Slurry Erosion–Corrosion Characteristics of As-Built Ti-6Al-4V Manufactured by Selective Laser Melting
Source abstract
Abstract
Erosion and erosion–corrosion tests of as-built Ti-6Al-4V manufactured by Selective Laser Melting were investigated using slurries composed of SiO2 sand particles and either tap water (pure water) or 3.5% NaCl solution (artificial seawater). The microhardness value of selective laser melting (SLM)ed Ti-6Al-4V alloy increased as the impact angle increased. The synergistic effect of corrosion and erosion in seawater is always higher than erosion in pure water at all impact angles. The seawater environment caused the dissolution of vanadium oxide V2O5 on the surface of SLMed Ti-6Al-4V alloy due to the presence of Cl− ions in the seawater. These findings show lower microhardness values and high mass losses under the erosion–corrosion test compared to those under the erosion test at all impact angles.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical and Industrial Engineering, College of Engineering, Majmaah University, Al-Majmaah 11952, Saudi Arabia
Mechanical Engineering Department, Faculty of Engineering, Assiut University, Assiut 71516, Egypt
Funding
Majmaah University
References (63)
Show source-provided references
1. Matthew, J., and Donachie, J. (2000). Titamium: A Technical Guide, ASM International. [2nd ed.].10.31399/asm.tb.ttg2.9781627082693 ↗
2. Titanium alloy production technology, market prospects and industry development Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
3. Wexler, P. (2014). Titanium. Encyclopedia of Toxicology, Academic Press. [3rd ed.].
4. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
5. Li, Y., Song, L., Xie, P., Cheng, M., and Xiao, H. (2020). Enhancing hardness and wear performance of laser additive manufactured Ti6Al4V alloy through achieving ultrafine microstructure. Materials, 13.10.3390/ma13051210 ↗
6. Mechanical properties of titanium-based Ti–6Al–4V alloys manufactured by powder bed additive manufacture10.1080/02670836.2016.1172787 ↗
7. Erosion behavior and damage evolution of Ti-6Al-4V aeroengine titanium alloy10.1088/1757-899X/770/1/012083 ↗
8. Influence of Microstructure on High Temperature Solid Particle Erosion Behaviour of Ti–6Al–4V Alloy10.1007/s12666-013-0347-6 ↗
9. Solid Particle Erosion on Shield Surface of a Helicopter Rotor Blade Using Computational Fluid Dynamics10.1061/(ASCE)AS.1943-5525.0000962 ↗
10. Rahman, M.H. (2013). Design and Analysis of Hybrid Titanium-Composite Hull Structures Under Extreme Wave and Slamming Loads, Florida Atlantic University.
11. Doran, D., and Cather, B. (2014). Construction Materials Reference Book, Routledge. [2nd ed.].10.4324/9780080940380 ↗
12. Effect of heat treatment on erosive wear behaviour of Ti6Al4V alloy10.1179/1743284713Y.0000000239 ↗
13. Corrosion and erosion performance of HVOF/TiAlN PVD coatings and candidate materials for high pressure gate valve application10.1016/j.wear.2004.12.045 ↗
14. Thermal Oxidation of Ti6Al4V Alloy with Enhanced Wear and Corrosion Resistance for Oil and Gas Application: Effect of Temperature10.1142/S0218625X1550033X ↗
15. Enhanced erosion protection of TWAS coated Ti6Al4V Alloy using boride bond coat and subsequent laser treatment10.1007/s11665-010-9735-9 ↗
16. The analysis of causes of the damage of a turbine blade made of Ti-6Al-4V alloy10.4028/www.scientific.net/SSP.270.189 ↗
17. Studies on the role of HVOF coatings to combat erosion in turbine alloys10.1016/j.matpr.2018.01.119 ↗
18. Matyka, M., Ziaja, W., and Sieniawski, J. (2019). Modern production methods for titanium alloys: A review. Titanium Alloys—Novel Aspects of Their Manufacturing and Processing, IntechOpen.
19. Davis, R.J. (1998). Processing of Titanium and Titanium Alloys. Metals Handbook Desk Edition, ASM International.10.31399/asm.hb.mhde2.9781627081993 ↗
20. Study on the solid-liquid erosion resistance of ion-nitrided metal10.1016/S0043-1648(02)00013-3 ↗
21. Slurry Erosion Wear Resistance and Impact-Induced Phase Transformation of Titanium Alloys10.1007/s11249-018-1015-0 ↗
22. Slurry abrasion response of surface engineered Ti6Al4VELI10.1016/S0301-679X(99)00082-1 ↗
23. Erosion– and cavitation–corrosion of titanium and its alloys10.1016/S0043-1648(01)00709-8 ↗
24. Microstructure and erosive wear behaviors of Ti6Al4V alloy treated by plasma Ni alloying10.1016/j.apsusc.2015.10.231 ↗
25. Erosion-corrosion behavior and cathodic protection of alloys in seawater-sand slurries10.1007/BF02645684 ↗
26. Slurry pot investigation of the influence of erodant characteristics on the erosion resistance of titanium10.1016/j.wear.2014.10.005 ↗
27. Solid particle erosion behaviour of Ti6Al4V alloy10.1179/1751584X13Y.0000000043 ↗
28. Zhao, J.-R., Hung, F.-Y., Lui, T.-S., and Wu, Y.-L. (2019). The Relationship of Fracture Mechanism between High Temperature Tensile Mechanical Properties and Particle Erosion Resistance of Selective Laser Melting Ti-6Al-4V Alloy. Metals, 9.10.3390/met9050501 ↗
29. Laser cladding technique for erosive wear applications: A review10.1088/2053-1591/ab6894 ↗
30. International Organization for Standardization/ASTM International (2015). Additive Manufacturing—General Principles—Terminology (ISO/ASTM 52900) [Standard], ISO.
