Enhanced Properties of Tailored Alumina–Magnesia-Based Dry Ramming Mixes by Calcium Magnesium Aluminate (CMA)
Source abstract
Abstract
To achieve the goal of “dual-carbon”, induction furnaces with high efficiency and energy-saving advantages are paid more attention in the foundry and metallurgy industries. The service life and safety of induction furnaces strongly depended on the lining because expansion and forward sintering could result in the erosion and slag resistance of the lining. Focusing on the tailoring properties of alumina–magnesia-based dry ramming mixes, calcined magnesia particles were replaced with the novel multi-component materials of calcium magnesium aluminate (CaO-MgO-Al2O3, CMA) with a size of 200 mesh. Properties such as the bulk density, apparent porosity, strength, and slag corrosion resistance of alumina–magnesia-based dry ramming mix containing CMA were evaluated contrastively. The results demonstrate that the penetration index of manganese-bearing slag in dry ramming mixes first decreased and then slightly increased with the addition of CMA. Meanwhile, the permanent linear change in dry ramming mixes was gradually reduced. When the addition of CMA reached 4 wt%, the strength of the dry ramming mixes was slightly greater than the reference, and the slag penetration index was just 75% of the latter.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Materials Engineering and Processing · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China
Hubei Annaijie Lining Materials Co., Ltd., Xiangyang 441100, China
National-Provincial Joint Engineering Research Center of High Temperature Materials and Lining Technology, Wuhan University of Science and Technology, Wuhan 430081, China
References (49)
Show source-provided references
1. Influence of α-Al2O3 micropowder addition on properties of corundum dry ramming mix
2. Schacht, C.A. (2004). Refractories Handbook, Marcel Dekker, Inc.10.1201/9780203026328 ↗
3. Morphology and luminescence of MgAl2O4 ceramics obtained via spark plasma sintering10.1016/j.ceramint.2019.01.137 ↗
4. Distinctive features of diffusion-controlled radiation defect recombination in stoichiometric magnesium aluminate spinel single crystals and transparent polycrystalline ceramics10.1038/s41598-020-64778-8 ↗
5. Behaviour of spinel-forming DVM using crucible induction furnaces. A case study on material failure10.1016/j.ceramint.2016.03.163 ↗
6. Routschka, G. (2004). Pocket Manual Refractory Materials, Vulkan-Verlag GmbH.10.1002/3527600434.eap392 ↗
7. Basic slag attack of spinel-containing refractory castables10.1016/j.ceramint.2011.02.007 ↗
8. From macro to nanomagnesia: Designing the in situ spinel expansion10.1111/j.1551-2916.2008.02566.x ↗
9. Fundamentals and applications on in situ spinel formation mechanisms in Al2O3-MgO refractory castables10.1016/j.ceramint.2011.10.074 ↗
10. Effect of pre-synthesized spinel addition on alumina-magnesia dry vibration mix
11. Influence of spinel micropowder on properties of alumina-magnesia dry ramming mixes
12. Synthesis and densification of magnesium aluminate spinel: Effect of MgO reactivity10.1016/S0272-8842(03)00036-1 ↗
13. The impact of pre-formed and in situ spinel formation on the physical properties of cement-bonded high alumina refractory castables10.1016/j.ceramint.2010.04.005 ↗
14. Alumina-spinel castable for steel ladles: An overview10.1111/ijac.14213 ↗
15. Ternary system Al2O3-MgO-CaO: Part II, phase relationships in the subsystem Al2O3-MgAl2O4-CaAl4O710.1111/j.1151-2916.2000.tb01295.x ↗
16. Effect of TiO2 addition on the sintering densification and mechanical properties of MgAl2O4-CaAl4O7-CaAl12O19 composite10.1016/j.ceramint.2016.03.082 ↗
17. CA6 impact on the corrosion behavior of cement-bonded spinel-containing refractory castables: An analysis based on thermodynamic simulations10.1016/j.ceramint.2014.12.020 ↗
18. Corrosion mechanism of a density-reduced steel ladle lining containing porous spinel-calcium aluminate aggregates10.3390/ceramics3010015 ↗
19. Tang, H., Li, C., Gao, J., Touzo, B., Liu, C., and Yuan, W. (2021). Optimization of properties for alumina-spinel refractory castables by CMA (CaO-MgO-Al2O3) aggregates. Materials, 14.10.3390/ma14113050 ↗
20. Aneziris, C.G., and Gehre, P. (2016, January 28–29). Effects of magnesium aluminate spinel raw materials on the material properties of MgO-C refractories. Proceedings of the International Colloquium on Refractories, Aachen, Germany.
