Investigation of Microstructure, Hardness, and Wear Behavior of Hardfacing Produced by Wire Laser Additive Manufacturing
Source abstract
Abstract
Wire Laser Additive Manufacturing (WLAM) has emerged as a promising alternative for the fabrication and repair of components subjected to severe wear conditions due to its high deposition rate, efficient material utilization, and localized thermal control. In this study, the WLAM process using DUR600 wire as the feedstock material for the deposition of abrasion-resistant coatings was investigated. The deposited specimens were characterized by optical emission spectroscopy (OES), X-ray diffraction (XRD), optical microscopy (OM), scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (SEM/EDS), Vickers microhardness testing, and dry sand/rubber wheel abrasion testing in accordance with ASTM G65. The deposits exhibited a predominantly martensitic microstructure with retained austenite, as confirmed by XRD. Hardness values ranged from 749 to 817 HV, with an average of 783 ± 18 HV, while the average volumetric loss in the abrasive wear test was 150.26 mm3. This behavior was attributed to the presence of the martensitic matrix and retained austenite, whose combined effect directly influences the tribological performance of WLAM coatings produced using DUR600 wire.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Additive Manufacturing, Centro Universitário SATC, Criciúma 88805-380, Brazil
Department of Materials Engineering, Federal University of Santa Catarina (UFSC), Florianópolis 88040-900, Brazil
Department of Mining, Metallurgical and Materials Engineering, Federal University of Rio Grande do Sul (UFRGS), Porto Alegre 91501-970, Brazil
Funding
Fundação de Amparo à Pesquisa e Inovação do Estado de Santa Catarina
References (100+)
Show source-provided references
1. Gibson, I., Rosen, D., and Stucker, B. (2015). Additive Manufacturing Technologies: 3D Printing, Rapid Prototyping, and Direct Digital Manufacturing, Springer. [2nd ed.].10.1007/978-1-4939-2113-3 ↗
2. Metal Additive Manufacturing: A review10.1007/s11665-014-0958-z ↗
3. Processo de fabricação de peças metálicas por manufatura aditiva com fusão localizada de aços baixa liga
4. Optical emission spectroscopy for in-line control of laser additive manufacturing with metal wire of titanium–nickelide and magnesium alloys10.1007/s11082-025-08507-3 ↗
5. Current research status and prospect of laser wire additive manufacturing technology10.1007/s00170-025-15228-0 ↗
6. Manufatura aditiva por fusão localizada de arame ER70S-610.70185/2525-6025.2025.v10.457 ↗
7. Additive manufacturing of metallic components—Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
8. Laser additive manufacturing of metallic components: Materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
9. Additive Manufacturing of a 2205 Duplex Part with Coaxial Wire and Laser Beam Directed Energy Deposition10.1007/s11665-025-11152-2 ↗
10. Weldability, machinability and surfacing of commercial duplex stainless steel AISI2205 for marine applications—A recent review10.1016/j.jare.2017.01.002 ↗
11. Wire + Arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
12. Wire-feed additive manufacturing of metal components: Technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
13. Comparative analysis of residual stress distributions in a braking pedal from a historical motorbike manufactured via selective laser melting and wire arc additive manufacturing10.1007/s00170-025-15593-w ↗
14. An assessment of wire laser additive manufacturing with focus on characteristics research progress and quality improvement10.1007/s44245-025-00133-3 ↗
15. Cipriano, A., Malfatti, C.D.F., Casagrande, H.C., Daleffe, A., Castelan, J., and Possamai, P.H.M. (2025). Analysis of the Microstructure and Mechanical Properties of Austenitic Stainless Steel 310 Manufactured via WAAM. Materials, 18.10.3390/ma18163855 ↗
