journal article·2019-12-18Open access

Dictating Pt-Based Electrocatalyst Performance in Polymer Electrolyte Fuel Cells, from Formulation to Application

Tim Van Cleve, Sunilkumar Khandavalli, Anamika Chowdhury, Samantha Medina, Svitlana Pylypenko, Min Wang, Karren L. More, Nancy Kariuki, Deborah J. Myers, Adam Z. Weber, Scott A. Mauger, Michael Ulsh, K. C. Neyerlin

ACS Applied Materials & Interfaces· Volume 11· Issue 50

Abstract

In situ electrochemical diagnostics designed to probe ionomer interactions with platinum and carbon were applied to relate ionomer coverage and conformation, gleaned from anion adsorption data, with O2 transport resistance for low-loaded (0.05 mgPt cm–2) platinum-supported Vulcan carbon (Pt/Vu)-based electrodes in a polymer electrolyte fuel cell. Coupling the in situ diagnostic data with ex situ characterization of catalyst inks and electrode structures, the effect of ink composition is explained by both ink-level interactions that dictate the electrode microstructure during fabrication and the resulting local ionomer distribution near catalyst sites. Electrochemical techniques (CO displacement and ac impedance) show that catalyst inks with higher water content increase ionomer (sulfonate) interactions with Pt sites without significantly affecting ionomer coverage on the carbon support. Surprisingly, the higher anion adsorption is shown to have a minor impact on specific activity, while exhibiting a complex relationship with oxygen transport. Ex situ characterization of ionomer suspensions and catalyst/ionomer inks indicates that the lower ionomer coverage can be correlated with the formation of large ionomer aggregates and weaker ionomer/catalyst interactions in low-water content inks. These larger ionomer aggregates resulted in increased local oxygen transport resistance, namely, through the ionomer film, and reduced performance at high current density. In the water-rich inks, the ionomer aggregate size decreases, while stronger ionomer/Pt interactions are observed. The reduced ionomer aggregation improves transport resistance through the ionomer film, while the increased adsorption leads to the emergence of resistance at the ionomer/Pt interface. Overall, the high current density performance is shown to be a nonmonotonic function of ink water content, scaling with the local gas (H2, O2) transport resistance resulting from pore, thin film, and interfacial phenomena.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Chemistry and Nanoscience Center, National Renewable Energy Laboratory, Golden, Colorado 80401, United States

Energy Conversion Group, Energy Technologies Area, Lawrence Berkeley National Laboratory, Berkeley, California 94720, United States

Department of Chemical and Biomolecular Engineering, University of California, Berkeley, California 94720, United States

Colorado School of Mines, Golden, Colorado 80401, United States

Oak Ridge National Laboratory, Oak Ridge, Tennessee 37830, United States

Argonne National Laboratory, Lemont, Illinois 60439, United States

Funding

Fuel Cell Technologies Office · Office of Science

References (79)

