The Corrosion Susceptibility of 304L Stainless Steel Exposed to Crevice Environments
Source abstract
Abstract
The present study focuses on the corrosion behavior of 304L stainless steel in crevice corrosion environments. The specimen with a salt deposit of 0.1 g/m2 was assembled with a crevice former made of Poly-tetra fluoroethylene (PTFE) to make a test device. The assembled test devices were kept at the ambient temperature of 45 °C in combination with a relative humidity of 45%, 55%, and 70%. After testing for 5000 h, the corroded area of the specimen exposed to 70% humidity was three times larger than that subjected to 45% humidity. For the specimen sustaining a tensile force, the crack growth rate was approximately 1.4 mm/year at the stress level of 300 MPa in a crevice corrosion environment with 0.1 g/m2 of sea salt deposited on the surface. The small portion of intergranular cracking occurred at the surface due to the existed strain on the surface. As cracks propagate in a grain, the grain undergoes a greater localized deformation, and some secondary cracks would develop inside the grain; transgranular cracking was vigorous due to the path corrosion that nucleated at the slip steps.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.