Abstract

Narrow gap laser welding (NGLW) is a common solution for the welding of thick structures. NGLW was carried out on narrow-gap butt joints of 40 mm-thick Ti-6Al-4V alloy plates with a U-shaped groove. The distribution characteristics of the interlaminar microstructure in different height ranges of the joint were investigated, and the evolution behavior and formation mechanism of the interlaminar microstructure of the joint were also revealed. This showed that a large amount of short needle martensite nucleated and grew up near the fusion line and the upper boundary of the remelting zone. The “softening” phenomenon occurred in all welds except the cover layer weld. The microstructure evolution and defect migration, induced by multiple welding thermal cycles in the upper weld forming process, were the main reasons for the “softening” of the lower weld. The tensile strength of each sample changed in the range of 920~990 MPa; the fracture mode of the sample belongs to a transgranular ductile fracture. In addition, compared with the upper part of the joint, the plasticity and toughness of the weld area in the lower part of the joint was improved.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Additive Manufacturing Materials and Processes · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 211106, China

Funding

Defense Industrial Technology Development Program

References (31)

Show source-provided references
1. Effect of Base Material on Microstructure and Texture Evolution of a Ti–6Al–4V Electron-Beam Welded Joint10.1007/s40195-017-0528-0 ↗
2. Laser welding of Ti6Al4V titanium alloys10.1016/j.jmatprotec.2008.08.026 ↗
3. Surface morphology of Ti-6Al-4V plate fabricated by vacuum selective laser melting10.1007/s00340-015-6059-3 ↗
4. Comparison of bead shape, microstructure and mechanical properties of fiber laser beam welding of 2 mm thick plates of Ti-6Al-4V alloy10.1016/j.optlastec.2018.02.021 ↗
5. Effect of the forging pressure on the microstructure and residual stress development in Ti–6Al–4V linear friction welds10.1016/j.actamat.2009.07.055 ↗
6. Laser Beam Welding of Thick Titanium Sheets in the Field of Marine Technology10.1016/j.phpro.2014.08.046 ↗
7. Microstructures and fatigue properties of electron beam welds with beam oscillation for heavy section TC4-DT alloy10.1016/j.cja.2014.03.020 ↗
8. Microstructure, texture and mechanical properties of commercial high-purity thick titanium plates jointed by electron beam welding10.1016/j.msea.2016.09.030 ↗
9. Effect of heat treatment on corrosion behavior of Ti–6Al–4V alloy weldments10.1016/j.jmatprotec.2007.12.065 ↗
10. Fatigue inhomogeneity of 140 mm thick TC4 titanium alloy double-sided electron beam welded joints10.1016/j.ijfatigue.2022.107214 ↗
11. Characteristics of welding and arc pressure in TIG narrow gap welding using novel magnetic arc oscillation10.1007/s00170-016-9407-5 ↗
12. Comparison of microstructure and mechanical properties of ultra-narrow gap laser and gas-metal-arc welded S960 high strength steel10.1016/j.optlaseng.2016.11.011 ↗
13. Microstructure and mechanical properties of electron beam welded TC4/TA7 dissimilar titanium alloy joint10.1016/j.jmapro.2019.11.007 ↗
14. Microstructure, texture and tensile property as a function of scanning speed of Ti-47Al-2Cr-2Nb alloy fabricated by selective electron beam melting10.1016/j.msea.2017.12.020 ↗
15. Laser Multi-Pass Narrow-Gap Welding—A Promising Technology for Joining Thick-Walled Components of Future Power Plants10.1051/matecconf/201926902011 ↗
16. Study on the weldability, microstructure and mechanical properties of thick Inconel 617 plate using narrow gap laser welding method10.1016/j.matdes.2019.107823 ↗
17. Multi-pass laser welding of thick plate with filler wire by using a narrow gap joint configuration10.1007/s12206-013-0525-9 ↗
18. Effect of joint gap on the quality of laser beam welded near-β Ti-5553 alloy with the addition of Ti–6Al–4V filler wire10.1007/s10853-011-5866-0 ↗
19. Narrow-gap laser welding with beam wobbling and filler wire and microstructural performance of joints of thick TC4 titanium alloy plates10.1016/j.optlastec.2022.108089 ↗
20. Microstructure and mechanical properties of ultra-narrow gap laser weld joint of 100 mm-thick SUS304 steel plates10.1016/j.jmatprotec.2018.10.017 ↗
21. Evaluation of microstructural development in electron beam melted Ti-6Al-4V10.1016/j.matchar.2011.12.008 ↗
22. Microstructures and performances of the butt joint of TA1/Q235B bimetallic sheet with addition of a Mo interlayer by using narrow gap laser welding with filler wire10.1016/j.jmrt.2020.07.054 ↗
23. Effects of sidewall grain growth on pore formation in narrow gap oscillating laser welding10.1016/j.optlastec.2022.108483 ↗
24. Temperature-gradient induced microstructure evolution in heat-affected zone of electron beam welded Ti-6Al-4V titanium alloy10.1016/j.jmst.2019.04.004 ↗
25. Five-parameter characterization of intervariant boundaries in additively manufactured Ti-6Al-4V10.1016/j.matdes.2020.109177 ↗
26. Process-parameter interactions in ultra-narrow gap laser welding of high strength steels10.1007/s00170-015-7881-9 ↗
27. Direct observation of keyhole characteristics in deep penetration laser welding with a 10 kW fiber laser10.1364/OE.21.019997 ↗
28. Near-Threshold Fatigue Crack Growth Rates of Laser Powder Bed Fusion Produced Ti-6Al-4V10.1016/j.actamat.2020.07.049 ↗
29. Influence of crystallographic texture on the microstructure, tensile properties and residual stress state of laser-welded titanium joints10.1016/j.matdes.2016.03.148 ↗
30. Mechanical behaviour of similar and dissimilar AA5182-H111 and AA6016-T4 thin friction stir welds10.1016/j.matdes.2008.04.045 ↗
31. Microstructure and mechanical property improvement of Ti alloy and stainless steel joint based on a hybrid connection mechanism10.1016/j.matlet.2020.128012 ↗