16. Study of the Additive Manufacturing Process by Localized Melting for E71T-1 and ER70S-6 Alloys
17. From Process Parameters to Industrial Qualification: A Comprehensive Review of WAAM Technology
18. Investigação do comportamento metalúrgico do aço inoxidável austenítico 310 no processo WAAM10.70185/2525-6025.2025.v10.501 ↗
19. Caracterização microestrutural e de microdureza para o arame tubular UTP AF Ledurit 60 impresso através da técnica de manufatura aditiva por arco elétrico10.70185/2525-6025.2024.v9.422 ↗
20. Effect of process parameters in laser cladding on substrate melted areas and the substrate melted shape10.2351/1.4906376 ↗
21. Advances in inside-laser material feeding additive manufacturing technology10.1007/s00170-025-16549-w ↗
22. Effect of Heat Treatment on Microstructure and Mechanical Properties of GHS785L Alloy Steel Fabricated by Laser and Wire Additive Manufacturing10.1007/s11665-025-11541-7 ↗
23. Increasing the productivity of coaxial laser cold-wire additive manufacturing using Inconel 71810.1007/s40964-025-01295-y ↗
24. Robust interface and excellent as-built mechanical properties of Ti–6Al–4V fabricated through laser-aided additive manufacturing with powder and wire10.1007/s12613-024-3003-8 ↗
25. Manufatura Aditiva na Construção de peças Metálicas para uso na Indústria Cerâmica10.70185/2525-6025.2023.v8.342 ↗
26. Wire and Laser Additive Manufacturing of Titanium/Steel Composites: Effect of Copper Interlayer on Microstructure and Mechanical Properties of Ti–Cu–Fe Interface Region10.1007/s12666-024-03552-0 ↗
27. Laser cladding of a cobalt-based superalloy on austenitic stainless steel10.1590/0104-9224/si26.02 ↗
28. Effects of Laser Quenching on Ti-Cu Alloy Prepared via Wire-Powder Synchronous Arc Additive Manufacturing10.1007/s11665-025-11505-x ↗
29. Tandon, D., Li, H., Pan, Z., Yu, D., and Pang, W. (2023). A Review on Hardfacing, Process Variables, Challenges, and Future Works. Metals, 13.10.3390/met13091512 ↗
30. Son, W.C., Jong, Y.G., Pak, M.C., and Ma, J.S. (2021). Microstructure and wear resistance of Fe-Cr-C-Mo-V-Ti-N hardfacing layers. arXiv.
31. Hybrid Manufacturing Process and Hot Forging: Preform Manufacturing Through Localized Melting Material Deposition Using UTP AF DUR 600 Wire
32. Uso da manufatura aditiva por fusão localizada na recuperação de estampo para indústria cerâmica10.70185/2525-6025.2024.v9.420 ↗
33. Influences of boron on the microstructural characteristics and wear performance of hypereutectic Fe-Cr-C-Mo-xB hardfacing alloy10.1016/j.surfcoat.2024.130415 ↗
34. Effects of flux-cored arc welding technology on microstructure and wear resistance of Fe-Cr-C hardfacing alloy10.1016/j.mtcomm.2023.105569 ↗
35. Fe-Cr-C-V hardfacing coatings with molybdenum addition: Wear, corrosion, and cavitation performances10.1016/j.surfcoat.2024.130715 ↗
36. Investigation of thermal influence on weld microstructure and mechanical properties in wire and arc additive manufacturing of steels10.1016/j.msea.2022.143690 ↗
37. Klocke, F., Arntz, K., Klingbeil, N., and Schulz, M. (2017). Wire-based laser metal deposition for additive manufacturing of TiAl6V4: Basic investigations of microstructure and mechanical properties from build up parts. Laser 3D Manufacturing IV, SPIE.10.1117/12.2251336 ↗
38. Process parameter optimization for laser directed energy deposition (LDED) of Ti6Al4V using single-track experiments with small laser spot size10.1016/j.optlastec.2024.110861 ↗
39. Siahsarani, A., Barmouz, M., Davoodi, F., Azarhoushang, B., and Harta, V. (2026). Influence of Process Parameters on Geometry and Thermal Behavior in Wire Laser Cladding of Bronze on Stainless Steel Substrates. Machines, 14.10.3390/machines14050553 ↗
