Abstract

Glass fibers are widely used in cement-based precast products, given the reinforcing requirements for toughness and strength. However, inferior alkali resistance hinders the effectiveness of glass fibers in reinforcing cement-based materials. In this paper, nanoparticle coatings were applied on the surface of alkali-resistant glass fiber (ARGF) as a protective layer via the in situ chemical reaction of oleic acid (OA) and potassium permanganate (PP). The morphology and constituents of the as-prepared ARGFs were examined using scanning electron microscopy (SEM) and obtaining X-ray photoelectron spectroscopy (XPS) measurements. Mass loss and strength retention were investigated to characterize alkali resistance of modified ARGFs. Results showed that ARGFs could be optimally coated by a layer of MnO2-based nanoparticles consisting of approximately 70% MnO2, 18% MnO, and 12% MnSiO3, when modified with an optimum OA to PP ratio of 10 for 24 h. The dissolution of ARGFs matrix in 4% and 10% NaOH solutions were distinctly delayed to 28 d, as a consequence of the introduction of the MnO2-based nanoparticle layer, compared with nontreated ARGF occurring at 3 d in 4% NaOH solution. For the optimally modified ARGFs, the mass loss was controlled to 1.76% and 2.91% after 90 d of corrosion in 4% and 10% NaOH solutions, and the retention of tensile strength was increased by approximately 25%. With respect to the increment in alkali-resistant performance, the modified ARGFs can be promising candidates for wide applications in alkaline cement-based products.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Innovative concrete reinforcement materials · Concrete and Cement Materials Research · Smart Materials for Construction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

China United Cement Pingyi, Co., Ltd., Linyi 276000, China

Shandong Provincial Key Laboratory of Preparation and Measurement of Building Materials, University of Jinan, Jinan 250022, China

Funding

National Natural Science Foundation of China · Shandong Natural Science Foundation Project · Science and Technology Project of University of Jinan

References (27)

Show source-provided references
1. Effect of alkali-resistant glass fiber and silica fume on mechanical and shrinkage properties of cement-based mortars10.1016/j.conbuildmat.2021.125054 ↗
2. Influence of alkali-resistant glass fiber on seismic performance of precast ceramsite concrete sandwich wall panels10.1016/j.istruc.2022.01.081 ↗
3. Investigation on the alkali resistance of basalt fiber and its textile in different alkaline environments10.1016/j.conbuildmat.2020.121670 ↗
4. Multiscale Homogenization Analysis of Alkali-Silica Reaction (ASR) Effect in Concrete10.1016/j.eng.2019.02.007 ↗
5. Alkali Durability of Oxynitride Glass Fibers10.1111/j.1151-2916.1991.tb06909.x ↗
6. Effect of mental oxide on the structure and property of rare earth doped glass10.1088/1755-1315/565/1/012061 ↗
7. Nanostructured coatings of glass fibers: Improvement of alkali resistance and mechanical properties10.1016/j.actamat.2006.09.020 ↗
8. Environmental resistance and mechanical performance of alkali-resistant glass fibers with surface sizings10.1016/S0022-3093(03)00330-2 ↗
9. Effect of TiO2 on preparation condition, mechanical properties and alkali resistance of continuous basalt fibers10.1016/j.cemconcomp.2022.104861 ↗
10. Performance of Alkali-Resistant Glass Fibers Modified with Refused Coal Ore10.2320/matertrans.M2016321 ↗
11. Zr-rich basalt continuous fibers with increased alkali resistant properties10.1016/j.conbuildmat.2021.123089 ↗
12. Low-cost glass fiber composites with enhanced alkali resistance tailored towards concrete reinforcement10.1016/j.conbuildmat.2013.03.055 ↗
13. Effect of Different Constituent Fiber, Resin, and Sizing Combinations on Alkaline Resistance of Basalt, Carbon, and Glass FRP Bars10.1061/(ASCE)CC.1943-5614.0001009 ↗
14. Investigation of surface modification and volume content of glass and carbon fibres from fibre reinforced polymer waste for reinforcing concrete10.1016/j.jhazmat.2019.121797 ↗
15. Study on the durability of GFRP bars and carbon/glass hybrid fiber reinforced polymer (HFRP) bars aged in alkaline solution10.1016/j.compstruct.2020.113285 ↗
16. Nanocomposite coatings for healing surface defects of glass fibers and improving interfacial adhesion10.1016/j.compscitech.2007.10.009 ↗
17. Moisture barrier characteristics of organoclay-epoxy nanocomposites10.1016/j.compscitech.2004.10.014 ↗
18. Moisture diffusion through vinyl ester nanocomposites made with montmorillonite clay10.1002/pen.11078 ↗
19. Silica coating for interphase bond enhancement of carbon and AR-glass Textile Reinforced Mortar (TRM)10.1016/j.compositesb.2017.12.045 ↗
20. Carbon fibre surface modification using functionalized nanoclay: A hierarchical interphase for fibre-reinforced polymer composites10.1016/j.compscitech.2017.05.013 ↗
21. Failure mechanism of silica coated polypropylene fibres for Fibre Reinforced Concrete (FRC)10.1016/j.conbuildmat.2019.117549 ↗
22. Improved mechanical properties of the E-glass fibres through TiO2 nanoparticle coating10.1080/02670836.2022.2164817 ↗
23. Micro- and nanoparticle mineral coating for enhanced properties of carbon multifilament yarn cement-based composites10.1016/j.compositesb.2016.12.005 ↗
24. Lime-cement textile reinforced mortar (TRM) with modified interphase
25. (2012, September 15). Measurement Services Division of the National Institute of Standards and Technology of America, Available online: https://srdata.nist.gov/xps/selEnergyType.aspx.
26. Inhibition of Charge Disproportionation of MnO2 Electrocatalysts for Efficient Water Oxidation under Neutral Conditions10.1021/ja306499n ↗
27. Alkali-silica reaction in concrete containing glass10.1617/s11527-008-9465-8 ↗