Abstract

The aim of this work was to evaluate the effects of application time of an acid mixture solution on the surface roughness, phase transformation, and biaxial flexural strength of 3Y-TZP after sintering or air abrasion. For the biaxial flexural strength measurement, 220 3Y-TZP disk-shaped specimens were prepared after as-sintering or air abrasion. The etching solution comprised a mixture of hydrofluoric acid, sulfuric acid, hydrogen peroxide, methyl alcohol, and purified water. The samples were divided into 11 subgroups according to the etching times (Control, 1, 2, 3, 5, 8, 10, 12, 15, 20, and 30 min). The results showed that acid treatment on both as-sintered and air-abraded 3Y-TZP surfaces increased the surface roughness. However, it had no significant effects on the monoclinic phase or flexural strength of as-sintered zirconia. The monoclinic phase and flexural strength of air-abraded zirconia increased sharply after air abrasion; however, they gradually decreased after acid treatment, to a similar level to the case of the untreated surface. Surface treatment with acid mixture increased the roughness, but the lack of increase of monoclinic phase is thought to be because the loose monoclinic particles remaining on the surface were removed through the etching process.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Prosthodontics, Yonsei University College of Dentistry, 50-1 Yonsei-Ro, SeodaemunGu, Seoul 03722, Korea

CLF Dental Laboratory, 227 Moraenae-ro, Seodaemun Gu, Seoul 03695, Korea

Funding

the Yonsei University College of Dentistry Fund

References (55)

Show source-provided references
1. Applicability of zirconia dental prostheses for metal allergy patients
2. Has zirconia made a material difference in implant prosthodontics? A review10.1016/j.dental.2019.08.100 ↗
3. Cyclic fatigue in water of veneer-framework composites for all-ceramic dental bridges10.1016/j.dental.2006.01.011 ↗
4. Ageing kinetics and strength of airborne-particle abraded 3Y-TZP ceramics10.1016/j.dental.2017.04.014 ↗
5. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
6. Ceramics in restorative and prosthetic dentistry10.1146/annurev.matsci.27.1.443 ↗
7. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic10.1016/S0022-3913(08)60178-X ↗
8. Stabilized zirconia as a structural ceramic: An overview10.1016/j.dental.2007.05.005 ↗
9. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part II: Multiple-unit FDPs10.1016/j.dental.2015.02.013 ↗
10. Fatigue behavior of Y-TZP ceramic after surface treatments10.1016/j.jmbbm.2015.11.042 ↗
11. Adhesion/cementation to zirconia and other non-silicate ceramics: Where are we now?10.1016/j.dental.2010.10.022 ↗
12. Effects of alumina-blasting pressure on the bonding to super/ultra-translucent zirconia10.1016/j.dental.2019.02.025 ↗
13. The effect of nano-structured alumina coating on resin-bond strength to zirconia ceramics10.1016/j.dental.2010.03.013 ↗
14. An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface10.1016/S0022-3913(08)60286-3 ↗
15. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
16. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering ceramics10.1016/j.dental.2005.11.014 ↗
17. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
18. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic10.1016/j.jdent.2005.06.006 ↗
19. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
20. Aging of 3Y-TZP dental zirconia and yttrium depletion10.1016/j.dental.2017.07.011 ↗
21. Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
22. Thickness dependence of light transmittance, translucency and opalescence of a ceria-stabilized zirconia/alumina nanocomposite for dental applications10.1016/j.dental.2016.02.004 ↗
23. Y-TZP zirconia regeneration firing: Microstructural and crystallographic changes after grinding10.4012/dmj.2016-124 ↗
24. Hydrofluoric acid etching of dental zirconia. Part 1: Etching mechanism and surface characterization10.1016/j.jeurceramsoc.2015.09.021 ↗
25. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic10.1016/j.dental.2004.07.010 ↗
26. Effect of surface condition of dental zirconia ceramic (Denzir) on bonding10.4012/dmj.25.626 ↗
27. Air–particle abrasion on zirconia ceramic using different protocols: Effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
28. Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis10.1016/j.dental.2016.03.021 ↗
29. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
30. Optimal sandblasting conditions for conventional-type yttria-stabilized tetragonal zirconia polycrystals10.1016/j.dental.2018.11.009 ↗
31. Effect of etching with distinct hydrofluoric acid concentrations on the flexural strength of a lithium disilicate-based glass ceramic10.1002/jbm.b.33619 ↗
32. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: Conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
33. Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin10.1590/S1806-83242007000100002 ↗
34. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics10.1016/S0022-3913(02)52704-9 ↗
35. Resin-ceramic bonding: A review of the literature10.1067/mpr.2003.50 ↗
36. Effect of zirconia surface treatment using nitric acid-hydrofluoric acid on the shear bond strengths of resin cements10.4047/jap.2017.9.2.77 ↗
37. Dental zirconia can be etched by hydrofluoric acid10.4012/dmj.2013-243 ↗
38. In vitro short-term bonding performance of zirconia treated with hot acid etching and primer conditioning etching and primer conditioning10.4012/dmj.2013-010 ↗
39. Effects of different surface treatments on the cyclic fatigue strength of one-piece CAD/CAM zirconia implants10.1016/j.jmbbm.2018.05.002 ↗
40. Effect of extrinsic pigmentation and surface treatments on biaxial flexure strength after cyclic loading of a translucent ZrO2 ceramic10.1016/j.dental.2019.08.117 ↗
41. Effect of sandblasting and residual stress on strength of zirconia for restorative dentistry applications10.1016/j.jmbbm.2013.09.004 ↗
42. Improvement of mechanical properties of Y-TZP by thermal annealing with monoclinic zirconia nanoparticle coating10.1016/j.dental.2019.04.002 ↗
43. Influence of surface treatment of yttria-stabilized tetragonal zirconia polycrystal with hot isostatic pressing on cyclic fatigue strength10.4012/dmj.2012-247 ↗
44. Strength and reliability of surface treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
45. Xie, H., Shen, S., Qian, M., Zhang, F., Chen, C., and Tay, F.R. (2015). Effects of Acid Treatment on Dental Zirconia: An In Vitro Study. PLoS ONE, 10.10.1371/journal.pone.0136263 ↗
46. Depolymerization of microcrystalline cellulose to value added chemicals using sulfate ion promoted zirconia catalyst10.1016/j.biortech.2016.08.109 ↗
47. The effect of sulfate contents on the surface properties of iron–manganese doped sulfated zirconia catalysts10.1016/j.powtec.2013.12.045 ↗
48. Hydroxylation of dental zirconia surfaces: Characterization and bonding potential10.1002/jbm.b.31126 ↗
49. An in vitro comparison of shear bond strength of zirconia to enamel using different surface treatments10.1111/jopr.12075 ↗
50. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
51. Phase transformation and subsurface damage in 3Y-TZP after sandblasting10.1016/j.dental.2013.03.005 ↗
52. Zirconia changes after grinding and regeneration firing10.1016/j.prosdent.2016.09.026 ↗
53. Effect of thickness and surface modifications on flexural strength of monolithic zirconia10.1016/j.prosdent.2017.08.007 ↗
54. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
55. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