Durability and Self-Sealing Examination of Concretes Modified with Crystalline Waterproofing Admixtures
Source abstract
Abstract
Repairing concrete structures costs billions of dollars every year all around the globe. For overcoming durability concerns and creating enduring economical structures, chemical admixtures, as a unique solution, have recently attracted a lot of interest. As permeability of a concrete structure is considered to play a significant role in its durability, Permeability Reducing Admixtures (PRA) is one of the ideal solutions for protecting structures exposed to water and waterborne chemicals. Different products have been developed to protect concrete structures against water penetration, which, based on their chemistry, performance, and functionality, have been categorized into PRA. As it has previously been tested by authors and proven to be a promising solution, a hydrophilic Crystalline Waterproofing Admixtures (CWA) has been considered for this study. This paper aims to investigate how this product affects concrete’s overall freeze–thaw resistance, self-sealing, and corrosion resistance. Various testing methods have been utilized to examine the performance of CWA mixtures, including the linear polarization resistance, resonance frequency testing, half-cell potential, and self-sealing test. The reinforcement corrosion potential and rate measurements indicated superior performance for CWA-treated samples. After being exposed to 300 freeze–thaw cycles, concrete mixes containing CWA—even non-air-entrained ones—showed a Durability Factor (DF) of more than 80% with no signs of failure, while non-air-entrained control samples indicated the lowest DF (below 60%) but the greatest mass loss. The major causes are a reduction in solution permeability and lack of water availability in the concrete matrix—due to the presence of CWA crystals. Furthermore, evidence from the self-sealing test suggests that CWA-treated specimens can seal wider cracks and at a faster rate.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Concrete Corrosion and Durability · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Civil Engineering, Facility for Innovative Materials and Infrastructure Monitoring (FIMIM), University of Victoria, 3800 Finnerty Rd., Victoria, BC V8W 3R4, Canada
Kryton International Inc., 1645 East Kent Ave N, Vancouver, BC V5P 2S8, Canada
References (68)
Show source-provided references
1. Effect of a crystalline admixture on the self-healing capability of high-performance fiber reinforced concretes in service conditions10.1016/j.conbuildmat.2018.04.003 ↗
2. Perkins, P.H. (1997). Repair, Protection and Waterproofing of Concrete Structures, E. & F.N. Spon. [3rd ed.].10.4324/9780203475720 ↗
3. Goguen, C. (2021, July 10). 5 Rules of Watertightness. Available online: https://precast.org/2012/11/5-rules-of-watertightness/.
4. ACI Committee 212 (2016). Report on Chemical Admixtures for Concrete, American Concrete Institute (ACI).
5. García Calvo, J.L., Sánchez Moreno, M., Carballosa, P., Pedrosa, F., and Tavares, F. (2019). Improvement of the Concrete Permeability by Using Hydrophilic Blended Additive. Materials, 12.10.3390/ma12152384 ↗
6. Crystalline Admixtures and Their Effect on Selected Properties of Concrete10.14311/AP.2016.56.0306 ↗
7. Use of Secondary Crystallization and Fly Ash in Waterproofing Materials to Increase Concrete Resistance to Aggressive Gases and Liquids10.1155/2019/7530325 ↗
8. Durability of Cement Based Mortars Containing Crystalline Additives10.4028/www.scientific.net/DDF.382.246 ↗
9. Effect of Humidity on the Properties of Cement Mortars with a Crystalline Additive10.4028/www.scientific.net/SSP.276.53 ↗
10. Mortars with crystalline additive in aggressive environments10.1088/1757-899X/385/1/012066 ↗
11. Influence of a Crystalline Additive on the Porosity of Cement Mortars10.4028/www.scientific.net/DDF.382.254 ↗
12. Performance of crystalline forming additive materials in concrete10.1016/j.conbuildmat.2019.117056 ↗
13. Assessment of self-healing and durability parameters of concretes incorporating crystalline admixtures and Portland Limestone Cement10.1016/j.cemconcomp.2019.02.017 ↗
14. Azarsa, P. (2018). Multi-Scale Investigation and Resistivity-Based Durability Modeling of EShC Containing Crystalline Admixtures. [Ph.D. Thesis, University of Victoria].
