Abstract
In this study, the effects of titanium dioxide (TiO2) nanoparticles on the sulfate attack resistance of ordinary Portland cement (OPC) and slag-blended mortars were investigated. OPC and slag-blended mortars (OPC:Slag = 50:50) were made with water to binder ratio of 0.4 and a binder to sand ratio of 1:3. TiO2 was added as an admixture as 0%, 3%, 6%, 9% and 12% of the binder weight. Mortar specimens were exposed to an accelerated sulfate attack environment. Expansion, changes in mass and surface microhardness were measured. Scanning Electron Microscopy (SEM), Energy Dispersive Spectroscopy (EDS), X-ray Diffraction (XRD), Thermogravimetry Analysis (TGA) and Differential Scanning Calorimetry (DSC) tests were conducted. The formation of ettringite and gypsum crystals after the sulfate attack were detected. Both these products had caused crystallization pressure in the microstructure of mortars and deteriorated the mortars. Our results show that the addition of nano-TiO2 accelerated expansion, variation in mass, loss of surface microhardness and widened cracks in OPC and slag-blended mortars. Nano-TiO2 containing slag-blended mortars were more resistant to sulfate attack than nano-TiO2 containing OPC mortars. Because nano-TiO2 reduced the size of coarse pores, so it increased crystallization pressure due to the formation of ettringite and gypsum thus led to more damage under sulfate attack.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Civil and Environmental Engineering, Hanyang University, 222, Wangsimni-ro, Seongdong-gu, Seoul 04763, Korea
References (45)
Show source-provided references
1. Photocatalytic construction and building materials: From fundamentals to applications10.1016/j.buildenv.2009.01.002 ↗
2. Photocatalytic cement-based materials: Comparison of nitrogen oxides and toluene removal potentials and evaluation of self-cleaning performance10.1016/j.buildenv.2011.03.004 ↗
3. Strini, A., Roviello, G., Ricciotti, L., Ferone, C., Messina, F., Schiavi, L., Corsaro, D., and Cioffi, R. (2016). TiO2-based photocatalytic geopolymers for nitric oxide degradation. Materials, 9.10.3390/ma9070513 ↗
4. Ohama, Y., and Van Gemert, D. (2011). Application of Titanium Dioxide Photocatalysis to Construction Materials: State-of-the-Art Report of the Rilem Technical Committee 194-TDP, Springer Science & Business Media.10.1007/978-94-007-1297-3 ↗
5. Experimental study of photocatalytic concrete products for air purification10.1016/j.buildenv.2009.04.010 ↗
6. Siddique, R., and Khan, M.I. (2011). Supplementary Cementing Materials, Springer Science & Business Media.10.1007/978-3-642-17866-5 ↗
7. Virgalitte, S.J., Luther, M.D., Rose, J.H., Mather, B., Bell, L.W., Ehmke, B.A., Klieger, P., Roy, D.M., Call, B.M., and Hooton, R.D. (1995). Ground Granulated Blast-Furnace Slag as a Cementitious Constituent in Concrete, American Concrete Institute. ACI Report 233R-95.
8. Bastos, G., Patiño-Barbeito, F., Patiño-Cambeiro, F., and Armesto, J. (2016). Nano-inclusions applied in cement-matrix composites: A review. Materials, 9.10.3390/ma9121015 ↗
9. Mechanism of expansion of mortars immersed in sodium sulfate solutions10.1016/j.cemconres.2012.10.001 ↗
10. Investigation of the influence of blast-furnace slag on the resistance of concrete against organic acid or sulphate attack by means of accelerated degradation tests10.1016/j.cemconres.2011.09.009 ↗
11. Sulfate attack research—Whither now?10.1016/S0008-8846(01)00510-5 ↗
12. The confused world of sulfate attack on concrete10.1016/j.cemconres.2004.04.004 ↗
13. Marchand, J., Odler, I., and Skalny, J.P. (2003). Sulfate Attack on Concrete, CRC Press.
14. Hydration and properties of nano-TiO2 blended cement composites10.1016/j.cemconcomp.2012.02.009 ↗
15. Incorporation of titanium dioxide nanoparticles in mortars—Influence of microstructure in the hardened state properties and photocatalytic activity10.1016/j.cemconres.2012.09.007 ↗
16. Effect of nano-TiO2 on the mechanical properties of cement mortar10.1016/j.conbuildmat.2011.10.047 ↗
17. Lee, B.Y. (2012). Effect of Titanium Dioxide Nanoparticles on Early Age and Long Term Properties of Cementitious Materials, Georgia Institute of Technology.
