journal article·2023-03-04Open access

The Effect of a Duplex Surface Treatment on the Corrosion and Tribocorrosion Characteristics of Additively Manufactured Ti-6Al-4V

Kelsey Ann Vella, Joseph Buhagiar, Glenn Cassar, Martina Marie Pizzuto, Luana Bonnici, Jian Chen, Xiyu Zhang, Zhiquan Huang, Ann Zammit

Materials· Volume 16· Issue 5

Abstract

The use of additively manufactured components specifically utilizing titanium alloys has seen rapid growth particularly in aerospace applications; however, the propensity for retained porosity, high(er) roughness finish, and detrimental tensile surface residual stresses are still a limiting factor curbing its expansion to other sectors such as maritime. The main aim of this investigation is to determine the effect of a duplex treatment, consisting of shot peening (SP) and a coating deposited by physical vapor deposition (PVD), to mitigate these issues and improve the surface characteristics of this material. In this study, the additive manufactured Ti-6Al-4V material was observed to have a tensile and yield strength comparable to its wrought counterpart. It also exhibited good impact performance undergoing mixed mode fracture. It was also observed that the SP and duplex treatments resulted in a 13% and 210% increase in hardness, respectively. Whilst the untreated and SP treated samples exhibited a similar tribocorrosion behavior, the duplex-treated sample exhibited the greatest resistance to corrosion-wear observed by the lack of damage on the surface and the diminished material loss rates. On the other hand, the surface treatments did not improve the corrosion performance of the Ti-6Al-4V substrate.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Surface Treatment and Residual Stress · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Metallurgy and Materials Engineering, University of Malta, MSD 2080 Msida, Malta

School of Materials Science and Engineering, Southeast University, Nanjing 211189, China

Funding

Malta Council for Science and Technology (MCST) · Ministry of Science and Technology (MOST) of the People’s Republic of China

References (64)

