Abstract
Room-temperature liquid metals (LMs) are attractive candidates for thermal interface materials (TIMs) because of their moderately high thermal conductivity and liquid nature, which allow them to conform well to mating surfaces with little thermal resistance. However, gallium-based LMs may be of concern due to the gallium-driven degradation of many metal microelectronic components. We present a three-component composite with LM, copper (Cu) microparticles, and a polymer matrix, as a cheaper, noncorrosive solution. The solid copper particles alloy with the gallium in the LM, in situ and at room temperature, immobilizing the LM and eliminating any corrosion issues of nearby components. Investigation of the structure–property–process relationship of the three-component composites reveals that the method and degree of additive blending dramatically alter the resulting thermal transport properties. In particular, microdispersion of any combination of the LM and Cu additives results in a large number of interfaces and a thermal conductivity below 2 W m –1 K –1 . In contrast, a shorter blending procedure of premixed LM and Cu particle colloid into the polymer matrix yields a composite with polydispersed filler and effective intrinsic thermal conductivities of up to 17 W m –1 K –1 (effective thermal conductivity of up to 10 W m –1 K –1 ). The LM–Cu colloid alloying into CuGa 2 provides a limited, but practical, time frame to cast the uncured composite into the desired shape, space, or void before the composite stiffens and cures with permanent characteristics.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Thermal properties of materials · Ferroelectric and Piezoelectric Materials · Thermal Radiation and Cooling Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School for Engineering of Matter, Transport, and Energy, Arizona State University, Tempe, Arizona 85287, United States
Funding
Arizona State University · Division of Materials Research
References (74)
Show source-provided references
1. 10.1016/j.mattod.2014.04.00310.1016/j.mattod.2014.04.003 ↗
2. 2015
3. Intel.Intel Xeon Processor E5-2695 v4.http://ark.intel.com/products/91316/Intel-Xeon-Processor-E5-2695-v4-45M-Cache-2_10-GHz.
4. 10.1038/nature1067610.1038/nature10676 ↗
5. 10.1115/1.402661610.1115/1.4026616 ↗
6. 10.1016/S1359-4311(01)00042-410.1016/S1359-4311(01)00042-4 ↗
7. Blazej D. · Electron. Cool. · 2003 · 9 · 14
8. 10.1115/1.403160210.1115/1.4031602 ↗
9. 10.1016/j.expthermflusci.2011.04.01210.1016/j.expthermflusci.2011.04.012 ↗
10. Off. J. Eur. Union · 2011 · 54 · 88
11. 10.1007/s00339-012-6887-510.1007/s00339-012-6887-5 ↗
12. 10.1016/j.applthermaleng.2016.01.03610.1016/j.applthermaleng.2016.01.036 ↗
13. 10.1016/j.microrel.2015.08.02010.1016/j.microrel.2015.08.020 ↗
14. 10.1115/1.403502510.1115/1.4035025 ↗
15. Li, G.; Ji, Y.; Wu, M.; Ma, H.InHighly Conductive Thermal Paste of Liquid Metal Alloy Dispersed with Copper Particles, Proceedings of the ASME 2016 Heat Transfer Summer Conference;American Society of Mechanical Engineers:Washington, DC, 2016.10.1115/HT2016-7374 ↗
16. 10.1021/je400882q10.1021/je400882q ↗
17. Wilcox, M.; Ghoshal, U.; Grimm, D.; Ibrani, S.; Feicht, D.; Miner, A.High-performance liquid metal cooling loops. InSemiconductor Thermal Measurement and Management Symposium, 2005, IEEE Twenty First Annual IEEE; pp19–19.
18. Geratherm Medical AG. Safety Data Sheet for Galinstan fluid.http://www.rgmd.com/msds/msds.pdf(accessed Oct 6, 2017) .