18. Photocatalytic NOX abatement by calcium aluminate cements modified with TiO2: Improved NO2 conversion10.1016/j.cemconres.2015.01.011 ↗
19. (2018). Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution American, American Society for Testing and Materials. ASTM C1012/C1012M-18a.
20. Van Tittelboom, K., De Belie, N., and Hooton, R.D. (2013). Test methods for resistance of concrete to sulfate attack—A critical review. Performance of Cement-Based Materials in Aggressive Aqueous Environments, Springer.10.1007/978-94-007-5413-3_10 ↗
21. Developing a more rapid test to assess sulfate resistance of hydraulic cements10.6028/jres.110.080 ↗
22. Ferraris, C.F., Clifton, J.R., Stutzman, P.E., and Garboczi, E. (1997). Mechanisms of Chemical Degradation of Cement-Based Systems, CRC Press.
23. (2016). Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50-mm] Cube Specimens), American Society for Testing and Materials. ASTM C109/C109M-16a.
24. (2002). Standard Test Method for Flexural Strength and Modulus of Hydraulic Cement Mortars, American Society for Testing and Materials. ASTM, C348-02.
25. (2013). Standard Test Method for Density, Absorption and Voids in Hardened Concrete, American Society for Testing and Materials. ASTM, C642-13.
26. Microhardness testing of cementitious materials10.1016/S1065-7355(96)90051-6 ↗
27. Sarkar, S.L., Aimin, X., and Jana, D. (2001). Scanning electron microscopy, X-ray microanalysis of concretes-7. Handbook of Adhesives Raw Materials, Noyes Publications.10.1016/B978-081551437-4.50010-2 ↗
28. Lothenbach, B., Durdzinski, P., and De Weerdt, K. (2016). Thermogravimetric analysis. A Practical Guide to Microstructural Analysis of Cementitious Materials, CRC Press.
29. The effect of TiO2 nanoparticles on water permeability and thermal and mechanical properties of high strength self-compacting concrete10.1016/j.msea.2010.09.074 ↗
30. Canadian use of ground granulated blast-furnace slag as a supplementary cementing material for enhanced performance of concrete10.1139/l00-014 ↗
31. Mehta, P.K. (1986). Concrete: Structure, Properties and Materials, Prentice Hall.
32. Durability properties of concrete containing 50% and 65% slag10.1016/j.conbuildmat.2009.02.040 ↗
33. Bensted, J., and Barnes, P. (2002). Blast furnace cements. Structure and Performance of Cements, Spon Press. [2nd ed.].
34. Menéndez, E., Matschei, T., and Glasser, F.P. (2013). Sulfate attack of concrete. Performance of Cement-Based Materials in Aggressive Aqueous Environments, Springer.10.1007/978-94-007-5413-3_2 ↗
35. The impact of alumina availability on sulfate resistance of slag composite cements10.1016/j.conbuildmat.2016.05.015 ↗
36. Durability of self-consolidating concrete to sulfate attack under combined cyclic environments and flexural loading10.1016/j.cemconres.2008.12.003 ↗
37. Crystallization in pores10.1016/S0008-8846(99)00002-2 ↗
38. Influence of additions of anatase TiO2 nanoparticles on early-age properties of cement-based materials10.3141/2141-08 ↗
39. Effects of nano-TiO2 on strength, shrinkage and microstructure of alkali activated slag pastes10.1016/j.cemconcomp.2014.11.009 ↗
40. Influences of nano-TiO2 on the properties of cement-based materials: Hydration and drying shrinkage10.1016/j.conbuildmat.2015.02.003 ↗
41. Characteristics and efficiency of photocatalytic cementitious materials: Type of binder, roughness and microstructure10.1016/j.cemconres.2015.02.003 ↗
42. TiO2 nanoparticles effects on physical, thermal and mechanical properties of self compacting concrete with ground granulated blast furnace slag as binder10.1016/j.enbuild.2010.12.025 ↗
43. Mechanism of sulfate attack: A fresh look: Part 2. Proposed mechanisms10.1016/S0008-8846(02)00958-4 ↗
44. Effect of pore structure on salt crystallization damage of cement-based materials: Consideration of w/b and nanoparticle use10.1016/j.cemconres.2017.04.002 ↗
45. Durability properties and microstructure of ground granulated blast furnace slag cement concrete10.1007/s40069-013-0063-y ↗