Abstract

In low Earth orbit (LEO), hazards such as atomic oxygen (AO) or electrostatic discharge (ESD) degrade polymeric materials, specifically, the extensively used polyimide (PI) Kapton. We prepared PI-based nanocomposite films that show both AO durability and ESD protection by incorporating polyhedral oligomeric silsesquioxane (POSS) and carbon nanotube (CNT) additives. The unique methods that are reported prevent CNT agglomeration and degradation of the CNT properties that are common in dispersion-based processes. The influence of the POSS content on the electrical, mechanical, and thermo-optical properties of the CNT-POSS-PI films was investigated and compared to those of control PI and CNT-PI films. CNT-POSS-PI films with 5 and 15 wt % POSS content exhibited sheet resistivities as low as 200 Ω/□, and these resistivities remained essentially unchanged after exposure to AO with a fluence of ∼2.3 × 10(20) O atoms cm(-2). CNT-POSS-PI films with 15 wt % POSS content exhibited an erosion yield of 4.8 × 10(-25) cm(3) O atom(-1) under 2.3 × 10(20) O atoms cm(-2) AO fluence, roughly one order of magnitude lower than that of pure PI films. The durability of the conductivity of the composite films was demonstrated by rolling film samples with a tight radius up to 300 times. The stability of the films to thermal cycling and ionizing radiation was also demonstrated. These properties make the prepared CNT-POSS-PI films with 15 wt % POSS content excellent candidates for applications where AO durability and electrical conductivity are required for flexible and thermally stable materials. Hence, they are suggested here for LEO applications such as the outer layers of spacecraft thermal blankets.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicone and Siloxane Chemistry · Synthesis and properties of polymers · Conducting polymers and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Space Environment Department, Soreq NRC, Yavne 81800, Israel

Department of Chemistry and Biochemistry, Montana State University, Bozeman, Montana 59717, United States

Funding

U.S. Department of Defense

References (57)

