Microstructure-Dependent Corrosion Behavior of Ferritic–Martensitic 17Cr Stainless Steel in CO2-Saturated Brine at 230 °C Under High Pressure

Song He, Zhile Yang, Xuesong Xing, Weiru Zheng, Xijin Xing, Xiaoqi Yue

Abstract

The corrosion behavior of ferritic–martensitic 17Cr stainless steel in CO2-saturated brine was investigated using static autoclave immersion tests in 4.12 wt% NaCl solution at 230 °C under CO2 partial pressures of 6.36, 18.28, and 24.57 MPa. The calculated in situ pH values obtained using the OLI System were 3.79, 3.55, and 3.49, respectively. Corrosion morphology, microstructural evolution, and corrosion products were characterized by SEM, EDS, EBSD, and Raman spectroscopy. The average mass-loss corrosion rate increased from 0.138 ± 0.0221 mm/year at 6.36 MPa pCO2 to 0.326 ± 0.0142 mm/year at 24.57 MPa pCO2. Although the specimens did not show severe macroscopic pitting, localized attack preferentially occurred in fine-grained martensitic banded regions. EBSD analysis revealed that these regions exhibited higher local misorientation and defect density, which may reduce the stability of Cr-rich surface films. Raman spectra identified Cr(OH)3 in the corrosion products, and the Cr(OH)3 signal became more evident with increasing CO2 partial pressure. The results indicate that, under fixed temperature and salinity, the corrosion behavior of 17Cr stainless steel is governed by CO2 partial pressure and microstructural heterogeneity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.