40. Weidemann, T.C., Aduabiah, M., Shaqour, B., Day, R., Bergs, T., and Plapper, P. (2024). Influence on the bead geometry in Laser Metal Deposition with wire. J. Manuf. Mater. Process., 8, Available online: https://wlt.de/sites/default/files/2023-09/Contribution_239.pdf.10.3390/jmmp8050204 ↗
41. Evaluating residual stresses in metal additive manufacturing: A comprehensive review of detection methods, impact, and mitigation strategies10.1007/s12289-024-01855-7 ↗
42. Bian, P., Jammal, A., Xu, K., Ye, F., Zhao, N., and Song, Y. (2025). A Review of the Evolution of Residual Stresses in Additive Manufacturing During Selective Laser Melting Technology. Materials, 18.10.3390/ma18081707 ↗
43. Huang, W., Garmestani, H., and Liang, S.Y. (2025). Microstructure Evolution and the Influence on Residual Stress in Metal Additive Manufacturing with Analytics. Crystals, 15.10.20944/preprints202503.1866.v1 ↗
44. Effect of path strategy on residual stress and distortion in laser and cold metal transfer hybrid additive manufacturing
45. A new method to estimate the residual stresses in additive manufacturing characterized by point heat source10.1007/s00170-019-04443-1 ↗
46. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
47. Metal additive manufacturing: Technology, metallurgy and modelling10.1016/j.jmapro.2020.07.025 ↗
48. Elevated temperature tensile and fracture behavior of Ti-6Al-4 V alloy fabricated by wire-based laser additive manufacturing: Microstructural evolution and deformation mechanism10.1016/j.matchar.2026.116124 ↗
49. Microstructure and mechanical properties of wire-fed laser additive manufacturing Inconel 718 single-bead wall10.1016/j.msea.2026.150330 ↗
50. Shim, Y.R., Kim, J.K., Jo, D.H., Yang, H.P., Yoon, S.W., Yu, U.Y., Lee, H., Eo, D., Yoon, J.C., and Shin, S. (2025). Microstructure and Mechanical Properties of Wire Laser Additive Manufactured Deposits and Their Tungsten Inert Gas Welds. Materials, 18.10.3390/ma18061308 ↗
51. Bassis, M., Ron, T., Shirizly, A., and Aghion, E. (2023). Effect of Microstructure Modifications on Stress Corrosion Endurance of 15-5 PH Stainless Steel Formed by Wire Laser Additive Manufacturing (WLAM). Metals, 13.10.3390/met13101748 ↗
52. Ghanadi, N., and Pasebani, S. (2024). A Review on Wire-Laser Directed Energy Deposition: Parameter Control, Process Stability, and Future Research Paths. J. Manuf. Mater. Process., 8.10.3390/jmmp8020084 ↗
53. Effect of laser-induced texture on lubrication retention and tribological properties of 40Cr alloy surfaces10.1016/j.triboint.2023.108651 ↗
54. Insight into the tribological behavior of the dual-phase nickel aluminum bronze alloy by multiscale characterization10.1016/j.wear.2024.205530 ↗
55. Microstructure of Fe-Based Alloy Hardfacing Coating Reinforced by TiC-VC Particles10.1016/S1006-706X(06)60078-2 ↗
56. Liu, L., Lin, Y., Peng, L., Kang, X., and Wang, X. (2024). Progress in Microstructure Design and Control of High-Hardness Fe-Based Alloy Coatings via Laser Cladding. Coatings, 14.10.3390/coatings14111351 ↗
57. Hardfacing of metals: A review of consumables, properties and strengthening processes10.1016/j.jmrt.2025.04.221 ↗
58. A process-driven experimental analysis of different wire-fed Directed Energy Deposition processes employing the Laser, Electric Arc and Plasma sources10.1007/s00170-025-15581-0 ↗
59. Defect sensitivity and fatigue design: Deterministic and probabilistic aspects in additively manufactured metallic materials10.1016/j.pmatsci.2024.101290 ↗
60. (1983). Filler Metals Used in Surfacing—Designation, Technical Conditions of Delivery (Standard No. DIN 8555-1).
61. VOESTALPINE BÖHLER WELDING (2026, July 07). VTP: Manutenção e Cladding. [S. l.: S. n., n. d.]. Technical catalogue. VOESTALPINE BÖHLER WELDING. UTP Maintenance 2014: Filler Metals for Repair, Hardfacing and Cladding Applications, Available online: https://sbrrevestimentos.com.br/assets/pdfs/utp-maintenance2014.pdf.
