Abstract
To achieve laser direct welding of glass and metal without optical contact is hard, owing to the large difference in thermal expansion and thermal conductivity between glass and metal and an insignificant melting area. In this study, the high-power picosecond pulsed laser was selected to successfully weld the aluminosilicate glass/6061 aluminum alloy with a gap of 35 ± 5 μm between glass and metal. The results show that the molten glass and metal diffuse and mix at the interface. No defects such as microcracks or holes are observed in the diffusion mixing zone. Due to the relatively large gap, the glass collapsed after melting and caulking, resulting in an approximately arc-shaped microcrack between modified glass and unmodified glass or weakly modified glass. The shape of the glass modification zone and thermal accumulation are influenced by the single-pulse energy and linear energy density of the picosecond laser during welding, resulting in variations in the number and size of defects and the shape of the glass modification zone. By reasonably tuning the two factors, the shear strength of the joint reaches 15.98 MPa. The diffusion and mixing at the interface and the mechanical interlocking effect of the glass modification zone are the main reasons for achieving a high shear strength of the joint. This study will provide reference and new ideas for the laser transmission welding of glass and metal in the non-optical contact conditions.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Laser Material Processing Techniques · Adhesion, Friction, and Surface Interactions · Ocular and Laser Science Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China
School of Materials Engineering, Shandong Institute of Shipbuilding Technology, Weihai 264209, China
School of Mechanical & Electrical Engineering, Xuzhou University of Technology, Xuzhou 221018, China
CRRC Academy (Qingdao), Qingdao 266109, China
Funding
Natural Science Foundation for Excellent Young Scholars of Shandong Province · Taishan Scholars Foundation of Shandong Province
References (31)
Show source-provided references
1. Robert, E.L., Steven, L., Frankie, M., and Stephen, L. (2020). Ultrafast laser bonding of glasses and crystals to metals for epoxy-free optical instruments. Components and Packaging for Laser Systems VI, SPIE.
2. Quick bonding using a universal adhesive10.1007/s00784-019-03149-8 ↗
3. Li, S., Ma, C., Hou, B., and Liu, H. (2022). Rational design of adhesives for effective underwater bonding. Front. Chem., 10.10.3389/fchem.2022.1007212 ↗
4. The selection and performance of adhesives for a steel–glass connection10.1016/j.ijadhadh.2011.06.001 ↗
5. Research on mechanical clinching process for dissimilar aluminum alloy sheets with inclined surface10.1016/j.jmapro.2023.01.073 ↗
6. Lab-on-a-chip devices: How to close and plug the lab?10.1016/j.mee.2014.10.013 ↗
7. Optimized solder alloy for glass-to-metal joints by simultaneous soldering and anodic bonding10.1016/j.jmatprotec.2016.05.017 ↗
8. Homogenization of the zirconium carbide–titanium interface domain10.1016/j.scriptamat.2015.09.006 ↗
9. Microstructure and fracture behavior of SiO2 glass ceramic and TC4 alloy joint brazed with TiZrNiCu alloy10.1007/s11771-009-0118-z ↗
10. Vacuum brazing of SiO2 glass ceramic and Ti–6Al–4V alloy using AgCuTi filler foil10.1016/j.msea.2008.08.008 ↗
11. Femtosecond laser Bessel beam welding of transparent to non-transparent materials with large focal-position tolerant zone10.1364/OE.26.000917 ↗
12. New application of a new generation femtosecond laser in hyperfine cold processing
13. Space-selective laser joining of dissimilar transparent materials using femtosecond laser pulses10.1063/1.2221393 ↗
14. Picosecond laser welding of similar and dissimilar materials10.1364/AO.53.004233 ↗
15. Direct microwelding of dissimilar glass and Kovar alloy without optical contact using femtosecond laser pulses10.1007/s11771-022-5091-9 ↗
16. Mechanism and optimization of femtosecond laser welding fused silica and aluminum10.1016/j.apsusc.2023.158327 ↗
17. Direct joining of quartz glass and copper by nanosecond laser10.1016/j.ceramint.2023.08.285 ↗
18. Welding of Transparent Materials Using Femtosecond Laser Pulses10.1143/JJAP.44.L687 ↗
19. Avoiding the requirement for pre-existing optical contact during picosecond laser glass-to-glass welding10.1364/OE.23.018645 ↗
20. Toward laser welding of glasses without optical contacting10.1007/s00339-015-9377-8 ↗
21. Towards industrial ultrafast laser microwelding: SiO2 and BK7 to aluminum alloy10.1364/AO.56.004873 ↗
22. Welding of Glass and Copper with a Rough Surface using Femtosecond Fiber Laser Pulses10.2961/jlmn.2018.01.0005 ↗
23. Direct welding of glass and metal by 1 kHz femtosecond laser pulses10.1364/AO.54.008957 ↗
24. Fermann, M.E., Galvanauskas, A., and Sucha, G. (2002). Ultrafast Lasers Technology and Applications, CRC Press.10.1201/9780203910207 ↗
25. Recent developments in compact ultrafast lasers10.1038/nature01938 ↗
26. Fabrication of a leaf-like superhydrophobic CuO coating on 6061Al with good self-cleaning, mechanical and chemical stability10.1016/j.ceramint.2020.03.013 ↗
27. Effect of laser textured patterns on the interfacial characteristics and mechanical properties of 6061Al/GFRTP joints via hot-pressing10.1016/j.tws.2023.110916 ↗
28. Ultrafast Laser Enabling Hierarchical Structures for Versatile Superhydrophobicity with Enhanced Cassie–Baxter Stability and Durability10.1021/acs.langmuir.9b02986 ↗
29. Investigation of metal mixing in laser keyhole welding of dissimilar metals10.1016/j.matdes.2020.109056 ↗
30. Phase separation in an ionomer glass: Insight from calorimetry and phase transitions10.1016/j.jnoncrysol.2015.02.012 ↗
31. A new sealing technology for ultra-thin glass to aluminum alloy by laser transmission welding method10.1007/s00170-021-07226-9 ↗