journal article·2023-07-22Open access

Corrosion and Erosion Wear Behaviors of HVOF-Sprayed Fe-Based Amorphous Coatings on Dissolvable Mg-RE Alloy Substrates

Jun Yang, Yijiao Sun, Minwen Su, Xueming Yin, Hongxiang Li, Jishan Zhang

Materials· Volume 16· Issue 14

Abstract

To suppress the corrosion and erosion wear of dissolvable magnesium alloy ball seats in wellbores, Fe-based amorphous coatings were deposited on dissolvable Mg-RE alloy substrates, and their microstructure, corrosion behavior, and erosion wear behavior were studied. The thickness of Fe-based amorphous coatings on dissolvable Mg-RE alloy substrates can reach 1000 μm without any cracks, and their porosity and amorphous contents are 0.79% and 86.8%, respectively. Although chloride ions will damage the compactness and protective efficacy of passive films, Fe-based amorphous coatings still maintain low corrosion current density (3.31 μA/cm2) and high pitting potential (1 VSCE) in 20 wt% KCl solution. Due to their higher hardness, the erosion wear resistance of Fe-based amorphous coatings is about 4.16 times higher than that of dissolvable Mg-RE alloy substrates when the impact angle is 30°. Moreover, the erosion rates of Fe-based amorphous coatings exhibit a nonlinear relationship with the impact angle, and the erosion rate reaches the highest value when the impact angle is 60°. The erosion wear mechanisms of Fe-based AMCs vary with the impact angles, including cutting, delamination, splat fracture, and deformation wear. This work can provide effective guidance for the corrosion and wear protection of plugging tools made from dissolvable magnesium alloy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Engineering Laboratory for Exploration and Development of Low-Permeability Oil & Gas Fields, Xi’an 710018, China

Changqing Downhole Technology Company, Chuanqing Drilling Engineering Co., Ltd., Xi’an 710018, China

State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China

Funding

National Engineering Laboratory for Exploration and Development of Low-Permeability Oil and Gas Fields · National Natural Science Foundation of China · Key Scientific Research Project in Shanxi Province · “Dingxinbeike” Project

References (42)