62. Ribeiro, R. (2004). Avaliação da Resistência ao Desgaste Abrasivo de Revestimentos Soldados do Tipo Fe-C-Cr Utilizados na Indústria Sucroalcooleira. [Master’s Thesis, UNESP]. Available online: https://repositorio.unesp.br/server/api/core/bitstreams/443c5946-a8ff-4eea-a5fd-b7f75c018d90/content.
63. High deposition rate powder- and wire-based laser directed energy deposition of metallic materials: A review10.1016/j.ijmachtools.2022.103942 ↗
64. Zhong, C., Liu, J., Zhao, T., Schopphoven, T., Fu, J., Gasser, A., and Schleifenbaum, J.H. (2020). Laser metal deposition of Ti6Al4V-A brief review. Appl. Sci., 10.10.3390/app10030764 ↗
65. (2016). Standard Test Method for Measuring Abrasion Using the Dry Sand/Rubber Wheel Apparatus (Standard No. ASTM G65-16).
66. (2021). Standard Test Method for Analysis of Carbon and Low-Alloy Steel by Spark Atomic Emission Spectrometry (Standard No. ASTM E415-21).
67. (2025). Standard Test Methods and Practices for Chemical Analysis of Steel Products (Standard No. ASTM A751-25).
68. Standard Test Method for Analysis of Austenitic Stainless Steel by Spark Atomic Emission Spectrometry (Standard No. ASTM E1086).
69. (2025). Standard Test Method for Analysis of Aluminum and Aluminum Alloys by Spark Atomic Emission Spectrometry (Standard No. ASTM E1251-25).
70. (2021). Standard Test Method for Analysis of Titanium and Titanium Alloys by Spark Atomic Emission Spectrometry and Glow Discharge Atomic Emission Spectrometry (Performance-Based Method) (Standard No. ASTM E2994-21).
71. (2022). Standard Test Method for Microindentation Hardness of Materials (Standard No. ASTM E384-22).
72. (2023). Standard Test Methods for Vickers Hardness and Knoop Hardness of Metallic Materials (Standard No. ASTM E92-23).
73. (2015). Sand for Standard Mortar—Specification (Standard No. ABNT NBR 7214:2015).
74. Avaliação da resistência ao desgaste abrasivo e análise microestrutural do ELETRODO UTP 7200D através do processo de soldagem SMAW10.70185/2525-6025.2024.v9.369 ↗
75. Estudo dos efeitos da aplicação de revestimentos duros em aço baixo carbono através do processo de soldagem SMAW10.4322/2176-1523.20222397 ↗
76. Wear performance of Fe-Cr-C-B hardfacing coatings: Dry sand/rubber wheel test and ball-on-disc test10.1016/j.ijrmhm.2018.07.006 ↗
77. The effect of microstructure on abrasive wear of a Fe–Cr–C–Nb hardfacing alloy deposited by the open arc welding process10.1016/j.surfcoat.2015.06.026 ↗
78. Falat, L., Džupon, M., Ťavodová, M., Hnilica, R., Ľuptáčiková, V., Čiripová, L., Homolová, V., and Ďurišinová, K. (2019). Microstructure and Abrasive Wear Resistance of Various Alloy Hardfacings for Application on Heavy-Duty Chipper Tools in Forestry Shredding and Mulching Operations. Materials, 12.10.3390/ma12132212 ↗
79. Synergistic enhancement of strength and wear resistance in nickel-based superalloy fabricated by oscillating laser directed energy deposition via laser shock peening10.1016/j.jmrt.2026.02.104 ↗
80. Kim, Y.S., Chae, H., Huang, E.-W., Jain, J., Harjo, S., Kawasaki, T., Hong, S.I., and Lee, S.Y. (2022). Microstructural Evolution and Mechanical Properties of Non-Equiatomic (CoNi)74.66Cr17Fe8C0.34 High-Entropy Alloy. Materials, 15.10.3390/ma15041312 ↗
81. Chen, C., Wang, J., Ge, Y., Zhuang, M., and Ma, Z. (2023). Microstructure and Wear Resistance of High-Chromium Cast Iron with Multicomponent Carbide Coating via Laser Cladding. Coatings, 13.10.3390/coatings13081474 ↗
