journal article·2020-04-30Open access

Characterizing Micromechanical Properties of Friction Welding Interface between TiAl Alloy and GH3039 Superalloy

Suigeng Du, Songlin Wang, Wanting Xu

Materials· Volume 13· Issue 9

Abstract

To explore the macro-fracture mechanism of a friction welded joint between TiAl alloy and GH3039 superalloy, the micromechanical properties of intermediate phases at the joint interface are characterized and the relationship between the macro-fracture and micro-fracture of the joint is established. The indentation technique has been employed to calculate the nano-hardness and fracture toughness of the intermediate phases. The dynamic in-situ tensile test in SEM has been applied to observe the initiation and propagation process of cracks at the interface. It has been found that Al3NiTi2 and AlNi2Ti have the highest nano-hardness and elastic recovery rates, while TiAl and GH3039 base metals have the lowest nano-hardness and elastic recovery rates. This indicates that the harder the materials, the more prone they are to elastic deformation. Nevertheless, the fracture toughness of Al3NiTi2 and AlNi2Ti are the two lowest, which were 1.7 MPa·m1/2 and 2.7 MPa·m1/2, respectively. The cracks sprouted from Al3NiTi2 and AlNi2Ti and then spread throughout the entire intermediate phase zone. In other words, the fracture mainly happened in these two phase layers. It has been concluded that Al3NiTi2 and AlNi2Ti were the two weakest phases at the interface and their poor fracture toughness results in low joint strength.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory of High Performance Manufacturing for Aero Engine, School of Mechanical Engineering, Northwestern Polytechnical University, Xi’an 710072, China

Funding

National Natural Science Foundation of China

References (28)

Show source-provided references
1. Microstructure and mechanical properties of vacuum diffusion bonding joints for γ-TiAl based alloy10.1016/j.vacuum.2018.01.035 ↗
2. A novel continuous and controllable method for fabrication of as-cast TiAl alloy10.1016/j.jallcom.2019.03.050 ↗
3. The transient liquid phase bonding process of a γ-TiAl alloy with brazing solders containing Fe or Ni10.1016/j.intermet.2018.12.004 ↗
4. Microstructure characteristics and mechanical properties of laser-welded joint of γ-TiAl alloy with pure Ti filler metal10.1016/j.optlastec.2017.07.011 ↗
5. CuTiNiZrV Amorphous Alloy Foils for Vacuum Brazing of TiAl Alloy to 40Cr Steel10.1016/j.jmst.2014.04.003 ↗
6. Interface structure and mechanical properties of the TiAl/42CrMo steel joint vacuum brazed with Ag-Cu/Ti/Ag-Cu filler metal10.1016/j.scriptamat.2006.03.055 ↗
7. Du, S., Wang, S., and Ding, K. (2020). A novel method of friction-diffusion welding between TiAl alloy and GH3039 high temperature alloy. J. Manuf. Process., under review.10.1016/j.jmapro.2020.05.046 ↗
8. Characterization of material property variation across an inertia friction welded CrMoV steel component using the inverse analysis of nanoindentation data10.1016/j.ijmecsci.2016.01.023 ↗
9. Size effect and strain induced double twin by nanoindentation in DSS weld metal of vibration-assisted GTAW10.1016/j.matchemphys.2018.07.055 ↗
10. Nanoindentation study on micromechanical behaviors of Au–Ni–Sn intermetallic layers in Au–20Sn/Ni solder joints10.1016/j.msea.2015.11.099 ↗
11. Double side friction stir welding of AA6082 sheets: Microstructure and nanoindentation characterization10.1016/j.msea.2013.10.031 ↗
12. Nanoindentation and microstructure analysis of Ti/Fe dissimilar joint10.1016/j.matlet.2018.11.152 ↗
13. A comparison between fracture toughness at different locations of SMAW and GTAW welded joints of primary coolant piping10.1016/j.engfracmech.2018.09.021 ↗
14. Microstructure and high temperature fracture toughness of NG-TIG welded Inconel 617B superalloy10.1016/j.jmst.2019.07.021 ↗
15. Measurement of fracture toughness by nanoindentation methods: Recent advances and future challenges10.1016/j.cossms.2015.04.003 ↗
16. Nanomechanical properties of additively and traditionally manufactured nickel-chromium-based superalloys through instrumented nanoindentation10.1016/j.mfglet.2019.09.003 ↗
17. Fracture toughness of WC-Fe cermet in W-WC-Fe composite by nanoindentation10.1016/j.jallcom.2017.09.070 ↗
18. Fracture toughness of carbides in tool steels evaluated by nanoindentation10.1016/j.actamat.2007.03.028 ↗
19. Investigation of microstructure and fracture toughness of Fe-Zr welded joints10.1016/j.matlet.2018.08.038 ↗
20. In-situ micro-tensile testing of AA2024-T3 fibre laser welds with digital image correlation as a function of welding speed
21. Evaluation of the microstructure related strength of CrMoV weldment by using the in-situ tensile test of miniature specimen10.1016/j.msea.2018.08.099 ↗
22. In situ investigation of the tensile deformation of laser welded Ti2AlNb joints10.1016/j.matchar.2016.11.009 ↗
23. Characteristics of reaction phases and effects of phases on mechanical properties of TiAl/42CrMo steel brazed joint
24. A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack Measurements10.1111/j.1151-2916.1981.tb10320.x ↗
25. Generalized means as an approach for predicting Young’s moduli of multiphase materials10.1016/j.msea.2003.09.066 ↗
26. Hardness and friction coefficient of fused silica under scratching considering elastic recovery10.1016/j.ceramint.2019.12.048 ↗
27. A different type of indentation size effect10.1016/j.scriptamat.2008.07.026 ↗
28. Effects of brazing filler on properties of brazed joints between TiAl and metallic materials10.1016/S0966-9795(00)00129-1 ↗