21. Corrosion mechanism of MgO-CMA-C ladle brick with high service life10.1002/srin.201900436 ↗
22. (2010). Refractories Standard Compilation, Standards Press of China. [4th ed.].
23. (2010). Refractories Standard Compilation, Standards Press of China. [4th ed.].
24. (2010). Refractories Standard Compilation, Standards Press of China. [4th ed.].
25. (2010). Refractories Standard Compilation, Standards Press of China. [4th ed.].
26. Spinel-containing alumina-based refractory castables10.1016/j.ceramint.2011.03.049 ↗
27. Thermomechanical properties and fracture mechanisms of calcium hexaluminate10.1016/S0955-2219(00)00274-0 ↗
28. Tailoring the microstructure of cement-bonded alumina-magnesia refractory castables10.1111/j.1551-2916.2010.03956.x ↗
29. Effects of TiO2 addition on the expansion behavior of alumina-magnesia refractory castables10.1016/j.matchemphys.2015.06.047 ↗
30. Effect of alumina content on the crystal structure, lattice thermal expansion and thermal conductivity of aluminium-rich spinel solid solutions10.1016/j.matchemphys.2022.126366 ↗
31. Corrosion of high alumina and near stoichiometric spinels in iron-containing silicate slags10.1016/S0955-2219(02)00170-X ↗
32. High-pressure synchrotron X-ray diffraction and Raman spectroscopic study of plumbogummite10.1088/1674-1056/27/1/017402 ↗
33. Pressure effects on phase equilibria and solid solubility in MgO-Y2O3 nanocomposites10.1063/1.3691219 ↗
34. Phase transformations in hypereutectic MgO-Y2O3 nanocomposites at 5.5 GPa10.1063/1.4807913 ↗
35. Temperature dependence of the inversion degree in three-cation spinel solid solutions: Experimental evaluation by XRD10.1017/S0885715615000093 ↗
36. Structure-reactivity study of mechanically activated zinc ferrite10.1006/jssc.1996.0157 ↗
37. Equilibrium order-disorder in spinels10.1111/j.1151-2916.1967.tb15002.x ↗
38. Spectroscopic study of ordering in non-stoichiometric magnesium aluminate spinel10.2138/am-2015-5266 ↗
39. Mordekovitz, Y., Shoval, Y., Froumin, N., and Hayun, S. (2020). Effect of structure and composition of non-stoichiometry magnesium aluminate spinel on water adsorption. Materials, 13.10.3390/ma13143195 ↗
40. The properties characterization and strengthening-toughening mechanism of Al2O3-CA6-MA-Ni multi-phase composites prepared by adding calcined dolomite10.1016/j.matchar.2022.111810 ↗
41. Novel calcium hexaluminate/spinel-alumina composites with graded microstructures and mechanical properties10.1038/srep04333 ↗
42. Self-reinforced Ca-hexaluminate/alumina composites with graded microstructures10.1016/j.ceramint.2006.10.001 ↗
43. Biswas, S., and Sarkar, D. (2020). Introduction to Refractories for Iron-and Steelmaking, Springer.10.1007/978-3-030-43807-4 ↗
44. Reaction behavior of slag and spinel in steel ladle castables10.2109/jcersj2.119.595 ↗
45. The corrosion and microstructure relationship for cement-bonded spinel refractory castables10.1016/j.ceramint.2011.10.061 ↗
46. Time-resolved high-temperature X-ray diffraction for studying the kinetics of corrosion of high-alumina refractory by molten oxides10.1016/j.corsci.2018.05.003 ↗
47. Effects of MnO on slag viscosity and wetting behaviour between slag and refractory10.1179/1743281215Y.0000000048 ↗
48. Corrosion mechanism of MgAl2O4-CaAl4O7-CaAl12O19 composite by steel ladle slag: Effect of additives10.1016/j.jeurceramsoc.2017.02.025 ↗
49. Improvement of densification and mechanical properties of MgAl2O4-CaAl4O7-CaAl12O19 composite by addition of MnO10.1016/j.ceramint.2016.12.091 ↗