Steam Oxidation of Austenitic Heat-Resistant Steels TP347H and TP347HFG at 650–800 °C

Zhiyuan Liang, Qinxin Zhao

Materials· Volume 12· Issue 4

Abstract

Steam oxidation of austenitic heat-resistant steels TP347H and TP347HFG at 650–800 °C was investigated. Comprehensive micro-characterization technologies containing Scanning Electron Microscope (SEM), Energy Dispersive X-ray Spectroscopy (EDS), X-ray Diffraction (XRD), and X-ray Photoelectron Spectroscopy (XPS) were employed to observe and analyze the oxidation products. Results show that breakaway oxidation behaviors were observed on TP347H at 700 °C and 800 °C. The oxidation kinetics of TP347HFG at 650–800 °C followed a parabolic law. The oxide scales formed on TP347HFG were composed of MnCr2O4 and Cr2O3. A thin and protective Cr-rich oxide scale was replaced by Fe2O3 nodules due to the insufficient outward migration of metallic ions, including Cr and Mn at the subsurface of coarse-grain TP347H. Smaller grain of TP347HFG promoted the formation of the compact Cr-rich oxide scales. At higher temperatures, the incubation period for breakaway oxidation of the Cr-rich oxide scale was much shorter because of quick evaporation of the Cr2O3 oxide scale and the slower outward diffusion of metallic ions via the grain boundaries.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Subcritical and Supercritical Water Processes · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory of Thermal Fluid Science and Engineering of MOE, School of Energy and Power Engineering, Xi’an Jiaotong University, Xi’an 710049, China

Funding

National Natural Science Foundation of China

References (38)

Show source-provided references
1. Boiler materials for ultra-supercritical coal power plants—Steamside oxidation10.1361/105994906X108756 ↗
2. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: A review10.1016/j.pmatsci.2007.11.001 ↗
3. Long-term performance of high-temperature foil alloys in water vapor containing environment. Part I: Oxidation Behavior10.1007/s11085-012-9343-1 ↗
4. Birks, N., Meier, G.H., and Pettit, F.S. (2006). Introduction to the High-Temperature Oxidation of Metals, Cambridge University Press.10.1017/CBO9781139163903 ↗
5. Corrosion in high-temperature and supercritical water and aqueous solutions: A review10.1016/S0896-8446(03)00031-7 ↗
6. Oxidation behavior of super 304H steel in steam at 700~900 °C
7. Viswanathan, R. (1999). Advanced Heat Resistant Steels for Power Generation, CRC Press.
8. Mahanen, J. (2011). Steam-side Oxidation of Materials for Supercritical Boilers. [Master’s Thesis, Tamper University of Technology].
9. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
10. Steamside oxidation behaviour of candidate USC materials at temperatures between 650 and 800 °C10.1179/174892408X383076 ↗
11. Study of the corrosion behavior of a 18Cr-oxide dispersion strengthened steel in supercritical water10.1016/j.corsci.2012.08.021 ↗
12. An investigation of key experimental parameters in steam oxidation testing and the impact they have on the interpretation of experimental results
13. Managing steam-side oxidation and exfoliation in USC boiler tubes
14. Oxidation kinetics, breakaway oxidation, and inversion phenomenon in 9Cr-1Mo steels10.1007/BF00659183 ↗
15. Microstructural investigation of the oxide formed on TP 347HFG during long-term steam oxidation10.1002/maco.200905439 ↗
16. Impact specimen geometry on T23 and TP347HFG steels behaviour during steam oxidation at harsh conditions
17. Investigation of steam oxidation behaviour of TP347H FG. Part 2: Exposure at 91 bar10.1002/maco.200403856 ↗
18. Microstructure evolution during steam oxidation of a Nb stabilized austenitic stainless steel10.1007/s11085-009-9182-x ↗
19. Enhanced internal oxidation as trigger for breakaway oxidation of Fe-Cr alloys in gases containing water vapor10.1016/j.scriptamat.2007.06.058 ↗
20. Investigation into the failure mechanism of chromia scale thermally grown on an austenitic stainless steel in pure steam10.1016/j.corsci.2016.03.021 ↗
21. Effect of shot blasting on oxidation behavior of TP304H steel at 610–770 °C in water vapor10.1016/j.matlet.2005.08.046 ↗
22. Review of factors affecting steam oxidation testing10.3184/096034011X13185043039504 ↗
23. Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air10.1016/j.actamat.2005.07.019 ↗
24. Influence of the alloy grain size on the oxidation behaviour of PM2000 alloy10.1016/S0010-938X(01)00182-2 ↗
25. Role of grain boundaries on the cyclic steam oxidation behaviour of 18-8 austenitic stainless steel10.1007/s11085-015-9603-y ↗
26. High Temperature Oxidation of Newly Developed Alloy 282 in the Flowing-Air and Steam Condition at 900–1100 °C10.1007/s11085-015-9555-2 ↗
27. Effect of thermally grown oxides on colour development of stainless steel10.1179/0960340914Z.00000000083 ↗
28. In situ study of the initiation of hydrogen bubbles at the aluminium metal/oxide interface10.1038/nmat4336 ↗
29. Effect of alloy grain size and silicon content on the oxidation of austenitic Fe-Cr-Ni-Mn-Si alloys in pure O210.1007/BF00662967 ↗
30. Effect of grain refinement on corrosion of ferritic-martensitic steels in supercritical water environment10.1002/maco.200905446 ↗
31. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
32. Stability of MnCr2O4 spinel and Cr2O3 in high temperature carbonaceous environments with varied oxygen partial pressures10.1016/j.corsci.2010.02.040 ↗
33. The effect of manganese additions on the reactive evaporation of chromium in Ni-Cr alloys10.1016/j.scriptamat.2006.01.026 ↗
34. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation10.1023/A:1004642310974 ↗
35. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor10.1023/A:1018875024306 ↗
36. Evaporation of Cr2O3 in atmospheres containing H2O10.1023/A:1023671206976 ↗
37. Steam oxidation and chromia evaporation in ultrasupercritical steam boilers and turbines10.1149/1.3155442 ↗
38. Chromium Volatilization Rates from Cr2O3, scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