Show source-provided references
1. Tribble A. C. · 1995
2. Finckenor M. · 1999
3. Ghosh M. · 1996
4. Reddy M. R. · Surf. Coat. Technol. · 1993 · 58 · 110.1016/0257-8972(93)90169-O ↗
5. Banks B. A. · J. Spacecr. Rockets · 2004 · 41 · 33510.2514/1.10726 ↗
6. Angirasa D. · J. Spacecr. Rockets · 2014 · 51 · 75010.2514/1.A32742 ↗
7. Gotlib-Vainstein K. · ACS Appl. Mater. Interfaces · 2015 · 7 · 353910.1021/am5072817 ↗
8. Packirisamy S. · J. Mater. Sci. · 1995 · 30 · 30810.1007/BF00354390 ↗
9. Kleiman J. · 1999 · 210.1007/978-94-011-4768-2 ↗
10. Iskanderova Z. · Mater. Chem. Phys. · 1998 · 54 · 9110.1016/S0254-0584(98)00018-2 ↗
11. Gudimenko, Y.; Ng, R.; Kleiman, J.; Iskanderova, Z.; Tennyson, R.; Hughes, P.; Milligan, D.; Grigorevski, A.; Shuiski, M.; Kiseleva, L.InEnhancement of Surface Durability of Space Materials and Structures in LEO Environment;Proceedings of the 9th International Symposium on Materials in a Space Environment, Noordwijk, The Netherlands, June 16-20, 2003;ESA Publications:Noordwijk, The Netherlands, 2003; pp95–106.
12. Wang M. · Polym. Degrad. Stab. · 2004 · 86 · 52110.1016/j.polymdegradstab.2004.06.004 ↗
13. Watson K. A. · Macromolecules · 2002 · 35 · 496810.1021/ma0201779 ↗
14. Fischer H. R. · ACS Appl. Mater. Interfaces · 2010 · 2 · 221810.1021/am100223v ↗
15. Miyazaki E. · Acta Astronaut. · 2010 · 66 · 92210.1016/j.actaastro.2009.09.002 ↗
16. Brunsvold A. L. · High Perform. Polym. · 2004 · 16 · 30310.1177/0954008304044121 ↗
17. Minton T. K. · ACS Appl. Mater. Interfaces · 2012 · 4 · 49210.1021/am201509n ↗
18. Verker R. · Acta Mater. · 2009 · 57 · 111210.1016/j.actamat.2008.10.054 ↗
19. Verker R. · Polymer · 2007 · 48 · 1910.1016/j.polymer.2006.10.035 ↗
20. Verker R. · Compos. Sci. Technol. · 2009 · 69 · 217810.1016/j.compscitech.2009.06.001 ↗
21. Chou W.-J. · Compos. Sci. Technol. · 2008 · 68 · 220810.1016/j.compscitech.2008.04.008 ↗
22. Jiang X. · Polymer · 2005 · 46 · 741810.1016/j.polymer.2005.05.127 ↗
23. Ogasawara T. · Composites, Part A · 2004 · 35 · 6710.1016/j.compositesa.2003.09.003 ↗
24. Ounaies Z. · Compos. Sci. Technol. · 2003 · 63 · 163710.1016/S0266-3538(03)00067-8 ↗
25. Smith J. · Polymer · 2004 · 45 · 82510.1016/j.polymer.2003.11.024 ↗
26. So H. H. · Eur. Polym. J. · 2007 · 43 · 375010.1016/j.eurpolymj.2007.06.025 ↗
27. Yuan W. · Chem. Mater. · 2011 · 23 · 414910.1021/cm200909x ↗
28. Zhu B. K. · Compos. Sci. Technol. · 2006 · 66 · 54810.1016/j.compscitech.2005.05.038 ↗
29. Atar N. · ACS Appl. Mater. Interfaces · 2014 · 6 · 2040010.1021/am505811g ↗
30. Ma P. C. · Composites, Part A · 2010 · 41 · 134510.1016/j.compositesa.2010.07.003 ↗
31. David-Pur M. · Biomed. Microdevices · 2013 · 16 · 4310.1007/s10544-013-9804-6 ↗
32. TB, Pyralin Polyimide Coating PI 2545 PI 2540, Product Information, Du Pont, February 1993.
33. Hergenrother P. M. · 1989
34. van der Pauw L. · Philips Res. Rep. · 1958 · 12 · 1
35. Poinas P. · 2004
36. 2002
37. Jung C.-H. · Nucl. Instrum. Methods Phys. Res., Sect. B · 2008 · 266 · 349110.1016/j.nimb.2008.06.019 ↗
38. Li B. · Carbon · 2013 · 60 · 18610.1016/j.carbon.2013.04.012 ↗
39. Lubkowski G. · IEEE Trans. Nucl. Sci. · 2012 · 59 · 79210.1109/TNS.2012.2188644 ↗
40. Nielsen K. L. · Polym. Degrad. Stab. · 2008 · 93 · 16910.1016/j.polymdegradstab.2007.10.010 ↗
41. Holmes-Siedle A. · 1993
42. Buczala D. M. · J. Spacecr. Rockets · 2006 · 43 · 42110.2514/1.16402 ↗
43. 2014
44. Peplinski, D. R.; Arnold, G. S.; Borson, E. N. In 13th Space Simulation Conf.: Introduction to Simulation of Upper Atmosphere Oxygen Satellite Exposed to Atomic Oxygen in Low Earth Orbit;NASA:United States, 1984; pp133–145.
45. 2008
46. Kapton® HN Polyimide Film, MSDS No. K-15345-1 Technical Data Sheet,Du Pont, April 2011.
47. Godet C. · Diamond Relat. Mater. · 2003 · 12 · 15910.1016/S0925-9635(03)00017-7 ↗
48. Li Q. · Adv. Mater. · 2007 · 19 · 335810.1002/adma.200602966 ↗
49. Heltzel S. · High Perform. Polym. · 2004 · 16 · 23510.1177/0954008304044100 ↗
50. Semprimoschnig C. O. · High Perform. Polym. · 2004 · 16 · 20710.1177/0954008304044098 ↗
51. Zhu Y. · ACS Nano · 2011 · 5 · 647210.1021/nn201696g ↗
52. Cairns D. R. · Appl. Phys. Lett. · 2000 · 76 · 142510.1063/1.126052 ↗
53. Zhang J. · ACS Appl. Mater. Interfaces · 2009 · 1 · 65310.1021/am800186m ↗
54. Roro K. T. · Mater. Sci. Eng., B · 2012 · 177 · 58110.1016/j.mseb.2012.03.017 ↗
55. Camacho R. · JOM · 2007 · 59 · 3910.1007/s11837-007-0037-0 ↗
56. Nicholson K. T. · Prog. Org. Coat. · 2003 · 47 · 44310.1016/S0300-9440(03)00134-6 ↗
57. Banks B. A. · 200410.1557/PROC-851-NN8.1 ↗