journal article·2020-10-27Open access

Preliminary Interpretation of the Induction Period in Hydration of Sodium Hydroxide/Silicate Activated Slag

Yibing Zuo, Guang Ye

Materials· Volume 13· Issue 21

Abstract

Many calorimetric studies have been carried out to investigate the reaction process of alkali-activated slag paste. However, the origin of the induction period and action mechanism of soluble Si in the dissolution of slag are still not clear. Moreover, the mechanisms behind different reaction periods are not well described. In this study, the reaction kinetics of alkali-activated slag paste was monitored by isothermal calorimetry and the effect of soluble Si was investigated through a dissolution test. The results showed that occurrence of the induction period in hydration of alkali-activated slag paste depended on the presence of soluble Si in alkaline activator and the soluble Si slowed down the dissolution of slag. A dissolution theory-based mechanism was introduced and applied to the dissolution of slag, showing good interpretation of the action mechanism of soluble Si. With this dissolution theory-based mechanism, origin of the induction period in hydration of alkali-activated slag was explicitly interpreted.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Civil and Hydraulic Engineering, Huazhong University of Science and Technology, Wuhan 430074, China

Faculty of Civil Engineering and Geosciences, Delft University of Technology, Stevinweg 1, 2628 CN Delft, The Netherlands

Funding

China Scholarship Council · Fundamental Research Funds for the Central Universities

References (58)

