journal article·2015-11-04

A Highly Thermostable Ceramic-Grafted Microporous Polyethylene Separator for Safer Lithium-Ion Batteries

Xiaoming Zhu, Xiaoyu Jiang, Xinping Ai, Hanxi Yang, Yuliang Cao

Publisher page

Abstract

The safety concern is a critical obstacle to large-scale energy storage applications of lithium-ion batteries. A thermostable separator is one of the most effective means to construct the safe lithium-ion batteries. Herein, we demonstrate a novel ceramic (SiO2)-grafted PE separator prepared by electron beam irradiation. The separator shows similar thickness and pore structure to the bare separator, while displaying strong dimensional thermostability, as the shrinkage ratio is only 20% even at an elevated temperature of 180 °C. Besides, the separator is highly electrochemically inert, showing no adverse effect on the energy and power output of the batteries. Considering the excellent electrochemical and thermal stability, the SiO2-grafted PE separator developed in this work is greatly beneficial for constructing safer lithium-ion batteries.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Hubei Collaboration Innovation Center of Non-power Nuclear Technology, Hubei University of Science and Technology, Xianning 437100, P. R. China

School of Nuclear Technology & Chemistry and Biology, Hubei University of Science and Technology, Xianning 437100, P. R. China

College of Chemistry and Molecular Science, Hubei Key Laboratory of Electrochemical Power Sources, Wuhan University, Wuhan 430072, China

Funding

Natural Science Foundation of Hubei Province · Hubei National Funds for Distinguished Young Scholars · Program for New Century Excellent Talents in University · Hubei Province

References (32)

Show source-provided references
1. 10.1038/3510464410.1038/35104644 ↗
2. 10.1016/j.jpowsour.2011.01.06810.1016/j.jpowsour.2011.01.068 ↗
3. 10.1016/j.jpowsour.2004.05.06410.1016/j.jpowsour.2004.05.064 ↗
4. 10.3390/en304086610.3390/en3040866 ↗
5. 10.1016/j.jpowsour.2006.10.06510.1016/j.jpowsour.2006.10.065 ↗
6. 10.1021/cr020738u10.1021/cr020738u ↗
7. 10.1007/s10008-010-1264-910.1007/s10008-010-1264-9 ↗
8. 10.1016/S0378-7753(98)00168-210.1016/S0378-7753(98)00168-2 ↗
9. 10.1016/j.jpowsour.2010.06.11210.1016/j.jpowsour.2010.06.112 ↗
10. 10.1016/S0011-9164(02)00465-410.1016/S0011-9164(02)00465-4 ↗
11. 10.1016/j.jpowsour.2009.10.08510.1016/j.jpowsour.2009.10.085 ↗
12. 10.1016/j.jpowsour.2010.11.03710.1016/j.jpowsour.2010.11.037 ↗
13. 10.1039/c4ra01309c10.1039/c4ra01309c ↗
14. 10.1016/j.jpowsour.2012.03.03810.1016/j.jpowsour.2012.03.038 ↗
15. 10.1149/1.273072710.1149/1.2730727 ↗
16. 10.1016/j.jpowsour.2009.11.02010.1016/j.jpowsour.2009.11.020 ↗
17. 10.1002/aenm.20120111210.1002/aenm.201201112 ↗
18. 10.1021/am508149n10.1021/am508149n ↗
19. 10.1016/j.electacta.2014.04.10910.1016/j.electacta.2014.04.109 ↗
20. 10.1039/C5RA01061F10.1039/C5RA01061F ↗
21. 10.1016/j.electacta.2009.01.05510.1016/j.electacta.2009.01.055 ↗
22. 10.1016/j.jpowsour.2009.12.05610.1016/j.jpowsour.2009.12.056 ↗
23. 10.1016/S0141-3910(00)00186-510.1016/S0141-3910(00)00186-5 ↗
24. 10.1007/s10800-014-0661-710.1007/s10800-014-0661-7 ↗
25. Mostafavi M. · 2008
26. 10.1016/S0079-6700(03)00047-910.1016/S0079-6700(03)00047-9 ↗
27. Reichmanis, E.; Frank, C. W.; O’Donnell, H.; Hill, D. J.InIrradiation of Polymeric Materials;Reichmanis, E.; Frank, C. W.; O’Donnell, H.; Hill, D. J., Eds.American Chemical Society:Washington, DC, 1993; Chapter 1, pp1–8.10.1021/bk-1993-0527.ch001 ↗
28. 10.1021/cr400549910.1021/cr4005499 ↗
29. 10.1016/j.apsusc.2005.09.06810.1016/j.apsusc.2005.09.068 ↗
30. 10.1016/S0142-9418(01)00124-610.1016/S0142-9418(01)00124-6 ↗
31. 10.1016/j.electacta.2009.02.08810.1016/j.electacta.2009.02.088 ↗
32. 10.1149/2.003309jes10.1149/2.003309jes ↗