journal article·2022-03-10Open access

Additive Manufacturing of AlSi10Mg and Ti6Al4V Lightweight Alloys via Laser Powder Bed Fusion: A Review of Heat Treatments Effects

Emanuele Ghio, Emanuela Cerri

Materials· Volume 15· Issue 6

Abstract

Laser powder bed fusion (L-PBF) is an additive manufacturing technology that is gaining increasing interest in aerospace, automotive and biomedical applications due to the possibility of processing lightweight alloys such as AlSi10Mg and Ti6Al4V. Both these alloys have microstructures and mechanical properties that are strictly related to the type of heat treatment applied after the L-PBF process. The present review aimed to summarize the state of the art in terms of the microstructural morphology and consequent mechanical performance of these materials after different heat treatments. While optimization of the post-process heat treatment is key to obtaining excellent mechanical properties, the first requirement is to manufacture high quality and fully dense samples. Therefore, effects induced by the L-PBF process parameters and build platform temperatures were also summarized. In addition, effects induced by stress relief, annealing, solution, artificial and direct aging, hot isostatic pressing, and mixed heat treatments were reviewed for AlSi10Mg and Ti6AlV samples, highlighting variations in microstructure and corrosion resistance and consequent fracture mechanisms.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Engineering and Architecture, University of Parma, 43124 Parma, Italy

References (100+)