Show source-provided references
1. Alkali-activated slag cement and concrete: A review of properties and problems10.1680/adcr.1995.7.27.93 ↗
2. Alkali-activated cements opportunities and challenges10.1016/S0008-8846(98)00093-3 ↗
3. Technical and commercial progress in the adoption of geopolymer cement10.1016/j.mineng.2011.09.009 ↗
4. Alkali-activated binders: A review: Part 1. Historical background, terminology, reaction mechanisms and hydration products10.1016/j.conbuildmat.2007.10.015 ↗
5. A critical review on application of alkali activated slag as a sustainable composite binder
6. The role of inorganic polymer technology in the development of ‘green concrete’10.1016/j.cemconres.2007.08.018 ↗
7. Assessment of CO2 reduction of alkali-activated concrete10.1016/j.jclepro.2012.08.001 ↗
8. Alkali-activated slag mortars: Mechanical strength behaviour10.1016/S0008-8846(99)00154-4 ↗
9. Durability of alkali-activated binders: A clear advantage over Portland cement or an unproven issue?10.1016/j.conbuildmat.2011.12.017 ↗
10. Durability of alkali-activated materials: Progress and perspectives10.1111/jace.12831 ↗
11. Influence of starting material on the early age hydration kinetics, microstructure and composition of binding gel in alkali activated binder systems10.1016/j.cemconcomp.2013.11.010 ↗
12. Alkali activation of a slag at ambient and elevated temperatures10.1016/j.cemconcomp.2011.08.003 ↗
13. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag–Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
14. A method based on isothermal calorimetry to quantify the influence of moisture on the hydration rate of young cement pastes10.1016/j.cemconres.2010.02.005 ↗
15. Modeling hydration properties and temperature developments of early-age concrete pavement using calorimetry tests10.1016/j.tca.2010.09.003 ↗
16. Fine limestone additions to regulate setting in high volume fly ash mixtures10.1016/j.cemconcomp.2011.09.004 ↗
17. Isothermal and solution calorimetry to assess the effect of superplasticizers and mineral admixtures on cement hydration10.1007/s10973-011-1479-8 ↗
18. Study of the hydration of Portland cement blended with blast-furnace slag by calorimetry and thermogravimetry10.1007/s10973-010-0841-6 ↗
19. Characteristics of the hydration heat evolution of composite binder at different hydrating temperature10.1016/j.tca.2014.04.010 ↗
20. Reaction kinetics in sodium silicate powder and liquid activated slag binders evaluated using isothermal calorimetry10.1016/j.tca.2012.07.010 ↗
21. Very early-age reaction kinetics and microstructural development in alkali-activated slag10.1016/j.cemconcomp.2014.09.001 ↗
22. A calorimetric study of early hydration of alkali-slag cements10.1016/0008-8846(95)00126-W ↗
23. Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag–fly ash blends10.1016/j.conbuildmat.2015.01.065 ↗
24. Evolution of binder structure in sodium silicate-activated slag-metakaolin blends10.1016/j.cemconcomp.2010.09.004 ↗
25. Study on the interaction mechanism between slags and alkali silicate activators: A hydration kinetics approach10.1016/j.conbuildmat.2020.118900 ↗
26. Ouyang, X., Ma, Y., Liu, Z., Liang, J., and Ye, G. (2019). Effect of the sodium silicate modulus and slag content on fresh and hardened properties of alkali-activated fly ash/slag. Minerals, 10.10.3390/min10010015 ↗
27. Reaction kinetics and kinetics models of alkali activated phosphorus slag10.1016/j.conbuildmat.2019.117728 ↗
28. Temperature and activator effect on early-age reaction kinetics of alkali-activated slag binders10.1016/j.conbuildmat.2016.03.098 ↗
29. The hydration of slag, Part 1: Reaction models for alkali-activated slag10.1007/s10853-006-0873-2 ↗
30. ASTM (2014). Standard Practice for Measuring Hydration Kinetics of Hydraulic Cementitious Mixtures Using Isothermal Calorimetry, ASTM International. C1679-14.
31. Ye, G. (2003). Experimental Study and Numerical Simulation of the Development of the Microstructure and Permeability of Cementitious Materials. [Ph.D. Thesis, Delft University of Technology].
32. Zuo, Y., and Ye, G. (2018). Pore Structure Characterization of Sodium Hydroxide Activated Slag Using Mercury Intrusion Porosimetry, Nitrogen Adsorption, and Image Analysis. Materials, 11.10.3390/ma11061035 ↗
33. Thermodynamic equilibrium calculations in cementitious systems10.1617/s11527-010-9592-x ↗
34. GEM-Selektor geochemical modeling package: Revised algorithm and GEMS3K numerical kernel for coupled simulation codes
35. GEM-Selektor geochemical modeling package: TSolMod library and data interface for multicomponent phase models10.3749/canmin.50.5.1173 ↗
36. A thermodynamic model for C-(N-)A-S-H gel: CNASH_ss. Derivation and validation10.1016/j.cemconres.2014.07.005 ↗
37. Thermodynamic modelling of alkali-activated slag cements10.1016/j.apgeochem.2015.06.006 ↗
38. Geopolymers and related alkali-activated materials10.1146/annurev-matsci-070813-113515 ↗
39. Hydration of alkali-activated slag: Thermodynamic modelling10.1680/adcr.2007.19.2.81 ↗
40. Hydration products of alkali activated slag cement10.1016/0008-8846(95)00045-E ↗
41. The characterization of hardened alkali-activated blast-furnace slag pastes and the nature of the calcium silicate hydrate (C-S-H) phase10.1016/0008-8846(94)90002-7 ↗
42. Coupled thermodynamic modelling and experimental study of sodium hydroxide activated slag10.1016/j.conbuildmat.2018.08.087 ↗
43. Kinetic study on hydration of alkali-activated slag10.1016/0008-8846(93)90062-E ↗
44. Theoretical prediction of the thermodynamic behavior of aqueous electrolytes by high pressures and temperatures; IV, Calculation of activity coefficients, osmotic coefficients, and apparent molal and standard and relative partial molal properties to 600 degrees C and 5 kb10.2475/ajs.281.10.1249 ↗
45. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
46. Quantitative analysis of phase assemblage and chemical shrinkage of alkali-activated slag10.3151/jact.14.245 ↗
47. The mechanism, rates and consequences of basaltic glass dissolution: I. An experimental study of the dissolution rates of basaltic glass as a function of aqueous Al, Si and oxalic acid concentration at 25 C and pH = 3 and 1110.1016/S0016-7037(01)00664-0 ↗
48. General kinetic description of multioxide silicate mineral and glass dissolution10.1016/S0016-7037(01)00710-4 ↗
49. Mechanism, rates, and consequences of basaltic glass dissolution: II. An experimental study of the dissolution rates of basaltic glass as a function of pH and temperature10.1016/S0016-7037(03)00176-5 ↗
50. The effect of aluminum, pH, and chemical affinity on the rates of aluminosilicate dissolution reactions10.1016/0016-7037(94)90281-X ↗
51. Designing precursors for geopolymer cements10.1111/j.1551-2916.2008.02787.x ↗
52. Variation of Crystal Dissolution Rate Based on a Dissolution Stepwave Model10.1126/science.1058173 ↗
53. Mechanisms of classical crystal growth theory explain quartz and silicate dissolution behavior10.1073/pnas.0507777102 ↗
54. Dissolution theory applied to the induction period in alite hydration10.1016/j.cemconres.2010.01.012 ↗
55. New insights into the hydration of slag in alkaline media using a micro-reactor approach10.1016/j.cemconres.2015.09.015 ↗
56. Ion-specific effects influencing the dissolution of tricalcium silicate10.1016/j.cemconres.2014.02.006 ↗
57. Microscopy and microanalysis of inorganic polymer cements. 2: The gel binder10.1007/s10853-008-3078-z ↗
58. The mechanism of geopolymer gel formation investigated through seeded nucleation10.1016/j.colsurfa.2007.12.019 ↗