Show source-provided references
1. Carlton, J.S. (2007). Marine Propellers and Propulsion, Butterworth-Heinemann. [2nd ed.].10.1016/B978-075068150-6/50004-8 ↗
2. The Application and Prospect of Titanium Materials in Marine Engineering Equipments
3. Leyens, C., and Peters, M. (2003). Titanium and Titanium Alloys: Fundamentals and Applications, Wiley. [1st ed.].10.1002/3527602119 ↗
4. Microstructure and Mechanical Properties of Wrought and Additive Manufactured Ti-6Al-4V Cylindrical Bars10.1016/j.protcy.2015.07.037 ↗
5. Microstructure and mechanical properties of selective laser melted Ti6Al4V alloy10.1088/1757-899X/266/1/012009 ↗
6. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
7. Effect of shotpeening on sliding wear and tensile behavior of titanium implant alloys10.1016/j.matdes.2013.11.052 ↗
8. Chowdhury, M.A. (2018). Advanced Surface Engineering Research, IntechOpen.10.5772/intechopen.75772 ↗
9. Microstructure change and corrosion resistance of selective laser melted Ti-6Al-4V alloy subjected to pneumatic shot peening and ultrasonic shot peening10.1088/2051-672X/ac4c83 ↗
10. Tribological Behavior and Corrosion Resistance of S30432 Steel after Different Shot Peening Processes10.1007/s11665-021-06249-3 ↗
11. Tribocorrosion properties and mechanism of a shot peened AISI 4140 low-alloy steel10.1016/j.surfcoat.2022.128444 ↗
12. Effects of combined plasma-carburizing and shot-peening on fatigue and wear properties of Ti–6Al–4V alloy10.1016/j.surfcoat.2008.11.013 ↗
13. Surface engineering to improve the durability and lubricity of Ti–6Al–4V alloy10.1016/j.wear.2010.11.021 ↗
14. Davis, J.R. (2001). Surface Engineering for Corrosion and Wear Resistance, ASM International.10.31399/asm.tb.secwr.9781627083157 ↗
15. Improving corrosion resistance of Ti–6Al–4V alloy through plasma-assisted PVD deposited nitride coatings10.1016/j.corsci.2014.07.047 ↗
16. Comparison of dry sliding friction and wear of Ti6Al4V alloy treated by plasma electrolytic oxidation and PVD coating10.1016/j.wear.2007.01.045 ↗
17. Improved structural, mechanical, corrosion and tribocorrosion properties of Ti45Nb alloys by TiN, TiAlN monolayers, and TiAlN/TiN multilayer ceramic films
18. Wear behaviours of PVD-TiN coating onTi-6Al-4V alloy processed by laser powder bed fusion or conventionally processed. Int10.1007/s00170-021-06714-2 ↗
19. Structural, mechanical and tribocorrosion behaviour in artificial seawater of CrN/AlN nano-multilayer coatings on F690 steel substrates10.1016/j.apsusc.2017.09.166 ↗
20. Improvement in the tribocorrosion performance of CrCN coating by multilayered design for marine protective application10.1016/j.apsusc.2020.147061 ↗
21. The Adhesion of CrN Thin Films Deposited on Modified 42CrMo4 Steel10.1155/2017/4064208 ↗
22. Investigations on the adhesion and fatigue characteristics of hybrid surface-treated titanium alloy10.1016/j.surfcoat.2021.128002 ↗
23. Effect of substrate roughness on adhesion and tribological properties of nc-TiAlN/a-Si3N4nanocomposite coatings deposited by cathodic arc PVD process10.1179/1743294415Y.0000000005 ↗
24. Effect of high energy shot peening on the wear resistance of TiN films on a TA2 surface10.1016/j.surfcoat.2019.07.045 ↗
25. Lekoadi, P., Tlotleng, M., Annan, K., Maledi, N., and Masina, B. (2021). Evaluation of Heat Treatment Parameters on Microstructure and Hardness Properties of High-Speed Selective Laser Melted Ti6Al4V. Metals, 11.10.3390/met11020255 ↗
26. Characterization on surface mechanical properties of Ti–6Al–4V after shot peening10.1016/j.jallcom.2016.01.119 ↗
27. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
28. Fabrication and characterization of selective laser melting printed Ti–6Al–4V alloys subjected to heat treatment for customized implants design10.1016/j.pnsc.2016.12.006 ↗
29. The effect of substrate surface roughness on the wear of DLC coatings10.1016/S0043-1648(99)00351-8 ↗
30. Selective Laser Melting of Titanium Alloys and Titanium Matrix Composites for Biomedical Applications: A Review10.1002/adem.201500419 ↗
31. Effect of different surface asperities and surface hardness induced by shot-peening on the fretting wear behavior of Ti-6Al-4V10.1016/j.surfcoat.2018.06.092 ↗
32. Control of Structure and Properties of Nanostructured Multilayer Composite Coatings Applied to Cutting Tools as a Way to Improve Efficiency of Technological Cutting Operations10.4028/www.scientific.net/JNanoR.37.51 ↗
33. Bartolomeu, F., Gasik, M., Silva, F.S., and Miranda, G. (2022). Mechanical Properties of Ti6Al4V Fabricated by Laser Powder Bed Fusion: A Review Focused on the Processing and Microstructural Parameters Influence on the Final Properties. Metals, 12.10.3390/met12060986 ↗