15. Azarsa, P., Gupta, R., and Biparva, A. (2020). Inventive Microstructural and Durability Investigation of Cementitious Composites Involving Crystalline Waterproofing Admixtures and Portland Limestone Cement. Materials, 13.10.3390/ma13061425 ↗
16. Specimen preparation for nano-scale investigation of cementitious repair material10.1016/j.micron.2018.01.007 ↗
17. Electrical Resistivity of Concrete for Durability Evaluation: A Review10.1155/2017/8453095 ↗
18. Azarsa, P., Gupta, R., and Biparva, A. (2018, January 25–27). Crystalline Waterproofing Admixtures Effects on Self-healing and Permeability of Concrete. Proceedings of the International Conference on New Horizons in Green Civil Engineering, Victoria, BC, Canada.
19. ACI 318 (2019). Building Code Requirements for Structural Concrete, American Concrete Institute (ACI).
20. Abro, F.u.R., Buller, A.S., Lee, K.-M., and Jang, S.Y. (2019). Using the Steady-State Chloride Migration Test to Evaluate the Self-Healing Capacity of Cracked Mortars Containing Crystalline, Expansive, and Swelling Admixtures. Materials, 12.10.3390/ma12111865 ↗
21. Self-Crack Closing Ability of Mortar with Different Additives
22. Jaroenratanapirom, D., and Sahamitmongkol, R. (2010, January 20–22). Effects of Different Mineral Additives and Cracking Ages on Self-Healing Performance of Mortar. Proceedings of the 6th Annual Concrete Conference, Phetchaburi, Thailand.
23. Self-healing of surface cracks in mortars with expansive additive and crystalline additive10.1016/j.cemconcomp.2012.01.005 ↗
24. Effect of exposure conditions on self healing behavior of strain hardening cementitious composites incorporating various cementitious materials10.1016/j.conbuildmat.2013.01.012 ↗
25. A “fracture testing” based approach to assess crack healing of concrete with and without crystalline admixtures10.1016/j.conbuildmat.2014.07.008 ↗
26. Self-healing capability of concrete with crystalline admixtures in different environments10.1016/j.conbuildmat.2015.03.091 ↗
27. Effect of crystalline admixtures on the self-healing capability of early-age concrete studied by means of permeability and crack closing tests10.1016/j.conbuildmat.2016.03.196 ↗
28. On the use of crystalline admixtures in cement based construction materials: From porosity reducers to promoters of self healing10.1088/0964-1726/25/8/084002 ↗
29. A methodology to assess crack-sealing effectiveness of crystalline admixtures under repeated cracking-healing cycles10.1016/j.conbuildmat.2018.05.261 ↗
30. Synergetic effect of superabsorbent polymer (SAP) and crystalline admixture (CA) on mortar macro-crack healing10.1016/j.conbuildmat.2020.118521 ↗
31. Robertson, I. (2014). Performance of Corrosion Inhibiting Admixtures in a Marine Environment. Construction Materials and Structures, IOS Press.
32. Innovative Test Technique to Evaluate “Self-Sealing” of Concrete10.1520/JTE20130285 ↗
33. Do crystalline water proofing admixtures affect restrained plastic shrinkage behavior of concrete?10.21041/ra.v7i1.172 ↗
34. ASTM C876 (2015). Test Method for Corrosion Potentials of Uncoated Reinforcing Steel in Concrete, ASTM International.
35. ASTM G109 (2013). Standard Test Method for Determining Effects of Chemical Admixtures on Corrosion of Embedded Steel Reinforcement in Concrete Exposed to Chloride Environments, ASTM International.
36. ASTM C666 (2015). Test Method for Resistance of Concrete to Rapid Freezing and Thawing, ASTM International.
37. ASTM C215 (2019). Test Method for Fundamental Transverse, Longitudinal, and Torsional Resonant Frequencies of Concrete Specimens, ASTM International.
38. 38. CSA Standard A23.1. (2019). Concrete Materials and Methods of Concrete Construction/Test Methods and Standard Practices for Concrete, CSA Group.
