Structure and Phase State of Ti49.4Ni50.6 (at%) Hydrogenated in Normal Saline

В. Н. Гришков, А. И. Лотков, Dorzhima Zhapova, Yu. P. Mironov, Victor Timkin, E. G. Barmina, Olga Kashina

Abstract

The paper analyzes the surface structure and phase state of Ti49.4Ni50.6 (at%) hydrogenated at 295 K in normal saline (0.9% NaCl aqueous solution with pH = 5.7) at 20 A/m2 for 0.5–6 h. The analysis shows that the average hydrogen concentration in the alloy increases with the hydrogenation time tH as follows: slowly to 50 ppm at tH = 0.5–1.5 h, steeply to 150 ppm at tH = 1.2–2 h, and linearly to 300 ppm at tH = 2–6 h. According to Bragg–Brentano X-ray diffraction data (θ–2 θ, 2 θ ≤ 50°, CoKα radiation), the alloy in its scanned surface layer of thickness ~5.6 µm reveals a TiNiHx phase with x = 0.64 and x = 0.54 after hydrogenation for 4 and 6 h, respectively. The structure of this phase is identifiable as an orthorhombic hydride similar to β1–TiFeH0.94 (space group Pmcm), rather than as a tetragonal TiNiHx hydride with x = 0.30–1.0 (space group I4/mmm). Time curves are presented to trace the lattice parameters and volume change during the formation of such an orthorhombic phase from the initial cubic B2 phase in Ti49.4Ni50.6 (at%).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen Storage and Materials · Titanium Alloys Microstructure and Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.