journal article·2025-02-05Open access

A Comparison Between the Residual Stresses of Ti6Al4V and Ti-6Al-2Sn-4Zr-6Mo Processed by Laser Powder Bed Fusion

Alberta Aversa, Alessandro Carrozza, Vincenza Mercurio, Flaviana Calignano, Olha Sereda, Vaclav Pejchal, Mariangela Lombardi

Materials· Volume 18· Issue 3

Abstract

Metal additive manufacturing processes induce residual stress in as-built components. These residual stresses are detrimental to part quality as they can induce defects such as warping and delamination. In some cases, when complex components are built, residual stress can even cause a build job to fail due to the recoater crashing into the distorted part. In this paper, the residual stress values of Ti6Al4V and Ti-6Al-2Sn-4Zr-6Mo alloys were evaluated by the cantilever approach and by the X-ray diffraction sin2(Ψ) method. The results showed that, as expected, Ti6Al4V as-built cantilevers displayed high distortion and von Mises equivalent stress values up to 494 MPa. On the contrary, as-built Ti-6Al-2Sn-4Zr-6Mo cantilevers were characterized by almost null warping and a residual stress value in the as-built state of 191 MPa. This different behavior is mainly due to the different properties of the hexagonal α’ martensite in Ti6Al4V and the soft orthorhombic α’’ martensite in Ti6246. The post-processing heat treatment significantly reduced the residual stress in Ti6Al4V, lowering it to 44 MPa, while, in the case of Ti-6Al-2Sn-4Zr-6Mo, the post-processing heat treatment did not affect the residual stress conditions. These findings suggest that Ti-6Al-2Sn-4Zr-6Mo could be a suitable candidate for the additive manufacturing production of extremely complex parts, as it could reduce the risks associated with recoater crashes and job failures.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Applied Science and Technology, Politecnico di Torino, Corso Duca Degli Abruzzi 24, 10129 Torino, Italy

Consorzio Interuniversitario Nazionale per la Scienza e Tecnologia dei Materiali (INSTM), Via G. Giusti 9, 50121 Firenze, Italy

Department of Management and Production Engineering (DIGEP), Politecnico di Torino, Corso Duca Degli Abruzzi 24, 10129 Torino, Italy

Centre Suisse d’Electronique et de Microtechnique (CSEM), Jaquet Droz 1, CH-2002 Neuchȃtel, Switzerland

Funding

European research project MANUELA Additive Manufacturing

References (27)

Show source-provided references
1. Mugwagwa, L., Yadroitsava, I., Makoana, N.W., and Yadroitsev, I. (2021). Residual stress in laser powder bed fusion. Fundamentals of Laser Powder Bed Fusion of Metals, Elsevier.10.1016/B978-0-12-824090-8.00014-7 ↗
2. Bastola, N., Jahan, M.P., Rangasamy, N., and Rakurty, C.S. (2023). A Review of the Residual Stress Generation in Metal Additive Manufacturing: Analysis of Cause, Measurement, Effects, and Prevention. Micromachines, 14.10.3390/mi14071480 ↗
3. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
4. Rapid calculation of part scale residual stress—Powder bed fusion of stainless steel, and aluminum, titanium, nickel alloys
5. An improved prediction of residual stresses and distortion in additive manufacturing10.1016/j.commatsci.2016.10.003 ↗
6. A thermo-metallurgical-mechanical model for selective laser melting of Ti6Al4V10.1016/j.matdes.2019.107642 ↗
7. Additive manufacturing of titanium alloys in the biomedical field: Processes, properties and applications
8. Towards Ad Hoc Heat Treatments and Mechanical Properties in the LPBF-processed Ti-6Al-2Sn-4Zr-6Mo alloy10.1016/j.matdes.2022.110512 ↗
9. A study on the microstructure and mechanical properties of the Ti-6Al- 2Sn-4Zr-6Mo alloy produced via Laser Powder Bed Fusion10.1016/j.jallcom.2021.159329 ↗
10. Peculiar microstructural evolution and hardness variation depending on laser powder bed fusion-manufacturing condition in Ti–6Al–2Sn–4Zr–6Mo
11. Rapid hardening response of ultra-hard Ti-6Al-2Sn-4Zr-6Mo alloy produced by laser powder bed fusion10.1016/j.scriptamat.2022.115209 ↗
12. Investigating Complex Geometrical Features in LPBF-Produced Parts: A Material-Based Comparison Between Different Titanium Alloys10.1007/s12540-023-01460-4 ↗
13. A novel solution treatment and aging for powder bed fusion-laser beam Ti-6Al-2Sn-4Zr-6Mo alloy
14. Microstructure and microhardness of heat-treated Ti-6Al-2Sn-4Zr-6Mo alloy10.1016/j.jallcom.2013.03.046 ↗
15. A modified X-ray diffraction method to measure residual normal and shear stresses of machined surfaces10.1007/s00170-021-08645-4 ↗
16. Residual stress and its role in failure10.1088/0034-4885/70/12/R04 ↗
17. Berechnung der röntgenographischen Elastızıtätskonstanten aus den Einkristallkoeffizienten hexagonal kristallisierender Metalle/Calculation of X-Ray Elastic Constants from Single Crystal Coefficients of Hexagonally Crystallizing Metals10.1515/ijmr-1971-620106 ↗
18. Martensitic Twinning in Alpha + Beta Ti-3.5Al-4.5Mo Titanium Alloy10.1155/2011/924032 ↗
19. The crystallography of the β-α transformation in titanium10.1016/0001-6160(54)90101-7 ↗
20. Heat treatment simulation of Ti-6Al-4V parts produced by selective laser melting
21. Validation of Mechanical Layer Equivalent Method for simulation of residual stresses in additive manufactured components10.1016/j.camwa.2018.08.016 ↗
22. Residual stresses and porosity in Ti-6Al-4V produced by laser powder bed fusion as a function of process atmosphere and component design
23. Martensitic transformation from β to α′ and α″ phases in Ti-V alloys: A first-principles study10.1557/jmr.2017.276 ↗
24. Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
25. Otte, A.L., Mai, P.T., Stark, A., Hoelzel, M., Hofmann, M., and Gibmeier, J. (2023). Kinetics of Martensite Decomposition and Microstructure Stability of Ti-6246 during Rapid Heating to Service Temperatures. Metals, 13.10.3390/met13030484 ↗
26. A first-principles study for the elastic and mechanical properties of Ti64, Ti6242 and Ti6246 alloys10.1140/epjb/s10051-021-00230-8 ↗
27. A critical review on additive manufacturing of Ti-6Al-4V alloy: Microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