journal article·2019-09-11

Stable and Unstable Diglyme-Based Electrolytes for Batteries with Sodium or Graphite as Electrode

Mustafa Goktas, Christoph Bolli, Johannes Buchheim, Erik J. Berg, Petr Novák, Francisco Bonilla, Teófilo Rojo, Shinichi Komaba, Kei Kubota, Philipp Adelhelm

ACS Applied Materials & Interfaces· Volume 11· Issue 36
Publisher page

Abstract

We study the stability of several diglyme-based electrolytes in sodium|sodium and sodium|graphite cells. The electrolyte behavior for different conductive salts [sodium trifluoromethanesulfonate (NaOTf), NaPF6, NaClO4, bis(fluorosulfonyl)imide (NaFSI), and sodium bis(trifluoromethanesulfonyl)imide (NaTFSI)] is compared and, in some cases, considerable differences are identified. Side reactions are studied with a variety of methods, including X-ray diffraction, scanning electron microscopy, transmission electron microscopy, online electrochemical mass spectrometry, and in situ electrochemical dilatometry. For Na|Na symmetric cells as well as for Na|graphite cells, we find that NaOTf and NaPF6 are the preferred salts followed by NaClO4 and NaFSI, as the latter two lead to more side reactions and increasing impedance. NaTFSI shows the worst performance leading to poor Coulombic efficiency and cycle life. In this case, excessive side reactions lead also to a strong increase in electrode thickness during cycling. In a qualitative order, the suitability of the conductive salts can be ranked as follows: NaOTf ≥ NaPF6 > NaClO4 > NaFSI ≫ NaTFSI. Our results also explain two recent, seemingly conflicting findings on the degree of solid electrolyte interphase formation on graphite electrodes in sodium-ion batteries [Maibach, J.; ACS Appl. Mater. Interfaces 2017, 9, 12373−12381; Goktas, M.; Adv. Energy Mater. 2018, 8, 1702724]. The contradictory findings are due to the different conductive salts used in both studies.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Technical Chemistry and Environmental Chemistry, Friedrich Schiller University Jena, Philosophenweg 7a, D-07743 Jena, Germany

Center for Energy and Environmental Chemistry Jena (CEEC Jena), Philosophenweg 7a, D-07743 Jena, Germany

Electrochemistry Laboratory, Paul Scherrer Institute (PSI), CH-5232 Villigen PSI, Switzerland

Department of Chemistry, Ångström Laboratory, Uppsala University, P.O. Box 538, SE-751 21 Uppsala, Sweden

CIC Energigune Parque Tecnológico, C/Albert Einstein, 48, 01510 Vitoria-Gasteiz, Álava, Spain

Department of Applied Chemistry, Tokyo University of Science, 1-3 Kagurazaka, Shinjuku, Tokyo 162-8061, Japan

Funding

Bundesministerium f?r Bildung und Forschung · Ministerio de Econom?a y Competitividad · Deutsche Forschungsgemeinschaft · Japan Science and Technology Agency

References (42)

Show source-provided references
1. 10.1002/anie.20170377210.1002/anie.201703772 ↗
2. 10.1002/aenm.20170303610.1002/aenm.201703036 ↗
3. 10.1002/anie.20141037610.1002/anie.201410376 ↗
4. 10.1039/c3ee40847g10.1039/c3ee40847g ↗
5. 10.1149/2.0151514jes10.1149/2.0151514jes ↗
6. 10.1002/aenm.20170046310.1002/aenm.201700463 ↗
7. 10.1021/cr500192f10.1021/cr500192f ↗
8. 10.1002/aenm.20160094310.1002/aenm.201600943 ↗
9. 10.1002/anie.20170377210.1002/anie.201703772 ↗
10. 10.1007/s41061-017-0168-x10.1007/s41061-017-0168-x ↗
11. 10.3762/bjnano.6.10510.3762/bjnano.6.105 ↗
12. 10.1039/C9CS00162J10.1039/C9CS00162J ↗
13. 10.1002/anie.20140373410.1002/anie.201403734 ↗
14. 10.1002/adfm.20140298410.1002/adfm.201402984 ↗
15. 10.1039/C6CP00651E10.1039/C6CP00651E ↗
16. 10.1039/C5EE02051D10.1039/C5EE02051D ↗
17. 10.1021/acs.jpcc.8b0791510.1021/acs.jpcc.8b07915 ↗
18. 10.1021/acs.nanolett.5b0418710.1021/acs.nanolett.5b04187 ↗
19. 10.1016/j.jpowsour.2015.05.11610.1016/j.jpowsour.2015.05.116 ↗
20. 10.1016/j.jpowsour.2016.01.08210.1016/j.jpowsour.2016.01.082 ↗
21. 10.1038/s41467-019-10551-z10.1038/s41467-019-10551-z ↗
22. 10.1021/acs.jpcc.6b1096210.1021/acs.jpcc.6b10962 ↗
23. 10.1021/acs.jpcc.8b0608910.1021/acs.jpcc.8b06089 ↗
24. 10.1016/j.nanoen.2017.03.01510.1016/j.nanoen.2017.03.015 ↗
25. 10.1002/aenm.20170272410.1002/aenm.201702724 ↗
26. 10.1021/acsami.6b1653610.1021/acsami.6b16536 ↗
27. 10.1016/j.jpowsour.2017.02.06510.1016/j.jpowsour.2017.02.065 ↗
28. 10.1021/acsaem.8b0036010.1021/acsaem.8b00360 ↗
29. 10.1016/j.electacta.2003.10.00910.1016/j.electacta.2003.10.009 ↗
30. 10.1021/acs.chemmater.7b0195310.1021/acs.chemmater.7b01953 ↗
31. 10.1021/acscentsci.5b0032810.1021/acscentsci.5b00328 ↗
32. 10.1021/acs.jpcc.6b0206110.1021/acs.jpcc.6b02061 ↗
33. 10.1039/C6CC05362A10.1039/C6CC05362A ↗
34. 10.1002/aenm.20160151910.1002/aenm.201601519 ↗
35. 10.1002/smtd.20180022710.1002/smtd.201800227 ↗
36. 10.1039/C3CP53077A10.1039/C3CP53077A ↗
37. 10.1149/2.0091513jes10.1149/2.0091513jes ↗
38. 10.1002/cssc.20190105610.1002/cssc.201901056 ↗
39. 10.1002/adma.20160666310.1002/adma.201606663 ↗
40. 10.1002/adfm.20190079010.1002/adfm.201900790 ↗
41. 10.1016/j.electacta.2019.03.03610.1016/j.electacta.2019.03.036 ↗
42. He, M. Elucidating Interface Reactions in Li-Ion Batteries and Supercapacitors by In Situ Gas Analysis. Doctoral Dissertation, Eidgenössische Technische Hochschule (ETH): Zürich, 2016.