39. ASTM C150 (2019). Standard Specification for Portland Cement, ASTM International.
40. 40. CSA A23.1-14. (2014). Standard for Concrete Materials and Methods of Concrete Construction, Canadian Standard Association.
41. ASTM C33/C33M-18 (2018). Standard Specification for Concrete Aggregates, ASTM International.
42. ASTM C127-15 (2015). Standard Test Method for Relative Density (Specific Gravity) and Absorption of Coarse Aggregate, ASTM International.
43. ASTM C192/C192M-15 (2015). Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory, ASTM International.
44. ASTM C39 (2020). Test Method for Compressive Strength of Cylindrical Concrete Specimens, ASTM International.
45. ASTM C143 (2020). Test Method for Slump of Hydraulic-Cement Concrete, ASTM International.
46. ASTM C231 (2017). Test Method for Air Content of Freshly Mixed Concrete by the Pressure Method, ASTM International.
47. Trejo, D., Halmen, C., and Reinschmidt, K. (2008). Corrosion Performance Tests for Reinforcing Steel in Concrete, Texas Department of Transportation and the U.S. Department of Transportation, Federal Highway Administration.
48. ASTM G59 (2014). Standard Test Method for Conducting Potentiodynamic Polarization Resistance Measurements, ASTM International.
49. ASTM G102 (2015). Standard Practice for Calculation of Corrosion Rates and Related Information from Electrochemical Measurements, ASTM International.
50. Song, H.H., and Yalagandula, P. (2007, January 7–12). Real-time End-to-end Network Monitoring in Large Distributed Systems. Proceedings of the 2007 2nd International Conference on Communication Systems Software and Middleware, Bangalore, India.10.1109/COMSWA.2007.382612 ↗
51. A comparative study of corrosion resistance of different coatings for mortar–embedded steel plates10.1016/j.conbuildmat.2014.01.059 ↗
52. Electrochemical Polarization10.1149/1.2428496 ↗
53. Test methods for on-site corrosion rate measurement of steel reinforcement in concrete by means of the polarization resistance method10.1007/BF02483292 ↗
54. Corrosion of reinforcing steel evaluated by means of concrete resistivity measurements10.1016/S0010-938X(01)00033-6 ↗
55. Environmental influences on linear polarisation corrosion rate measurement in reinforced concrete10.1016/S0963-8695(01)00008-1 ↗
56. ASTM C805 (2018). Test Method for Rebound Number of Hardened Concrete, ASTM International.
57. Biparva, A., Gupta, R., and Gavrilovic, S. (2011, January 12). Self-Sealing Concrete: Innovative Test Technique and Method of Analysis. Proceedings of the International Conference of Future Concrete, Dubai, United Arab Emirates.
58. Accelerated testing of plain and epoxy-coated reinforcement in simulated seawater and chloride solutions10.1016/S0008-8846(01)00487-2 ↗
59. Some Electrochemical Aspects of Corrosion of Steel in Concrete10.5006/1.3582998 ↗
60. Broomfield, J.P. (2019). Corrosion of Steel in Concrete: Understanding, Investigation and Repair, CRC Press. [2nd ed.].
61. Reliability of Rebound Hammer Test in Concrete Compressive Strength Estimation
62. Paine, K.A., Dhir, R.K., Moroney, R., and Kopasakis, K. (2002, January 9–11). Use of crumb rubber to achieve freeze thaw resisting concrete. Proceedings of the International Conference on Concrete for Extreme Conditions, Scotland, UK.10.1680/cfec.31784.0047 ↗
63. An equation for determining freeze-thaw fatigue damage in concrete and a model for predicting the service life10.1016/j.conbuildmat.2017.01.042 ↗
64. Frost resistance of recycled aggregate concrete10.1016/j.cemconres.2004.02.025 ↗
65. Rasband, W. (2018). ImageJ Software, National Institutes of Health.
66. Influence of Defects on Reinforced Concrete Fracture Performance in Improved Wedge Splitting Tests10.1520/JTE20170176 ↗
67. Influence of crack propagation on electrical resistivity and ultrasonic characteristics of normal concrete assessed by sequential TPB fracture test
68. Effects of coral, recycled and natural coarse aggregates on the mechanical properties of concrete10.1016/j.conbuildmat.2018.10.111 ↗