journal article·2019-01-30Open access

Structural and Mechanical Properties of Ti–Co Alloys Treated by High Pressure Torsion

Boris B. Straumal, Anna Korneva, Askar R. Kilmametov, Lidia Lityńska-Dobrzyńska, Alena S. Gornakova, Robert Chulist, Mikhail I. Karpov, Paweł Zięba

Materials· Volume 12· Issue 3

Abstract

The microstructure and properties of titanium-based alloys can be tailored using severe plastic deformation. The structure and microhardness of Ti–4 wt.% Co alloy have been studied after preliminary annealing and following high pressure torsion (HPT). The Ti–4 wt.% Co alloy has been annealed at 400, 500, and 600 °C, i.e., below the temperature of eutectoid transformation in the Ti–4 wt.% Co system. The amount of Co dissolved in α-Ti increased with increasing annealing temperature. HPT led to the transformation of α-Ti in ω-Ti. After HPT, the amount of ω-phase in the sample annealed at 400 °C was about 80­85%, i.e., higher than in pure titanium (about 40%). However, with increasing temperature of pre-annealing, the portion of ω-phase decreased (60–65% at 500 °C and about 5% at 600 °C). The microhardness of all investigated samples increased with increasing temperature of pre-annealing.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Solid State Physics and Chernogolovka Scientific Center, Russian Academy of Sciences, Chernogolovka 142432, Russia

Karlsruhe Institute of Technology (KIT), Institute of Nanotechnology, 76344 Eggenstein-Leopoldshafen, Germany

National University of Science and Technology «MISIS», Moscow 119049, Russia

Institute of Metallurgy and Materials Science, Polish Academy of Sciences, 30-059 Krakow, Poland

Funding

Deutsche Forschungsgemeinschaft · Russian Foundation for Fundamental Investigations · National Science Center of Poland

References (65)