82. How the micro-mechanical stability of carbides in chromium-rich hardfacings influences the impact-abrasion resistance at elevated temperatures10.1016/j.wear.2023.204693 ↗
83. Arsić, D., Lazić, V., Nikolić, R.R., Sczygiol, N., Krstić, B., Ivković, D., Hadzima, B., Pastorek, F., and Ulewicz, R. (2022). Weldability Assessment of Various Steels by Hard-Facing. Materials, 15.10.3390/ma15093082 ↗
84. Microstructural evolution and mechanical performance correlation of WC-reinforced iron-based coatings fabricated by laser cladding10.1038/s41598-026-50674-0 ↗
85. Grain refinement and strengthening of additively manufactured Nb by doping TiC nanoparticle prepared via laser directed energy deposition
86. LAM additive manufacturing: A fundamental review on mechanical properties, common defects, dominant processing variables, and its applications10.1007/s00170-023-12139-w ↗
87. Bi, Z., and Li, T. (2024). Microstructure and Wear Resistance of FeCrV15 Coatings by Laser Cladding. Metals, 14.10.3390/met14101136 ↗
88. Microstructure evolution, wear and corrosion behaviour of (Nb, V)C-reinforced Fe-based composite coatings by laser cladding10.1177/1478422X241261786 ↗
89. Li, M., Huang, K., and Yi, X. (2023). Crack Formation Mechanisms and Control Methods of Laser Cladding Coatings: A Review. Coatings, 13.10.3390/coatings13061117 ↗
90. Wu, S.-H., Tariq, U., Joy, R., Sparks, T., Flood, A., and Liou, F. (2024). Experimental, Computational, and Machine Learning Methods for Prediction of Residual Stresses in Laser Additive Manufacturing: A Critical Review. Materials, 17.10.3390/ma17071498 ↗
91. Ferreira, C.C.D.A., Siqueira, R.H.M., Nuñez, J.G., Mariani, F.E., Coelho, R.T., Chen, D., and Lima, M.S.F. (2025). Microstructural Characterization of Martensitic Stainless Steel Blades Manufactured by Directed Energy Deposition (DED). Metals, 15.10.3390/met15060612 ↗
92. Martensitic to stainless steel gradient by laser-based directed energy deposition: Effect of thermal history on microstructure and hardness10.1016/j.jmapro.2025.06.030 ↗
93. Cho, W.I., and Park, C. (2026). A Review of Directed Energy Deposition for Wear-Resistant Metal–Ceramic Coatings in High-Temperature Industrial Applications. Metals, 16.10.3390/met16040403 ↗
94. Comparative Study of the Abrasive Wear Resistance of Hardfacing FeCrC, FeCrC + Nb, FeTiCW, and FeMn Coating10.1115/1.4070135 ↗
95. Microstructural modification and wear behavior improvement in Fe-C-Cr hardfacing alloys through molybdenum addition10.2320/matertrans.MT-M2025101 ↗
96. Chen, F., Xia, X., Wang, W., Gong, X., Yuan, X., Tang, C., Lou, X., Guo, Z., Wang, L., and Wu, B. (2025). Effect of Mo2C Addition on Microstructure and Wear Behavior of HVOF Carbide-Metal Composite Coatings. Materials, 18.10.3390/ma18245622 ↗
97. Performance regulation of laser-cladded high-manganese steel coatings by laser remelting process10.1080/10426914.2026.2674580 ↗
98. Development of heating strategies to reduce crack formation in the manufacturing process of tool components using directed energy deposition10.1007/s40964-025-00971-3 ↗
99. Effect of substrate preheating and in situ cooling on dimensional accuracy, microstructure, and hardness of wire-arc directed energy deposition components10.1007/s40194-025-02104-4 ↗
100. Casagrande, H.C., Daleffe, A., Ferreira, C.A., Fritzen, D., March, G., Castelan, J., and Schaeffer, L. (2024). Fabricação de peças metálicas por manufatura aditiva em aços com baixo teor de carbono. Engenharias em Perspectiva: Ciência, Tecnologia e Inovação 2, Atena Editora.10.22533/at.ed.2642418075 ↗