Abstract
To improve the service life and reduce the repair cost of continuous casting rollers, a new welding-hammering hybrid remanufacturing process in which the roller was designed with a gradient structure was proposed, and corresponding equipment was developed. First, the failure modes and their causes for a continuous casting roller were analyzed by numerical simulation. The cyclic tension–compression shear stress, cyclic tension–compression normal stress, thermal cycle, and highly corrosive environment caused fatigue cracking and overall peeling of the roller surface. Second, the gradient structure composed of a base layer, transition layer, and strengthened layer of a continuous casting roller was designed, and materials for each layer were selected according to their different service conditions. Third, novel equipment for continuous welding-hammering composite remanufacturing was developed, and the optimized process parameters were obtained through welding experiments. Finally, an application test was carried out; the microscopic analysis showed that refined grains, fewer welding defects, and better surface toughness were obtained. Compared with traditional remanufacturing processes without hammering, the welding-hammering hybrid process achieved a forged structure instead of as-cast structure, which significantly improved the service life of the continuous casting roller by about 100%.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chongqing Key Laboratory of Advanced Mold Intelligent Manufacturing, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China
Chongqing Jiepin Technology Co., Ltd., Chongqing 400000, China
Funding
Chongqing Special Fund for Post-doctoral Program · National Natural Science Foundation of China
References (25)
Show source-provided references
1. Research of Surfacing Technology on Continuous Casting Roller
2. The Role of Laser Additive Manufacturing Methods of Metals in Repair, Refurbishment and Remanufacturing–Enabling Circular Economy10.1016/j.phpro.2016.08.077 ↗
3. Microstructures and abrasive wear performance of PTAW deposited Ni–WC overlays using different Ni-alloy chemistries10.1016/j.wear.2011.10.001 ↗
4. Microstructure and wear properties of nickel-based surfacing deposited by plasma transferred arc welding10.1016/j.surfcoat.2012.05.125 ↗
5. Influence of welding parameters on microstructure and wear behaviour of a typical NiCrBSi hardfacing alloy reinforced with tungsten carbide10.1016/j.surfcoat.2008.06.185 ↗
6. Laser cladding of Inconel 690 on Inconel 600 superalloy for corrosion protection in nuclear applications10.1016/j.optlaseng.2012.08.006 ↗
7. A comparison of the abrasive wear behaviour of iron-chromium based hardfaced coatings deposited by SMAW and electric arc spraying10.1016/j.wear.2007.04.008 ↗
8. Microstructure and mechanical properties of additive manufactured W-Ni-Fe-Co composite produced by selective laser melting10.1016/j.ijrmhm.2019.105111 ↗
9. Kołodziejczak, P., Golański, D., Chmielewski, T., and Chmielewski, M. (2021). Microstructure of Rhenium Doped Ni-Cr Deposits Produced by Laser Cladding. Materials, 14.10.3390/ma14112745 ↗
10. Kołodziejczak, P., Bober, M., and Chmielewski, T. (2022). Wear Resistance Comparison Research of High-Alloy Protective Coatings for Power Industry Prepared by Means of CMT Cladding. Appl. Sci., 12.10.3390/app12094568 ↗
11. Numerical Simulation of Hardfacing Remanufacturing for Large-Scale Damaged Grinding Roller10.1007/s00170-021-08073-4 ↗
12. Influence of welding technique and temperature on fatigue properties of steel deposited with Co-based alloy hardfacing coating
13. Characterization of boride-rich hardfacing on carbon steel by arc spray and GMAW processes10.1016/j.surfcoat.2010.02.028 ↗
14. Weld procedural effect on the performance of iron based hardfacing deposits on cast iron substrate10.1016/j.jmatprotec.2005.10.025 ↗
15. Influence of aging treatment on microstructure, wear and corrosion behavior of a nickel base hardfaced coating10.1016/j.wear.2011.05.041 ↗
16. The effect of nano-additives containing rare earth oxides on sliding wear behavior of high chromium cast iron hardfacing alloys10.1016/j.triboint.2016.06.041 ↗
17. Effect of nitrogen alloying on the microstructure and abrasive impact wear resistance of Fe-Cr-C-Ti-Nb hardfacing alloy10.1016/j.surfcoat.2016.10.029 ↗
18. Effect of rare earth oxide nano-additives on micro-mechanical properties and erosion behavior of Fe-Cr-C-B hardfacing alloys10.1016/j.jallcom.2016.08.323 ↗
19. Fe–24 wt.%Cr–4.1 wt.%C hardfacing alloy: Microstructure and carbide refinement mechanisms with ceria additive10.1016/j.matchar.2012.07.004 ↗
20. Lesiuk, G., Smolnicki, M., Rozumek, D., Krechkovska, H., Student, O., Correia, J., Mech, R., and De Jesus, A. (2020). Study of the fatigue crack growth in long-term operated mild steel under mixed-mode (I+II, I+III) loading conditions. Materials, 13.10.3390/ma13010160 ↗
21. Residual stress determination in a dissimilar weld overlay pipe by neutron diffraction10.1016/j.msea.2011.07.059 ↗
22. Experimental determination of the residual stresses in a spiral weld overlay tube10.1016/S0921-5093(97)00089-0 ↗
23. Degradation of renovation layers deposited on continuous steel casting rollers by submerged arc welding10.1177/0954405413493405 ↗
24. A comparison study on wear characteristics of Ni-based, Co-based and Fe-based alloys for heated hot stamping tools manufactured by surfacing technology10.1007/s00170-019-04888-4 ↗
25. Direct measurement of the residual stresses near a ‘boat-shaped’ repair in a 20 mm thick stainless steel tube butt weld10.1016/j.ijpvp.2004.08.007 ↗