Show source-provided references
1. A review on magnesium alloys for application of degradable fracturing tools10.1016/j.jma.2022.09.032 ↗
2. A review on shale oil and gas characteristics and molecular dynamics simulation for the fluid behavior in shale pore10.1016/j.molliq.2023.121507 ↗
3. Re-recognition of “unconventional” in unconventional oil and gas10.1016/S1876-3804(19)60244-2 ↗
4. Numerical simulation of the conveyance characteristics of fracturing ball in the horizontal section10.1016/j.jngse.2016.07.008 ↗
5. A new openhole multistage hydraulic fracturing system and the ball plug motion in a horizontal pipe10.1016/j.jngse.2017.11.019 ↗
6. Research on the effect of gas nitriding treatment on the wear resistance of ball seat used in multistage fracturing10.1016/j.matdes.2014.12.050 ↗
7. Sun, Y., Li, H., Yang, J., and Zhang, J. (2023). Effects of Temperature and Pressure on Corrosion Behavior of HVOF-Sprayed Fe-Based Amorphous Coating on the Mg-RE Alloy for Dissolvable Plugging Tools. Materials, 16.10.3390/ma16031313 ↗
8. Effect of trace Ni addition on microstructure, mechanical and corrosion properties of the extruded Mg–Gd–Y–Zr–Ni alloys for dissoluble fracturing tools10.1016/j.jma.2020.08.019 ↗
9. Finite element analysis and experimental study on the deformation characteristics of an aluminum alloy fracturing ball10.1016/j.jngse.2016.08.037 ↗
10. Numerical study on improving the erosion life of ball seat for oil and gas reservoir fracturing10.1016/j.engfailanal.2015.11.050 ↗
11. Cerium conversion coating and sol-gel coating for corrosion protection of the WE43 Mg alloy10.1016/j.corsci.2022.110527 ↗
12. Corrosion failure process of organic conductive coating on Mg-RE alloy with PEO in the simulated Xisha atmospheric solution10.1016/j.matchemphys.2022.126771 ↗
13. Enhancing the biodegradability and surface protective performance of AZ31 Mg alloy using polypyrrole/gelatin composite coatings with anodized Mg surface10.1016/j.surfcoat.2019.125139 ↗
14. Development of corrosion-resistant electroplating on AZ91 Mg alloy by employing air and water-stable eutectic based ionic liquid bath10.1016/j.surfcoat.2021.127881 ↗
15. Influence of biodegradable polymer coatings on corrosion, cytocompatibility and cell functionality of Mg-2.0Zn-0.98Mn magnesium alloy10.1016/j.colsurfb.2016.04.021 ↗
16. Corrosion resistance and chemical stability of super-hydrophobic film deposited on magnesium alloy AZ31 by microwave plasma-enhanced chemical vapor deposition10.1016/j.electacta.2010.06.064 ↗
17. Corrosion and wear resistance of micro-arc oxidation coating on glass microsphere reinforced Mg alloy composite10.1007/s10853-021-06252-y ↗
18. Wear behavior of HVOF sprayed WC coating under water-in-oil fracturing fluid condition10.1016/j.triboint.2017.05.002 ↗
19. Investigation on wear behaviour of SS 316L, atmospheric plasma and high velocity oxy-fuel sprayed WC-Cr3C2-Ni coatings for fracturing tools10.1016/j.surfcoat.2020.125679 ↗
20. Fe-based metallic glass coatings by thermal spraying: A focused review on corrosion properties and related degradation mechanisms10.1080/09506608.2022.2084670 ↗
21. Effect of hydrostatic pressure on the corrosion behavior of HVOF-sprayed Fe-based amorphous coating10.1016/j.jallcom.2018.05.100 ↗
22. Significantly enhanced resistance to SRB corrosion via Fe-based amorphous coating designed with high dose corrosion-resistant and antibacterial elements10.1016/j.corsci.2019.108305 ↗
23. Crystallization-dependent transition of corrosion resistance of an Fe-based bulk metallic glass under hydrostatic pressures10.1016/j.corsci.2020.109098 ↗
24. Slurry erosion–corrosion behaviour of high-velocity oxy-fuel (HVOF) sprayed Fe-based amorphous metallic coatings for marine pump in sand-containing NaCl solutions10.1016/j.corsci.2011.05.062 ↗
25. Effect of applied potential on passivation and erosion–corrosion of a Fe-based amorphous metallic coating under slurry impingement10.1016/j.corsci.2014.01.004 ↗
26. Determination of the critical flow velocities for erosion–corrosion of passive materials under impingement by NaCl solution containing sand10.1016/j.corsci.2014.07.043 ↗
27. Erosion–corrosion of HVOF-sprayed Fe-based amorphous metallic coating under impingement by a sand-containing NaCl solution10.1016/j.corsci.2013.07.006 ↗
28. Study on the effect of Ni60 transition coating on microstructure and mechanical properties of Fe/WC composite coating by laser cladding10.1016/j.optlastec.2023.109387 ↗
29. A dissolvable Mg-Gd-Y-Zn-Cu alloy possessing the highest yield strength for the fabrication of fracturing plugging tools10.1016/j.matlet.2023.134053 ↗
30. Effect of Cu micro-alloying on the microstructure, mechanical and corrosion properties of Mg-Gd-Y-Zn based alloy applied as plugging tools10.1016/j.jallcom.2023.168768 ↗
31. Synergistic Effect of Mo, W, Mn and Cr on the Passivation Behavior of a Fe-Based Amorphous Alloy Coating10.1007/s40195-017-0604-5 ↗
32. Influence of oxidation related structural defects on localized corrosion in HVAF-sprayed Fe-based metallic coatings10.1016/j.surfcoat.2017.12.038 ↗
33. Cr/GLC multilayered coating in simulated deep-sea environment: Corrosion behavior and growth defect evolution10.1016/j.corsci.2021.109528 ↗
34. Critical review on the passive film formation and breakdown on iron electrode and the models for the mechanisms underlying passivity10.1016/j.jelechem.2016.12.020 ↗
35. Niobium addition enhancing the corrosion resistance of nanocrystalline Ti5Si3 coating in H2SO4 solution10.1016/j.actamat.2013.10.040 ↗
36. Role of passive film in dominating the electrochemical corrosion behavior of FeCrMoCBY amorphous coating10.1016/j.jallcom.2019.151962 ↗
37. Electrochemical and XPS analytical investigation of the accelerative effect of bicarbonate/carbonate ions on AISI 304 in alkaline environment10.1016/j.apsusc.2019.06.198 ↗
38. Electrochemical behaviors and passive film properties of Fe-based bulk metallic glass in Cl−-containing acetic acid solutions under high temperature10.1016/j.jallcom.2018.07.029 ↗
39. The semiconductor properties of passive films and corrosion behavior of stainless steel reinforcing bars in simulated concrete pore solution10.1016/j.mtla.2019.100321 ↗
40. Effect of Cl− on the Properties of the Passive Films Formed on 316L Stainless Steel in Acidic Solution10.1016/j.jmst.2013.07.010 ↗
41. Interfacial bonding and corrosion behaviors of HVOF-sprayed Fe-based amorphous coating on 8090 Al-Li alloy10.1016/j.surfcoat.2022.128316 ↗
42. Effect of microwave exposure time on microstructure and slurry erosion behavior of Ni + 20% Cr7C3 composite clads10.1016/j.wear.2018.12.016 ↗