Show source-provided references
1. Borup R. · 2017
2. Borup R. · 201810.2172/1505949 ↗
3. Fuel Cell Multi-Year Research, Development and Demonstration Plan, 2012.
4. 10.1021/acs.jpclett.6b0021610.1021/acs.jpclett.6b00216 ↗
5. 10.1016/j.jpowsour.2003.12.05510.1016/j.jpowsour.2003.12.055 ↗
6. 10.1016/s0378-7753(01)01045-x10.1016/s0378-7753(01)01045-x ↗
7. 10.1016/s0378-7753(02)00542-610.1016/s0378-7753(02)00542-6 ↗
8. 10.1021/acsomega.7b0005410.1021/acsomega.7b00054 ↗
9. 10.1126/science.124906110.1126/science.1249061 ↗
10. 10.1021/acs.nanolett.8b0097810.1021/acs.nanolett.8b00978 ↗
11. 10.1021/acsenergylett.8b0018610.1021/acsenergylett.8b00186 ↗
12. 10.1016/j.nanoen.2016.04.00810.1016/j.nanoen.2016.04.008 ↗
13. 10.1002/aenm.20170125710.1002/aenm.201701257 ↗
14. 10.1149/2.008308jes10.1149/2.008308jes ↗
15. 10.1016/s0378-7753(01)01030-810.1016/s0378-7753(01)01030-8 ↗
16. 10.1021/acsaem.9b0103710.1021/acsaem.9b01037 ↗
17. Kocha S. · 2014
18. Ulsh M. · 2019
19. 10.1149/1.370196810.1149/1.3701968 ↗
20. Debe M. K. · 2010
21. Kabir S. · Meet. Abstr. · 2018 · 2018 · 174310.1149/MA2018-01/30/1743 ↗
22. 10.1021/acsami.9b1136510.1021/acsami.9b11365 ↗
23. 10.1149/2.040308jes10.1149/2.040308jes ↗
24. 10.1021/acscatal.7b0357110.1021/acscatal.7b03571 ↗
25. 10.1002/adfm.20160086110.1002/adfm.201600861 ↗
26. 10.1002/celc.20150013110.1002/celc.201500131 ↗
27. 10.1016/j.jpowsour.2016.02.09110.1016/j.jpowsour.2016.02.091 ↗
28. 10.1149/2.0571414jes10.1149/2.0571414jes ↗
29. 10.1021/ma300212f10.1021/ma300212f ↗
30. 10.1016/j.electacta.2016.04.02310.1016/j.electacta.2016.04.023 ↗
31. 10.1149/1.314396510.1149/1.3143965 ↗
32. 10.1149/2.0381702jes10.1149/2.0381702jes ↗
33. 10.1016/j.jpowsour.2016.05.03510.1016/j.jpowsour.2016.05.035 ↗
34. 10.1149/2.1251814jes10.1149/2.1251814jes ↗
35. 10.1038/ncomms622910.1038/ncomms6229 ↗
36. 10.1149/06917.0455ecst10.1149/06917.0455ecst ↗
37. 10.1149/2.0301813jes10.1149/2.0301813jes ↗
38. 10.1149/2.0301813jes10.1149/2.0301813jes ↗
39. 10.1002/cphc.20100019010.1002/cphc.201000190 ↗
40. 10.1149/2.0551512jes10.1149/2.0551512jes ↗
41. 10.1021/jp103413510.1021/jp1034135 ↗
42. 10.1016/j.electacta.2016.04.02310.1016/j.electacta.2016.04.023 ↗
43. 10.1149/2.0031907jes10.1149/2.0031907jes ↗
44. 10.1021/acsami.8b1503910.1021/acsami.8b15039 ↗
45. 10.1021/acs.jpcb.8b0649310.1021/acs.jpcb.8b06493 ↗
46. 10.1149/1.188836710.1149/1.1888367 ↗
47. 10.1149/1.315222610.1149/1.3152226 ↗
48. Zhang, J.; Paine, L.; Nayar, A.; Makharia, R. Methods and Processes to Recover Voltage Loss of PEM Fuel Cell Stack. U.S. Patent 0,195,324 A1, August 11, 2011.
49. 10.1149/2.063207jes10.1149/2.063207jes ↗
50. 10.1016/j.ijhydene.2017.01.03610.1016/j.ijhydene.2017.01.036 ↗
51. 10.1149/2.0031907jes10.1149/2.0031907jes ↗
52. 10.1107/s002188980900880210.1107/s0021889809008802 ↗
53. 10.1107/s002188981200403710.1107/s0021889812004037 ↗
54. 10.1107/s002188980900222210.1107/s0021889809002222 ↗
55. 10.1016/0956-7151(91)90062-610.1016/0956-7151(91)90062-6 ↗
56. 10.1098/rsta.2010.017510.1098/rsta.2010.0175 ↗
57. Hunter, R. J. Zeta Potential in Colloid Science; Academic Press, 1981; pp 59–124.10.1016/B978-0-12-361961-7.50007-9 ↗
58. 10.1021/acs.chemrev.6b0015910.1021/acs.chemrev.6b00159 ↗
59. 10.1021/acs.jpcc.5b0415510.1021/acs.jpcc.5b04155 ↗
60. 10.1016/j.jpowsour.2008.12.14110.1016/j.jpowsour.2008.12.141 ↗
61. 10.1021/ma301289v10.1021/ma301289v ↗
62. 10.1021/jp410510x10.1021/jp410510x ↗
63. 10.1149/2.0082001jes10.1149/2.0082001jes ↗
64. Israelachvili J. N. · 2011
65. 10.1063/1.132176710.1063/1.1321767 ↗
66. Derjaguin B. · Acta Physicochem. URSS · 1941 · 14 · 633
67. Verwey, E. J. W.; Overbeek, J. T. G. Theory of the Stability of Lyophobic Colloids: The Interaction of Sol Particles Having an Electric Double Layer; Elsevier: Amsterdam, 1948; pp 135–182.
68. 10.1021/am900600y10.1021/am900600y ↗
69. Mewis, J.; Wagner, N. Colloidal Suspension Rheology; Cambridge University Press: NY, 2012; pp 157–179.10.1017/CBO9780511977978 ↗
70. 10.1149/1.183764610.1149/1.1837646 ↗
71. 10.1007/s12678-013-0159-910.1007/s12678-013-0159-9 ↗
72. 10.1149/2.0401414jes10.1149/2.0401414jes ↗
73. 10.1149/2.0401414jes10.1149/2.0401414jes ↗
74. 10.1149/2.072308jes10.1149/2.072308jes ↗
75. 10.1149/2.061212jes10.1149/2.061212jes ↗
76. 10.1021/nl501233g10.1021/nl501233g ↗
77. 10.1016/j.jelechem.2013.01.02610.1016/j.jelechem.2013.01.026 ↗
78. 10.1016/j.jelechem.2013.09.01110.1016/j.jelechem.2013.09.011 ↗
79. 10.1149/08008.0321ecst10.1149/08008.0321ecst ↗