Optimization of CMT Characteristic Parameters for Swing Arc Additive Manufacturing of AZ91 Magnesium Alloy Based on Process Stability Analysis
Source abstract
Abstract
The droplet transfer behavior and stability of the swing arc additive manufacturing process of AZ91 magnesium alloy based on the cold metal transfer (CMT) technique were studied by analyzing the electrical waveforms and high-speed droplet images as well as the forces on the droplet, and the Vilarinho regularity index for short-circuit transfer (IVSC) based on variation coefficients was used to characterize the stability of the swing arc deposition process. The effect of the CMT characteristic parameters on the process stability was investigated; then, the optimization of the CMT characteristic parameters was realized based on the process stability analysis. The results show that the arc shape changed during the swing arc deposition process; thus, a horizontal component of the arc force was generated, which significantly affected the stability of the droplet transition. The burn phase current I_sc_wait presented a linear function relation with IVSC, while the other three characteristic parameters, i.e., boost phase current I_boost, boost phase duration t_I_boost and short-circuiting current I_sc2, all had a quadratic correlation with IVSC. A relation model of the CMT characteristic parameters and IVSC was established based on the rotatable 3D central composite design; then, the optimization of the CMT characteristic parameters was realized using a multiple-response desirability function approach.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, Tianjin 300354, China
School of Materials Science and Engineering, Tianjin University, Tianjin 300354, China
International Institute for Innovative Design and Intelligent Manufacturing of Tianjin University, Shaoxing 312000, China
Beijing Hangxing Machinery Co., Ltd., Beijing 100013, China
Funding
National Natural Science Foundation of China
References (36)
Show source-provided references
1. Transient liquid phase bonding of AZ31 magnesium alloy: Metallurgical structure and mechanical properties10.1016/j.jmapro.2018.08.002 ↗
2. Improving microstructural and tensile properties of AZ31B magnesium alloy joints by stationary shoulder friction stir welding10.1016/j.jmapro.2018.11.014 ↗
3. Properties of CO2 laser-welded butt joints of dissimilar magnesium alloys10.1016/j.jmatprotec.2008.03.072 ↗
4. TIG and laser-TIG hybrid filler wire welding of casting and wrought dissimilar magnesium alloy10.1016/j.jmapro.2018.06.005 ↗
5. The arc characteristics of cold metal transfer welding with AZ31 magnesium alloy wire10.1016/j.jmapro.2016.10.001 ↗
6. Exploring the concept of castability in magnesium die-casting alloys10.1016/j.jma.2020.05.008 ↗
7. Residual stress in wire and arc additively manufactured aluminum components10.1016/j.jmapro.2021.02.021 ↗
8. Wire arc additive manufacturing for repairing aluminium structures in marine applications10.1016/j.matlet.2021.130112 ↗
9. Wire arc additive manufacturing of Inconel 718: Constitutive modelling and its microstructure basis10.1016/j.jmapro.2022.01.067 ↗
10. Effect of crack-like defects on the fracture behaviour of wire + arc additively manufactured nickel-base alloy 718
11. The microstructure and mechanical properties of duplex stainless steel components fabricated via flux-cored wire arc-additive manufacturing10.1016/j.jmapro.2021.07.045 ↗
12. Hot cracking in tungsten inert gas welding of magnesium alloy AZ91D10.1179/174328407X213026 ↗
13. Wire-arc additive manufacturing of AZ31 magnesium alloy fabricated by cold metal transfer heat source: Processing, microstructure, and mechanical behavior10.1016/j.jmatprotec.2020.116895 ↗
14. Influence of calcium fluoride on underwater wet welding process stability10.1007/s40194-018-0642-2 ↗
15. Methods for the determination of arc stability10.1016/S0924-0136(03)00416-3 ↗
16. Current waveform effects on CMT welding of mild steel10.1016/j.jmatprotec.2017.01.004 ↗
17. Lap weld-brazing of aluminium to steel using novel cold metal transfer process10.1016/j.jmatprotec.2020.116728 ↗
18. Modified active control of metal transfer and pulsed GMAW of titanium
19. Effect of current waveform on droplet oscillation in GMAW
20. Grain refining of magnesium welds by arc oscillation10.1016/j.actamat.2016.06.036 ↗
21. Comparison between weave bead welding and multi-layer multi-pass welding for thick plate Invar steel10.1007/s00170-016-8926-4 ↗
22. Effect of swing arc on molten pool behaviors in narrow-gap GMAW of 5083 Al-alloy10.1016/j.jmatprotec.2018.04.026 ↗
23. Preliminary investigation of building strategies of maraging steel bulk material using wire+arc additive manufacture10.1007/s11665-018-3521-5 ↗
24. Control system for reducing weld spatter during the welding process by using high-speed visual sensing
25. Study on metal transfer modes and welding spatter characteristics of self-shielded flux cored wire10.1179/174329308X380354 ↗
26. The importance of spatter formed in shielded metal arc welding10.1016/j.matchar.2006.09.011 ↗
27. Microstructure and mechanical properties of AZ91 Mg alloy fabricated by cold metal transfer additive manufacturing10.1016/j.matlet.2020.128185 ↗
28. Microstructure and mechanical properties of AZ91 magnesium alloy fabricated by multi-layer and multi-pass CMT based WAAM technique10.1016/j.rineng.2023.101065 ↗
29. Metal transfer behaviour of CMT-based step-over deposition in fabricating slant features10.1016/j.jmapro.2021.09.027 ↗
30. Arc force and shapes with high-frequency pulsed-arc welding10.1080/13621718.2016.1277625 ↗
31. Research on short circuiting transfer mode of ultrasonic assisted GMAW method10.1179/1362171811Y.0000000058 ↗
32. Analysis of metal transfer in gas metal arc welding
33. The effect of metal transfer stability (spattering) on fume generation, morphology and composition in short-circuit MAG welding10.1016/j.jmatprotec.2014.02.012 ↗
34. Stability analysis of the cold metal transfer (CMT) brazing process for galvanized steel plates with ZnAl4 filler metal10.1007/s00170-019-03702-5 ↗
35. Welding current influences on Inconel 625/X65 cladding interface10.1080/10426914.2017.1364851 ↗
36. Shanmugam, R., Ramoni, M., Thangamani, G., and Thangaraj, M. (2021). Influence of additive manufactured stainless steel tool electrode on machinability of beta titanium alloy. Metals, 11.10.3390/met11050778 ↗