement mortars
14. Modifications induced by adding natural zeolitic pozzolans to cement paste10.3989/mc.2005.v55.i280.204 ↗
15. 10.1016/S0958-9465(03)00048-910.1016/S0958-9465(03)00048-9 ↗
16. 10.1016/S0008-8846(02)01006-210.1016/S0008-8846(02)01006-2 ↗
17. Subproducto del fraccionamiento catalítico del petróleo: características, actividad puzolánica y su efecto en las propiedades del mortero
18. 10.1016/S0008-8846(01)00693-710.1016/S0008-8846(01)00693-7 ↗
19. 10.1016/S0008-8846(02)00873-610.1016/S0008-8846(02)00873-6 ↗
20. 10.1016/S0008-8846(01)00646-910.1016/S0008-8846(01)00646-9 ↗
21. 10.1149/1.242849610.1149/1.2428496 ↗
22. Behaviour of corroded steel in a Ca(OH)(2)-saturated solution and in cement mortar. Possibility of rehabilitation
23. 10.1002/maco.1978029080410.1002/maco.19780290804 ↗
24. Effect of steel surface conditions on reinforcing steel corrosion in concrete exposed to marine environments
25. 10.1002/pse.21410.1002/pse.214 ↗
26. 10.1016/S0010-938X(99)00134-110.1016/S0010-938X(99)00134-1 ↗
27. 10.1016/S0958-9465(02)00120-810.1016/S0958-9465(02)00120-8 ↗
28. 10.1016/j.cemconcomp.2006.10.00510.1016/j.cemconcomp.2006.10.005 ↗
29. 10.1016/j.cemconcomp.2004.05.00610.1016/j.cemconcomp.2004.05.006 ↗
30. 10.1016/j.cemconres.2004.11.01010.1016/j.cemconres.2004.11.010 ↗
31. Obtaining effective half-cell potential measurements in reinforced concrete structures
32. 10.1680/adcr.2007.19.3.11710.1680/adcr.2007.19.3.117 ↗
33. Pore structure and carbonation in blended lime-cement pastes
34. Carbonation process in lime pastes with different water/binder ratio