Reducing Sintering Temperature While Optimizing Electrical Properties of BCZT-Based Lead-Free Ceramics by Adding MnO2 as Sintering Aid
Source abstract
Abstract
In order to reduce the sintering temperature, MnO2 was used as a sintering aid to prepare [(Ba0.85Ca0.15)0.999(Dy0.5Tb0.5)0.001](Zr0.1Ti0.9)O3-x mol% MnO2 (BCDTZT-x mol% MnO2, x = 0.05, 0.2, 0.4, 0.6, 0.8, 1, 1.5, 3) lead-free piezoelectric ceramics in which the effects of the MnO2 doping amount and sintering temperature on the phase structure, sintering behavior, and electrical properties of the BCDTZT-x mol% MnO2 ceramics were systematically analyzed. All ceramics have a single perovskite structure and coexist in multiple phases. The optimal sintering temperature was reduced from 1515 °C to 1425 °C, and the density of all ceramics was increased as compared with the undoped ceramic, reaching a maximum of 5.38 g/cm3 at x = 0.8 mol%. An appropriate MnO2 doping amount of 0.4 mol% could effectively suppress oxygen vacancies and improve electrical properties, resulting in the best comprehensive performance of the ceramics, with a dielectric constant maximum of 12,817, a high piezoelectric constant of 330 pC/N, and good strain value (Smax = 0.118%) and low strain hysteresis (Hys = 2.66%). The calculation of activation energy indicated that the high-temperature conductivity was dominated by oxygen vacancies in all ceramics. The results showed that the appropriate introduction of MnO2 as a sintering aid could improve the performance of BCZT-based ceramics while reducing the sintering temperature, presenting high practical application value in the fields of low electric field sensors and actuators.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.