34. Callister, W.D. (2007). Materials Science and Engineering: An Introduction, John Wiley and Sons, Inc.. [7th ed.].
35. Tensile behavior of Ti-6Al-4V alloy fabricated by selective laser melting: Effects of microstructures and as-built surface quality10.1007/s41230-018-8064-8 ↗
36. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
37. He, J., Li, D., Jiang, W., Ke, L., Qin, G., Ye, Y., Qin, Q., and Qiu, D. (2019). The Martensitic Transformation and Mechanical Properties of Ti6Al4V Prepared via Selective Laser Melting. Materials, 12.10.3390/ma12020321 ↗
38. Li, F., Qi, B., Zhang, Y., Guo, W., Peng, P., Zhang, H., He, G., Zhu, D., and Yan, J. (2021). Effects of Heat Treatments on Microstructures and Mechanical Properties of Ti6Al4V Alloy Produced by Laser Solid Forming. Metals, 11.10.3390/met11020346 ↗
39. Effects of defects on mechanical properties in metal additive manufacturing: A review focusing on X-ray tomography insights10.1016/j.matdes.2019.108385 ↗
40. Charpy impact testing of metallic selective laser melting parts10.1080/17452751003703894 ↗
41. Hernández, D.G. (2014). Mechanical Behaviour Assessment of the Ti6Al4V Alloy Obtained by Additive Manufacturing towards Aeronautical Industry. [Master’s Thesis, Instituto Superior Técnico (IST)].
42. Effect of Heat Treatment on Microstructure and Impact Toughness of Ti-6Al-4V Manufactured by Selective Laser Melting Process10.1515/amm-2017-0205 ↗
43. Variation of Impact Toughness of As-Built Dmls Ti6al4v (Eli) Specimens with Temperature
44. Anisotropy in the impact toughness of selective laser melted Ti–6Al–4V alloy10.1016/j.msea.2015.10.045 ↗
45. Kazachenok, M., Panin, A., Panin, S., and Vlasov, I. (2019, January 1–5). Impact toughness of Ti–6Al–4V parts fabricated by additive manufacturing. Proceedings of the International Conference on Advanced Materials with Hierarchical Structure for New Technologies and Reliable Structures 2019, Tomsk, Russia.10.1063/1.5132020 ↗
46. Effects of nanofeatures induced by severe shot peening (SSP) on mechanical, corrosion and cytocompatibility properties of magnesium alloy AZ3110.1016/j.actbio.2017.11.032 ↗
47. Effect of surface mechanical attrition treatment on corrosion fatigue behavior of AZ31B magnesium alloy10.1016/j.ijfatigue.2019.06.031 ↗
48. Effect of micro shot peening on the mechanical properties and corrosion behavior of two microstructure Ti–6Al–4V alloy10.1016/j.apsusc.2015.12.019 ↗
49. Yu, Z., Chen, Z., Qu, D., Qu, S., Wang, H., Zhao, F., Zhang, C., Feng, A., and Chen, D. (2022). Microstructure and Electrochemical Behavior of a 3D-Printed Ti-6Al-4V Alloy. Materials, 15.10.3390/ma15134473 ↗
50. Szklarska-Smialowska, Z. (2005). Pitting and Crevice Corrosion, NACE International.
51. Corrosion properties of S-phase layers formed on medical grade austenitic stainless steel10.1007/s10856-011-4516-z ↗
52. Influence of plasma-nitriding and surface roughness on the wear and corrosion resistance of thin films (PVD/PECVD)10.1016/j.surfcoat.2008.05.022 ↗
53. The effect of coating architecture and defects on the corrosion behaviour of a PVD multilayer Inconel 625/Cr coating10.1016/j.surfcoat.2017.06.009 ↗
54. Vilhena, L.M., Shumayal, A., Ramalho, A., and Ferreira, J.A.M. (2020). Tribocorrosion Behaviour of Ti6Al4V Produced by Selective Laser Melting for Dental Implants. Lubricants, 8.10.3390/lubricants8020022 ↗
55. Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy10.1016/j.jmatprotec.2018.11.008 ↗
56. Effects of load and sliding speed on the tribological behaviour of Ti6Al4V plasma nitrided different temperatures10.1016/S0043-1648(96)07419-4 ↗
57. Electrochemical and materials aspects of tribocorrosion systems10.1088/0022-3727/39/15/S01 ↗
58. Tribocorrosion Behaviour of Ti–6Al–4V Alloy in Biomedical Implants: Effects of Applied Load and Surface Roughness on Material Degradation10.1007/s40735-019-0277-x ↗
59. The corrosion–wear response of Cr–Ti coatings10.1016/j.wear.2006.12.058 ↗
60. Effect of interface roughness on the tribo-corrosion behavior of diamond like carbon coatings on titanium alloy10.1116/6.0001657 ↗
61. Effect of Substrate Surface Roughness on Microstructure and Mechanical Properties of Cold-Sprayed Ti6Al4V Coatings on Ti6Al4V Substrates10.1007/s11666-019-00926-5 ↗
62. Metallurgical and Mechanical Aspects of the Sea-Water Stress Corrosion of Titanium
63. Designed Ti/TiN sub-layers suppressing the crack and erosion of TiAlN coatings10.1016/j.surfcoat.2022.128419 ↗
64. Corrosion and tribocorrosion behavior of Ti/TiN PVD coating on 316L stainless steel substrate in Ringer’s solution10.1016/j.matchemphys.2014.08.025 ↗