Texture and High Yield Strength of Rapidly Solidified AZ31 Magnesium Alloy Extruded at 250 °C

Peiran Ye, Chao Yang, Zhenshuai Li, Shuai Bao, Yuchu Sun, Wucheng Ding, Yungui Chen

Abstract

In this study, commercial AZ31B magnesium alloy was used to compare the differences between the microstructure, texture, and mechanical properties of conventional solidification (as homogenized AZ31) and rapid solidification (as RS AZ31). The results demonstrate that a rapidly solidified microstructure leads to better performance after hot extrusion with a medium extrusion rate (6 m/min) and extrusion temperature (250 °C). The average grain size of as-homogenized AZ31 extruded rod is 100 μm after annealing and 4.6 μm after extrusion, respectively, but that of the as-RS AZ31 extruded rod is only about 5 μm and 1.1 μm, correspondingly. The as-RS AZ31 extruded rod attains a high average yield strength of 289.6 MPa, which is superior to the as-homogenized AZ31 extruded rod, and is improved by 81.3% in comparison. The as-RS AZ31 extruded rod shows a more random crystallographic orientation and has an unconventional weak texture component in <112¯1>/<202¯1> direction, which has not been reported yet, while the as-homogenized AZ31 extruded rod has an expected texture with prismatic <101¯0>/<1¯21¯0>//ED.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.