Show source-provided references
1. Titanium alloys in total joint replacement-a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
2. Recent metallic materials for biomedical applications10.1007/s11661-002-0109-2 ↗
3. Biocompatibility and osteogenesis of refractory metal implants, titanium, hafnium, niobium, tantalum and rhenium10.1016/S0142-9612(00)00275-1 ↗
4. The use of titanium for medical applications in the USA10.1016/0921-5093(96)10243-4 ↗
5. An evaluation of a NiTiCo alloy and its suitability for medical device applications10.1007/s11665-011-9845-z ↗
6. Evaluation of an experimental Ti-Co alloy for dental restorations10.1002/jbm.b.32961 ↗
7. Mechanical biocompatibilities of titanium alloys for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
8. Synthesis and characterization of Ti-Co alloy foam for biomedical applications10.1016/S1003-6326(15)64028-6 ↗
9. Binary titanium alloys as dental implant materials-a review10.1093/rb/rbx027 ↗
10. Surface investigations of oxide layers on cobalt-chromium alloyed orthopedic implants using ESCA technique
11. Preparation of high corrosion resistant titanium alloys by spark plasma sintering10.2320/jinstmet1952.63.9_1149 ↗
12. On superplasticity of two phase alpha-titanium-intermetallic Ti–(Co, Ni)–Al alloy10.1016/0956-7151(95)00032-Q ↗
13. Measurement of phase equilibria in Ti-Co-Pt ternary system10.1016/j.calphad.2017.12.007 ↗
14. Investigation of phase equilibria in the Ti-Co-Zr ternary system10.1016/j.calphad.2017.02.001 ↗
15. Phase equilibria in the crystallization interval in the Ti-Co-Sn system at above 50 at % Ti10.1016/j.jallcom.2016.01.160 ↗
16. Microstructural evolution in novel suction cast multicomponent Ti-Fe-Co alloys10.1007/s11661-014-2675-5 ↗
17. Microstructure and properties of Ti-Co-Si ternary intermetallic alloys10.1016/j.jallcom.2007.09.106 ↗
18. Effect of nickel addition on microstructure and properties of Ti-Co-Ni alloys10.1016/0142-9612(95)96876-2 ↗
19. Evaluation of microstructure, microhardness, and electrochemical properties of laser-deposited Ti-Co coatings on Ti-6Al-4V alloy10.1007/s00170-018-2106-7 ↗
20. Microstructural and tribological behavior of in situ synthesized Ti/Co coatings on Ti-6Al-4V alloy using laser surface cladding technique10.1007/s00170-017-1300-3 ↗
21. A study on the influence of laser power on microstructural evolution and tribological functionality of metallic coatings deposited on Ti-6Al-4V alloy
22. The effect of laser based synthesized Ti–Co coating on microstructure and mechanical properties of Ti6A14V alloy10.1016/j.promfg.2016.12.014 ↗
23. In-situ laser-fabrication and characterization of TiC-containing Ti-Co composite on pure Ti substrate10.1016/j.jallcom.2009.03.168 ↗
24. Study of phase separation in Ti-Co-N thin films on silicon substrate10.1007/s003390050510 ↗
25. CoSi2 formation in contact systems based on Ti-Co alloy with low cobalt content
26. The α→ω and β→ω phase transformations in Ti-Fe alloys under high-pressure torsion10.1016/j.actamat.2017.10.051 ↗
27. Transformations of α′ martensite in Ti-Fe alloys under high pressure torsion10.1016/j.scriptamat.2017.04.010 ↗
28. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
29. Mechanical alloying of Cu and Fe induced by severe plastic deformation of a Cu-Fe composite10.1016/j.actamat.2005.01.024 ↗
30. Grain boundary films in Al–Zn alloys after high pressure torsion10.1016/j.scriptamat.2013.09.019 ↗
31. Phase transitions in metallic alloys driven by the high pressure torsion10.1016/j.acme.2013.07.002 ↗
32. Phase transitions induced by severe plastic deformation: Steady-state and equifinality10.3139/146.111215 ↗
33. Phase transitions in Cu-based alloys under high pressure torsion10.1016/j.jallcom.2016.12.057 ↗
34. Donachie, M.J. (2000). Titanium: A Technical Guide, ASM International. [2nd ed.].10.31399/asm.tb.ttg2.9781627082693 ↗
35. Pressure-induced α→ω transition in titanium metal: A systematic study of the effects of uniaxial stress10.1016/j.physb.2004.10.030 ↗
36. New mechanism for the α to ω martensitic transformation in pure titanium10.1103/PhysRevLett.91.025701 ↗
37. Omega phase in materials10.1016/0079-6425(82)90002-0 ↗
38. Banerjee, S., and Mukhopadhyay, P. (2010). Phase Transformations: Examples from Titanium and Zirconium Alloy, Elsevier.
39. The formation of omega phase in titanium and zirconium alloys: A review10.1007/BF00550217 ↗
40. Transformation pathway upon heating of Ti–Fe alloys deformed by high-pressure torsion10.1002/adem.201700933 ↗
41. Thermal stability of athermal ω-Ti(Fe) produced upon quenching of β-Ti(Fe)
42. Phase transformations in Ti-Fe alloys induced by high pressure torsion10.1002/adem.201500143 ↗
43. Kilmametov, A.R., Ivanisenko, Y., Straumal, B.B., Gornakova, A.S., Mazilkin, A.A., and Hahn, H. (2018). The α→ω transformation in titanium-cobalt alloys under high-pressure torsion. Metals, 8.10.3390/met8010001 ↗
44. Diffusive and displacive phase transitions in Ti-Fe and Ti-Co alloys under high pressure torsion10.1016/j.jallcom.2017.11.317 ↗
45. Deformation behavior of amorphous Co-Fe-Cr-Si-B alloys in the initial stages of severe plastic deformation10.3103/S1062873814100165 ↗
46. Massalski, T.B. (1991). Binary Alloy Phase Diagrams, American Society for Metals.
47. Gornakova, A.S., Straumal, A.B., Khodos, I.I., Gnesin, I.B., Mazilkin, A.A., Afonikova, N.S., and Straumal, B.B. (2019). Effect of composition, annealing temperature and high pressure torsion on structure and hardness of Ti-V and Ti-V-Al alloys. J. Appl. Phys., 125.10.1063/1.5053937 ↗
48. Nanostructure formation on the surface of railway tracks10.1016/S0921-5093(00)01947-X ↗
49. Influence of the thermal treatment on the deformation-induced precipitation of a hypoeutectic Al-7 wt% Si casting alloy deformed by high-pressure torsion10.1016/j.jallcom.2010.09.122 ↗
50. The mechanism of formation of nanostructure and dissolution of cementite in a pearlitic steel during high pressure torsion10.1016/S1359-6454(03)00419-1 ↗
51. Deformation-induced anomalous phase transformations in nanocrystalline FCC Fe-Ni based alloys10.1016/S0965-9773(97)00150-5 ↗
52. Bulk mechanical alloying of Cu–Ag and Cu/Zr two-phase microstructures by accumulative roll-bonding process10.1016/j.actamat.2006.12.027 ↗
53. Structure and properties of amorphous and nanocrystalline NiTi prepared by severe plastic deformation and annealing10.1016/S0921-5093(02)00122-3 ↗
54. Alloy composition, deformation temperature, pressure and post-deformation annealing effects in severely deformed Ti-Ni based shape memory alloys10.1016/j.actamat.2005.02.032 ↗
55. Solid state amorphization in cold drawn Cu/Nb wires10.1016/S1359-6454(00)00338-4 ↗
56. Synthesis of non-equilibrium phases in immiscible metals mechanically mixed by high pressure torsion10.1007/s10853-010-5240-7 ↗
57. Ferromagnetic behaviour of ZnO: Role of grain boundaries10.3762/bjnano.7.185 ↗
58. Bulk nanocrystalline ferrite stabilized through grain boundary carbon segregation10.1002/adem.201800443 ↗
59. Fe–C nanograined alloys obtained by high pressure torsion: Structure and magnetic properties10.1016/j.msea.2008.03.052 ↗
60. Structure and properties of nanograined Fe–C alloys after severe plastic deformation10.1002/adem.201000312 ↗
61. The effect of pressure on migration of the [001] tilt grain boundaries in the tin bicrystals10.1016/0036-9748(84)90509-X ↗
62. The influence of pressure on indium diffusion along single tin–germanium interphase boundaries10.1016/0036-9748(83)90156-4 ↗
63. Elastic modulus of TI-6AL-4V titanium alloy10.22226/2410-3535-2015-1-67-69 ↗
64. In situ observations of lattice expansion and transformation rates of α and β phases in Ti-6Al-4V10.1016/j.msea.2004.08.084 ↗
65. Dependence of the specific energy of the β/α interface in the VT6 titanium alloy on the heating temperature in the interval 600–975 °C10.1134/S1063776116020205 ↗