Show source-provided references
1. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
2. Williams, J.C., and Boyer, R.B. (2020). Opportunities and issues in the application of titanium alloys for aerospace components. Metals, 10.10.3390/met10060705 ↗
3. Mechanical behavior of Ti6Al4V produced by laser bed fusion with engineered open porosity for dental applications10.1016/j.jmbbm.2021.104974 ↗
4. Analysis of greenhouse gas emissions related to aluminium transport applications10.1007/s11367-008-0058-0 ↗
5. High-temperature application of titanium alloys in gas turbine. Material life cycle opportunities and threats—An industrial perspective10.1080/09603409.2016.1184423 ↗
6. EOS GmBH—Electro Optical Systems (2021, December 06). Material Data Sheet: EOS Aluminium AlSi10Mg. München. Available online: www.eos.info.
7. On the precipitation hardening of selective laser melted AlSi10Mg10.1007/s11661-015-2980-7 ↗
8. Aluminium alloys for structural die casting
9. Ghio, E., and Cerri, E. (2021). Work hardening in heat-treated AlSi10Mg alloy manufactured by selective laser melting: Effect of Layer Thickness and Hatch Spacing. Materials, 14.10.3390/ma14174901 ↗
10. Mechanical properties of ALSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
11. Microstructural and small-scale characterization of additive manufactured AlSi10Mg alloy10.1007/s42452-019-0270-5 ↗
12. Phase-diagram: The Beginning of Wisdom10.1007/s11669-014-0343-5 ↗
13. Effect of heat treatment on the microstructure and anisotropy in mechanical properties of A357 alloy produced by selective laser melting10.1016/j.matdes.2018.05.026 ↗
14. Effect of the distance from BP and post-heat treatment of AlSi10Mg manufactured by single- and multi-laser selective laser melting10.1007/s11665-021-05577-8 ↗
15. Hypoeutectic Al-Si-Mg foundry alloys10.1007/s11661-999-0301-8 ↗
16. Effect of Si content on microstructure and mechanical properties of Al-Si-Mg alloys10.1016/j.matdes.2013.07.067 ↗
17. Donachie, M.J. (2000). Titanium: A Technical Guide, ASM International. [2nd ed.].10.31399/asm.tb.ttg2.9781627082693 ↗
18. Ducato, A., Fratini, L., La Cascia, M., and Mazzola, G. (2013, January 27–29). An automated visual inspection system for the classification of the phasaes of Ti6Al4V titanium alloy. Proceedings of the Computers Analysis of Images and Patterns, York, UK.10.1007/978-3-642-40246-3_45 ↗
19. Corrosion resistance of selective laser melted Ti-6Al-4V alloy in salt for environment
20. Microstructure and mechanical properties of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
21. Safety and efficacy of additive and subtractive surface modification of Ti6Al4V endossesous implant in goat bone10.1016/j.jmbbm.2015.11.019 ↗
22. The application of direct metal laser sintering (DMLS) of titanium alloy powder in fabricating components of aircraft structures10.4028/www.scientific.net/KEM.687.199 ↗
23. Review on direct metal laser deposition manufacturing technology for Ti6Al4V alloy10.1007/s00170-019-04851-3 ↗
24. Hot deformation and microstructural damage mechanisms in extra-low interstitial (ELI) grade Ti-6Al-4V10.1016/S0921-5093(99)00173-2 ↗
25. Study of alpha-beta transformation in Ti-6Al-4V ELI, Mechanical and Microstructural characteristics
26. A study of diffusion bonding of superplastic Ti-6Al-4V ELI grade10.1016/j.jmatprotec.2006.11.215 ↗
27. Chang, J.Z.-C., Tsai, P.-I., Kuo, M.Y.-P., Sun, J.-S., Chen, S.-Y., and Shen, H.-H. (2019). Augmentation of DMLS biomimetic dental implants with weight bearing strut to balance of biological and mechanical demands: From Bench to Animal. Materials, 12.10.3390/ma12010164 ↗
28. Effect of temperature and cooling rates of α + β morphology of Ti-6Al-4V alloy10.1016/j.prostr.2019.07.056 ↗
29. Zhong, C., Liu, J., Zhao, T., Schopphoven, T., Fu, J., Gasser, A., and Schleifenbaum, J.H. (2019). Laser metal deposition of Ti-6Al-4V—A brief review. Appl. Sci., 10.10.3390/app10030764 ↗
30. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
31. Influence of cooling rate and aging on the lamellar microstrucutre and fractography of TC21 titanium alloy10.1007/s13632-012-0055-3 ↗
32. Heat treatment of Ti6Al4V produced by selective laser melting: MicroStrucutre and Mechanical Properties10.1016/j.jallcom.2012.07.022 ↗
33. Energy and emissions saving potential of additive manufacturing: The Case of Lightweight Aircraft Components
34. 3D metal printing technology: The Need to Re-invent Design Practice10.1007/s00146-018-0809-9 ↗
35. (2000). Standard Terminology for Additive Manufacturing–General Principles–Terminology (Standard No. ASTM 52900:2015(E)).
36. Additive manufacturing a powerful tool for the aerospace industry10.1108/RPJ-01-2021-0009 ↗
