Fatigue Property and Small Crack Propagation Mechanism of MIG Welding Joint of 6005A-T6 Aluminum Alloy
Source abstract
Abstract
In this study, metal inert gas welding (MIG) was applied to 4 mm thick 6005A-T6 aluminum alloy welding. Compared with other parts, the hardness of the weld zone (WZ) was the lowest, about 67 HV. There was the Softening in WZ, which might make WZ the weakest zone. Then, fatigue tests were carried out on MIG welded joints. All the fatigue specimens fractured at the weld toe of the lap joint, and the fracture was characterized by a cleavage fracture. Crack closure induced by oxide was observed during the steady propagation of the fatigue crack. Impurities hindered crack propagation, changed the direction of crack propagation, and appeared in stepped fatigue strip distribution morphology; in the process of the main crack propagation, the initiation and propagation of small cracks were easily restricted and hindered by the main crack, which slowed down the propagation rate and even stopped the propagation directly.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Engineering, Shanghai University of Engineering Science, Shanghai 201620, China
Shanghai Laser Intelligent Manufacturing and Quality Inspection Professional Technical Service Platform, Shanghai 201620, China
Funding
the National Natural Science Foundation of China · the Shanghai Natural Science Foundation of China
References (27)
Show source-provided references
1. Microstructure, local and global mechanical properties of friction stir welds in aluminium alloy 6005A-T610.1016/j.msea.2007.08.041 ↗
2. Fatigue behaviour of friction stir welds without neither welding flash nor flaw in several aluminium alloys10.1016/j.ijfatigue.2009.06.015 ↗
3. Mechanisms of fatigue crack initiation and propagation in 6005A CMT welded joint10.1016/j.jallcom.2017.12.374 ↗
4. Low cycle fatigue behavior of aluminium 6063 alloy under the cyclic frequency of 0.2 Hz10.1016/j.matpr.2019.09.133 ↗
5. Fatigue crack nucleation and small crack growth in an extruded 6061 aluminum alloy10.1016/j.ijfatigue.2018.09.023 ↗
6. Experimental investigation and fatigue life prediction for 7475-T7351 aluminum alloy with and without shot peening-induced residual stresses10.1016/j.actamat.2011.03.013 ↗
7. Propagation of short fatigue cracks in permanent and semi-solid mold 357 aluminum alloy10.1016/j.ijfatigue.2011.08.009 ↗
8. Microstructure characterization and mechanism of fatigue crack propagation of 6082 aluminum alloy joints10.1016/j.matchemphys.2020.123734 ↗
9. Formation and fatigue property of MIG welded high-speed train 6005A-T6 aluminum alloy10.1088/2053-1591/ab047b ↗
10. Atom probe analysis of early-stage strengthening behaviour in an Al–Mg–Si–Cu alloy10.1016/j.ultramic.2010.11.009 ↗
11. Fatigue properties of continuous wave and pulsed wave laser cold-wire welding of thick section AA6005-T6 aluminum alloys10.1016/j.ijfatigue.2021.106184 ↗
12. Influence of surface enhanced treatment on microstructure and fatigue performance of 6005A aluminum alloy welded joint10.1016/j.jmapro.2020.10.076 ↗
13. Fatigue crack nucleation and microstructurally small crack growth mechanisms in high strength aluminum alloys10.1016/j.ijfatigue.2020.105790 ↗
14. Crack initiation mechanisms in low cycle fatigue of aluminium alloy 7075 T610.1016/0921-5093(89)90522-4 ↗
15. Fatigue crack surface crystallography near crack initiating particle clusters in precipitation hardened legacy and modern Al–Zn–Mg–Cu alloys10.1016/j.ijfatigue.2011.01.018 ↗
16. Influence of reversible and non-reversible fatigue on the microstructure and mechanical property evolution of 7075-T6 aluminum alloy10.1016/j.ijfatigue.2020.106094 ↗
17. Initiation of fatigue cracks in commercial aluminium alloys and the subsequent propagation of very short cracks10.1016/0013-7944(75)90004-1 ↗
18. The growth of small fatigue cracks in 7075–T6 aluminum10.1111/j.1460-2695.1982.tb01251.x ↗
19. Microstructure characterization and mechanism of fatigue crack initiation near pores for 6005A CMT welded joint10.1016/j.msea.2017.09.029 ↗
20. Effects of welding speed on the microstructure and hardness in friction stir welding joints of 6005A-T6 aluminum alloy10.1016/j.matdes.2012.09.040 ↗
21. Effect of aging state on corrosion fatigue properties of 7075 aluminum alloy10.1016/j.ijfatigue.2022.106916 ↗
22. Microstructure and stress corrosion behaviour of CMT welded AA6061 T-6 aluminium alloy joints10.1016/j.jmrt.2021.08.005 ↗
23. Comparison of small and long fatigue crack growth behavior in AA 7050-T745110.1016/j.engfracmech.2018.09.009 ↗
24. Fine equiaxed zone induced softening and failure behavior of 7050 aluminum alloy hybrid laser welds10.1016/j.msea.2021.141597 ↗
25. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
26. In-situ SEM study of fatigue micro-crack initiation and propagation behavior in pre-corroded AA7075-T765110.1016/j.ijfatigue.2020.105655 ↗
27. Investigation on laser beam remelted Al–Cu–Li alloy part I: Segregation and aging behavior at grain and dendrite boundaries10.1016/j.jallcom.2020.157519 ↗