31. Powder bed fusion process in additive manufacturing: An overview10.1016/j.matpr.2020.02.635 ↗
32. Mishurova, T., Cabeza, S., Artzt, K., Haubrich, J., Klaus, M., Genzel, C., Requena, G., and Bruno, G. (2017). An assessment of subsurface residual stress analysis in SLM Ti-6Al-4V. Materials, 10.10.3390/ma10040348 ↗
33. Selective Laser Melting of Titanium Alloys and Titanium Matrix Composites for Biomedical Applications: A Review10.1002/adem.201500419 ↗
34. Barriobero-Vila, P., Gussone, J., Haubrich, J., Sandlöbes, S., Da Silva, J.C., Cloetens, P., Schell, N., and Requena, G. (2017). Inducing stable α + β microstructures during selective laser melting of Ti-6Al-4V using intensified intrinsic heat treatments. Materials, 10.10.3390/ma10030268 ↗
35. Comparison of wear properties of commercially pure titanium prepared by selective laser melting and casting processes10.1016/j.matlet.2014.11.156 ↗
36. Differences in microstructure and properties between selective laser melting and traditional manufacturing for fabrication of metal parts: A review10.1007/s11465-015-0341-2 ↗
37. Ji, Y., Chen, L., and Chen, L.Q. (2018). Understanding Microstructure Evolution During Additive Manufacturing of Metallic Alloys Using Phase-Field Modeling, Elsevier Inc.. [1st ed.].10.1016/B978-0-12-811820-7.00008-2 ↗
38. He, J., Li, D., Jiang, W., Ke, L., Qin, G., Ye, Y., Qin, Q., and Qiu, D. (2019). The Martensitic Transformation and Mechanical Properties of Ti6Al4V Prepared via Selective Laser Melting. Materials, 12.10.3390/ma12020321 ↗
39. Heat-treatment effects on mechanical properties and microstructure evolution of Ti-6Al-4V alloy fabricated by laser powder bed fusion10.1016/j.jallcom.2019.152615 ↗
40. Mapping the geometry of Ti-6Al-4V: From martensite decomposition to localized spheroidization during selective laser melting10.1016/j.scriptamat.2020.02.043 ↗
41. Effects of laser power on geometry, microstructure and mechanical properties of printed Ti-6Al-4V parts10.1016/j.jmatprotec.2019.116539 ↗
42. Tao, P., Zhong, J., Li, H., Hu, Q., Gong, S., and Xu, Q. (2019). Microstructure, mechanical properties, and constitutive models for Ti–6Al–4V alloy fabricated by selective laser melting (SLM). Metals, 9.10.3390/met9040447 ↗
43. Agius, D., Kourousis, K.I., and Wallbrink, C. (2018). A review of the as-built SLM Ti-6Al-4V mechanical properties towards achieving fatigue resistant designs. Metals, 8.10.3390/met8010075 ↗
44. Dry sliding wear performance and behaviour of powder bed fusion processed Ti–6Al–4V alloy10.1016/j.wear.2019.203103 ↗
45. Beese, A.M. (2018). Microstructure and Mechanical Properties of AM Builds, Elsevier Inc.. [1st ed.].10.1016/B978-0-12-811820-7.00007-0 ↗
46. Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
47. On the role of different annealing heat treatments on mechanical properties and microstructure of selective laser melted and conventional wrought Ti-6Al-4V10.1108/RPJ-02-2016-0022 ↗
48. Torsional fatigue behavior of wrought and additive manufactured Ti-6Al-4V by powder bed fusion including surface finish effect10.1016/j.ijfatigue.2017.03.002 ↗
49. Evaluation of the mechanical and wear properties of titanium produced by three different additive manufacturing methods for biomedical application10.1016/j.msea.2019.06.024 ↗
50. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
51. Particle size effects on slurry erosion of 5117 steels10.1115/1.4002605 ↗
52. Design and Performance of Slurry Erosion Tester10.1115/1.4001449 ↗
53. Stepwise Erosion as a Method for Investigating the Wear Mechanisms at Different Impact Angles in Slurry Erosion10.1115/1.4026420 ↗
54. The effect of boronizing heat treatment on the slurry erosion of AISI 511710.1108/ILT-01-2017-0009 ↗
55. Characterization of the Structural and Tribological Properties of Medical Ti6Al4V Alloy Produced in Different Production Parameters Using Selective Laser Melting10.1089/3dp.2019.0017 ↗
56. Effect of wet shot peening on Ti-6Al-4V alloy treated by ceramic beads10.1016/S1003-6326(14)63112-5 ↗
57. Effect of Impact Angle on Slurry Erosion Behavior and Mechanisms of Carburized AISI 5117 Steel
58. Slurry erosion-corrosion of carburized AISI 5117 steel10.1007/s11249-013-0155-5 ↗
59. Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
60. Fretting fatigue behavior of shot-peened Ti-6Al-4V under seawater environment10.1016/j.msea.2006.01.031 ↗
61. Effect of thermal oxidation on corrosion and corrosion-wear behaviour of a Ti-6Al-4V alloy10.1016/j.biomaterials.2003.10.009 ↗
62. Corrosion behaviour of Ti-6Al-7Nb and Ti-6Al-4V ELI alloys in the simulated body fluid solution by electrochemical impedance spectroscopy10.1016/j.electacta.2006.06.018 ↗
63. Sherif, E.-S.M., Ragab, S.A., and Abdo, H.S. (2020). Role of Vanadium Additions on the Corrosion Mitigation of Ti-6Al-xV Alloy in Simulated Body Fluid. Metals, 10.10.3390/met10070903 ↗