37. Giganto, S., Martínez-Pellitero, S., Cuesta, E., Zapico, P., and Barreiro, J. (2022). Proposal of design rules for improving the accuracy of selective laser melting (SLM) manufacturing using benchmarks parts. Rapid Prototyp. J.10.1108/RPJ-06-2021-0130 ↗
38. Zhou, Y., Abbara, M.E., Fiang, D., Azizi, A., Poliks, M.D., and Ning, F. (2022). High-cycle fatigue properties of curved-surface AlS10Mg parts fabricated by powder bed fusion additive manufacturing. Rapid Prototyp. J.10.1108/RPJ-09-2021-0253 ↗
39. Comparison of powder bed fusion and direct energy deposition for tailoring mechanical properties of traditionally brittle alloys10.1016/j.mfglet.2021.02.003 ↗
40. Teixeira, Ó., Silva, F.J.G., Ferreira, L.P., and Atzeni, E. (2020). A review of heat treatments on Improving the quality and residual stresses of the Ti-6Al-4V parts produced by Additive Manufacturing. Materials, 10.10.3390/met10081006 ↗
41. The additive manufacturing (AM) of titanium alloys10.1016/j.mprp.2016.12.062 ↗
42. Arias-Gonzáles, F., Rodríguez-Contreras, A., Punset, M., Manero, J.M., Barro, Ó., Fernández-Arias, M., Lusquiños, F., Javier Gil, F., and Pou, J. (2021). In-Situ laser direct energy deposition of biomedical Ti-Nb and Ti-Zr-Nb alloys from elemental powders. Materials, 11.10.3390/met11081205 ↗
43. Lasers in additive manufacturing: A Review10.1007/s40684-017-0037-7 ↗
44. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
45. Additive manufacturing of metals using powder-based technology
46. Yang, L., Hsu, K., Baughman, B., Godfrey, D., Medina, F., Menon, M., and Wiener, S. (2017). Additive Manufacturing of Metals: The Technology, Materials, Design and Production, Springer International Publishing.10.1007/978-3-319-55128-9 ↗
47. Statistical analysis of experimental parameters in selective laser sintering10.1002/adem.200500030 ↗
48. Prediction of a lack-of-fusion porosity for powder bed fusion
49. Letenneur, M., Kreitcberg, A., and Brailovski, V. (2019). Optimization of laser powder bed fusion processing using a combination of melt pool modeling and design of experiment approaches: Density Control. Manuf. Mater. Process., 3.10.3390/jmmp3010021 ↗
50. Bai, S., Perevoshchikova, N., Sha, Y., and Wu, X. (2019). The effects of selective laser melting process parameters on relative density of the AlSi10Mg parts suitable procedures of the archimedes method. Appl. Sci., 9.10.3390/app9030583 ↗
51. Reducing porosity in AlSi10Mg parts processed by selective laser melting
52. Investigation of T4 and T6 heat treatment influences on relative density and porosity of AlSi10Mg alloy components manufactured by SLM10.1016/j.cie.2019.106194 ↗
53. Study of heat treatment parameters for additively manufactured AlSi10Mg in comparison with corresponding cast alloy10.1016/j.msea.2018.10.026 ↗
54. Laser powder bed fusion of AlSi10Mg: Influence of Energy Intensities on Spatter and Porosity Evolution, Microstructure and Mechanical Properties10.1016/j.jallcom.2020.156300 ↗
55. Influence of storage conditions and reconditioning of AlSi10Mg powder on the quality of parts produced by laser powder bed fusion (LPBF)
56. Classifying shape on internal pores within AlSi10Mg alloy manufactured by laser powder bed fusion using 3d X-Ray microcomputed tomography: Influence of process parameters and heat treatment10.1016/j.matchar.2020.110225 ↗
57. High cycle fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
58. Fatigue performance evaluation of selective laser melted Ti-6Al-4V10.1016/j.msea.2014.01.041 ↗
59. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
60. On the role of different annealing heat treatments on mechanical properties and microstructure of selective laser melted and conventional wrought Ti-6Al-4V10.1108/RPJ-02-2016-0022 ↗
61. The effect of manufacturing defects of the fatigue life of selective laser melted Ti-6Al-4V structures10.1016/j.matdes.2020.108708 ↗
62. As-fabricated surface morphologies of Ti-6Al-4V samples fabricated by different laser processing parameters in selective laser melting
63. Study of residual stress in selective laser melting of Ti6Al4V10.1016/j.matdes.2020.108846 ↗
64. Effect of heat treatment on the microstructure and mechanical properties of Ti6Al4V gradient structures manufactured by selective laser melting10.1016/j.msea.2018.08.084 ↗
65. Mechanical and in vitro study of anisotropic Ti6Al4V lattice structure fabricated using selective lase melting10.1016/j.jallcom.2018.12.220 ↗
66. Rationally designed functionally graded porous Ti6Al4V scaffolds with high strength and toughness built via selective laser melting for load-bearing orthopedic applications10.1016/j.jmbbm.2020.103673 ↗
67. Selective laser melting of Ti6Al4V sub-millimetric cellular structures: Prediction of Dimensional Deviations and Mechanical Performance10.1016/j.jmbbm.2020.104123 ↗