19. 10.1115/1.402641410.1115/1.4026414 ↗
20. Lyon R. N. · 1952
21. 10.1016/j.actamat.2014.04.01110.1016/j.actamat.2014.04.011 ↗
22. 10.1007/s00339-009-5098-110.1007/s00339-009-5098-1 ↗
23. Ndieguene, A.; Albert, P.; Fortin, C.; Oberson, V.; Sylvestre, J. InEternal Packages: Liquid Metal Flip Chip Devices, 2016 IEEE 66th Electronic Components and Technology Conference 2016; pp580–587.10.1109/ECTC.2016.29 ↗
24. 10.1016/j.progpolymsci.2010.11.00410.1016/j.progpolymsci.2010.11.004 ↗
25. 10.3390/polym608224710.3390/polym6082247 ↗
26. 10.1109/MEI.2011.595406410.1109/MEI.2011.5954064 ↗
27. Sarvar, F.; Whalley, D.; Conway, P.InThermal Interface Materials - A Review of the State of the Art, 2006 1st Electronics Systemintegration Technology Conference, 2006; Vol. 2, pp1292–1302.10.1109/ESTC.2006.280178 ↗
28. 10.1177/002199830606732110.1177/0021998306067321 ↗
29. Ralphs M. I. · 2016
30. 10.1002/adma.20160064210.1002/adma.201600642 ↗
31. 10.1002/admi.20150018610.1002/admi.201500186 ↗
32. Prasher, R.InThermal Interface Materials: Historical Perspective, Status, and Future Directions, Proceedings of the IEEE;IEEE, 2006; Vol.94, pp1571–1586.10.1109/JPROC.2006.879796 ↗
33. 10.1016/j.ijthermalsci.2011.10.01410.1016/j.ijthermalsci.2011.10.014 ↗
34. 10.1021/am500009p10.1021/am500009p ↗
35. 10.1021/nn500134m10.1021/nn500134m ↗
36. Prasher R. S. · 2017 · 51110.1007/978-3-319-45098-8_12 ↗
37. 10.1016/j.compscitech.2017.03.02010.1016/j.compscitech.2017.03.020 ↗
38. 10.1016/j.applthermaleng.2014.02.04410.1016/j.applthermaleng.2014.02.044 ↗
39. 10.1163/156856108X32051910.1163/156856108X320519 ↗
40. 10.1088/0957-4484/27/17/17560110.1088/0957-4484/27/17/175601 ↗
41. 10.1063/1.479341910.1063/1.4793419 ↗
42. 10.1016/j.mser.2005.04.00210.1016/j.mser.2005.04.002 ↗
43. 10.1088/0957-4484/24/10/10540110.1088/0957-4484/24/10/105401 ↗
44. 10.1021/nn200847u10.1021/nn200847u ↗
45. 10.1073/pnas.161637711410.1073/pnas.1616377114 ↗
46. 10.1002/adma.20140525610.1002/adma.201405256 ↗
47. 10.1002/adma.20150624310.1002/adma.201506243 ↗
48. 10.1038/srep1825710.1038/srep18257 ↗
49. 10.1016/j.microrel.2015.02.01410.1016/j.microrel.2015.02.014 ↗
50. 10.1115/1.402511610.1115/1.4025116 ↗
51. 10.1088/0957-0233/27/11/11501410.1088/0957-0233/27/11/115014 ↗
52. ASTM D5470 · 2006
53. 10.1115/1.282608610.1115/1.2826086 ↗
54. 10.1016/j.eurpolymj.2008.11.01710.1016/j.eurpolymj.2008.11.017 ↗
55. Dow Corning. Electronics Sylgard 184 Silicone Elastomer.Product Datasheet 2013; pp1–3.http://www.dowcorning.com/DataFiles/090276fe80190b08.pdf(accessed Oct 10, 2017).
56. Predel B. · 199410.1007/10086090_1074 ↗
57. 10.1016/j.calphad.2008.03.00610.1016/j.calphad.2008.03.006 ↗
58. 10.1021/acsami.7b1025610.1021/acsami.7b10256 ↗
59. 10.1063/1.180824310.1063/1.1808243 ↗
60. 10.1002/adfm.20070121610.1002/adfm.200701216 ↗
61. 10.1021/la501202310.1021/la5012023 ↗
62. 10.1002/sia.181710.1002/sia.1817 ↗
63. 10.1109/JMEMS.2011.217442110.1109/JMEMS.2011.2174421 ↗
64. 10.1002/adma.20160598510.1002/adma.201605985 ↗
65. 10.1021/la404356r10.1021/la404356r ↗
66. 10.1021/am504301710.1021/am5043017 ↗
67. 10.1007/s10404-015-1665-210.1007/s10404-015-1665-2 ↗
68. 10.1177/073168440707252210.1177/0731684407072522 ↗
69. 10.1016/j.scriptamat.2006.11.00810.1016/j.scriptamat.2006.11.008 ↗
70. Pietrak K. · J. Power Technol. · 2015 · 95 · 14
71. 10.4028/www.scientific.net/DDF.326-328.22710.4028/www.scientific.net/DDF.326-328.227 ↗
72. 10.1103/PhysRevB.72.24542610.1103/PhysRevB.72.245426 ↗
73. 10.1063/1.152430510.1063/1.1524305 ↗
74. Stauffer D. · 1992