Electrochemical Migration Behavior of Copper-Clad Laminate and Electroless Nickel/Immersion Gold Printed Circuit Boards under Thin Electrolyte Layers
Source abstract
Abstract
The electrochemical migration (ECM) behavior of copper-clad laminate (PCB-Cu) and electroless nickel/immersion gold printed circuit boards (PCB-ENIG) under thin electrolyte layers of different thicknesses containing 0.1 M Na2SO4 was studied. Results showed that, under the bias voltage of 12 V, the reverse migration of ions occurred. For PCB-Cu, both copper dendrites and sulfate precipitates were found on the surface of FR-4 (board material) between two plates. Moreover, the Cu dendrite was produced between the two plates and migrated toward cathode. Compared to PCB-Cu, PCB-ENIG exhibited a higher tendency of ECM failure and suffered from seriously short circuit failure under high relative humidity (RH) environment. SKP results demonstrated that surface potentials of the anode plates were greater than those of the cathode plates, and those potentials of the two plates exhibited a descending trend as the RH increased. At the end of the paper, an electrochemical migration corrosion failure model of PCB was proposed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Nanoporous metals and alloys · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China
State Key Laboratory for Marine Corrosion and Protection, Luoyang Ship Material Research Institute, Qingdao 266101, China
Ningbo Institute of Material Technology & Engineering, Chinese Academy of Sciences, Ningbo 315201, China
References (29)
Show source-provided references
1. Leygraf, C., and Graedel, T. (2000). Atmospheric Corrosion, Wiley and Sons Press.
2. Effect of Ag on oxidation of Cu-base leadframe10.1016/j.microrel.2010.10.010 ↗
3. Surface failure analysis of a field-exposed copper-clad plate in a marine environment with industrial pollution10.1016/j.apsusc.2016.12.118 ↗
4. Copper patinas formed in the atmosphere—I. Introduction10.1016/0010-938X(87)90047-3 ↗
5. Reactions of copper patina compounds—I. Influence of some air pollutants10.1016/S1352-2310(98)00057-0 ↗
6. Reactions of copper patina compounds—II. Influence of sodium chloride in the presence of some air pollutants10.1016/S1352-2310(98)00058-2 ↗
7. Atmospheric corrosion of copper and the colour, structure and composition of natural patinas on copper10.1016/j.corsci.2005.09.011 ↗
8. Origin of surface defects in PCB final finishes by the electroless nickel immersion gold process10.1007/s11664-007-0360-9 ↗
9. Corrosion of RoHS-Compliant surface finishes in corrosive mixed flowing gas environments10.1007/s11664-011-1799-2 ↗
10. Electrochemical migration, whisker formation, and corrosion behavior of printed circuit board under wet H2S environment10.1016/j.electacta.2013.10.051 ↗
11. Effect of temperature and relative humidity on the impedance degradation of dust-contaminated electronics10.1149/2.024303jes ↗
12. Sliding contacts on printed circuit boards and wear behavior10.1051/epjap/2010020 ↗
13. Effect of mold on corrosion behavior of printed circuit board-copper and ENIG finished10.3724/SP.J.1037.2012.00033 ↗
14. The pH effect on black spots in surface finish: Electroless nickel immersion gold10.1016/j.apsusc.2010.06.033 ↗
15. On the electrochemical migration mechanism of tin in electronics10.1016/j.corsci.2011.06.015 ↗
16. Initial stage of silver electrochemical migration degradation10.1016/j.microrel.2006.07.080 ↗
17. Electromigration lifetimes and void growth at low cumulative failure probability10.1016/j.microrel.2006.08.001 ↗
18. Effect of bias voltage on the electrochemical migration behaviors of Sn and Pb10.1109/TDMR.2009.2026737 ↗
19. Microstructure of conductive anodic filaments formed during accelerated testing of printed wiring boards10.1108/eb044042 ↗
20. Copper dendrites: Synthesis, mechanism discussion, and application in determination of ltyrosine10.1021/cg7011028 ↗
21. Copper may destroy chip-level reliability: Handle with care-mechanism and conditions for copper migrated resistive short formation10.1109/55.737556 ↗
22. Electrochemistry on microcircuits. II: Copper dendrites in oxalic acid10.1016/j.mee.2007.12.054 ↗
23. The investigation of the corrosion properties of metals, covered with adsorbed electrolyte layers—A new experimental technique10.1016/0010-938X(87)90043-6 ↗
24. On the atmospheric corrosion of metals which are covered with thin electrolyte layers—I. Verification of the experimental technique10.1016/0010-938X(90)90032-Z ↗
25. On the atmospheric corrosion of metals which are covered with thin electrolyte layers—II. Experimental results10.1016/0010-938X(90)90033-2 ↗
26. Electrochemical migration of tin in thin electrolyte layer containing chloride ions10.1016/j.corsci.2013.04.015 ↗
27. In situ study the dependence of electrochemical migration of tin on chloride10.1016/j.elecom.2012.11.010 ↗
28. Comparing migratory resistive short formation abilities of conductor systems applied in advanced interconnection systems10.1016/S0026-2714(00)00093-7 ↗
29. Porosity of electrodeposited coatings: Its cause, nature, effect and management10.1515/CORRREV.1992.10.3-4.217 ↗