68. A review of selective laser sintering/melting (SLS/SLM) of aluminium powders: Processing, Microstructures and Properties10.1016/j.pmatsci.2015.03.002 ↗
69. Metel, A.S., Stebulyanin, M.M., Fedorov, V.S., and Okunkova, A.A. (2019). Powder density distribution for laser additive manufacturing (SLM): Potential, Fundamentals and Advanced Applications. Technologies, 7.10.3390/technologies7010005 ↗
70. Prediction of lack of fusion porosity in selective laser melting based on MP monitoring data
71. High fatigue performance of AlSi10mG alloy produced by selective laser melting10.1016/j.mechmat.2020.103499 ↗
72. Thermomechanical response of 3D laser-deposited Ti6Al4V ally over a wide range of strain rates and temperatures10.1016/j.msea.2015.08.043 ↗
73. Keyhole-induced porosities in laser-powder bed fusion (L-PBF) of Ti6Al4V: High-Fidelity Modeling and Experimental Validation
74. Mebolt, M., and Khahn, C.A. (2020). Influence of the inert gas flow on the laser powder bed fusion (LPBF) process. Industrializing Additive Manufacturing, Springer.
75. Formation and reduction of hydrogen during selective laser melting of AlS10Mg10.1016/j.jmatprotec.2015.02.013 ↗
76. Development of an empirical process model for adjusted porosity in laser-based powder bed fusion Ti-6Al-4V10.1007/s00170-021-07847-0 ↗
77. Residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
78. Influence of processing parameters on laser penetration depth and melting/re-melting densification during selective laser melting of aluminum alloy10.1007/s00339-016-0428-6 ↗
79. Influence od re-melting on surface roughness and porosity of AlSi10Mg parts fabricated by selective laser melting10.1016/j.jallcom.2019.04.017 ↗
80. Effect of build orientation on the quasi-static and dynamic response of SLM AlSi10Mg10.1016/j.msea.2020.139445 ↗
81. Additively manufactured Ti-6Al-4V thin structures via laser powder bed fusion: Effect of Building Orientation on Geometrical Accuracy and Mechanical Properties10.1016/j.jmbbm.2021.104495 ↗
82. Processing window and evaporation phenomena for Ti-6Al-4V produced by selective electron beam melting10.1016/j.actamat.2014.05.037 ↗
83. Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing10.1016/j.jmatprotec.2014.06.005 ↗
84. Dynamics of pore formation during laser powder bed fusion additive manufacturing10.1038/s41467-019-10009-2 ↗
85. Pores and the formation mechanisms of SLMed AlSi10Mg10.1108/RPJ-02-2020-0036 ↗
86. A new approach to the design and optimization of support structures in additive manufacturing10.1007/s00170-012-4403-x ↗
87. Influence on microstructure, strength and ductility of BP temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
88. Processing parameters in laser powder bed fusion metal additive manufacturing10.1016/j.matdes.2020.108762 ↗
89. Direct selective laser sintering of metals10.1108/13552549510078113 ↗
90. Brandt, M., and Deans, M. (2017). Powder bed fusion processes: An Overview. Additive Manufacturing: Materials, Design, Technologies and Applications, Woodhead Publishing.
91. Balling behavior of stainless steel and nickel powder during selective laser melting process
92. Single track formation in selective laser melting of metal powders10.1016/j.jmatprotec.2010.05.010 ↗
93. A novel titanium alloy manufactured by selective laser melting microstructure, high temperature oxidation10.1016/j.matdes.2015.10.092 ↗
94. Defect formation mechanisms in selective laser melting: A review10.1007/s10033-017-0121-5 ↗
95. Gouveia, R.M., Silva, F.J.G., Atzeni, E., Sormaz, D., Alves, J.L., and Pereira, A.B. (2020). Effect of scan strategies and use of support structures on surface quality and hardness of L-PBF AlSi10Mg parts. Materials, 13.10.3390/ma13102248 ↗
96. Zafer, Y.E., Goel, S., Ganvir, A., Jansson, A., and Joshi, S. (2020). Encapsulation of Electron Beam Melting produced alloy 718 to reduce surface connected defects by Hot Isostatic Pressing. Materials, 13.10.3390/ma13051226 ↗
97. Dass, A., and Moridi, A. (2019). State of the art in direct energy deposition: From Additive Manufacturing to Materials Design. Coatings, 9.10.3390/coatings9070418 ↗
98. Reducing lack of fusion during selective laser melting of CoCrMo alloy. Effect of laser power on geometrical features of tracks10.1016/j.matdes.2016.09.086 ↗
99. Computational assessment of thermokinetics and associated microstructural evolution in laser powder bed fusion manufacturing of Ti-6Al-4V alloy10.1038/s41598-020-63281-4 ↗
100. Heat and fluid flow in additive manufacturing—Part II: Powder Bed Fusion of Stainless Steel, and Titanium, Nickel and Aluminium Base Alloys10.1016/j.commatsci.2018.04.027 ↗