Long‐term polarisation and immersion for copper corrosion in high‐level nuclear waste environment
Source abstract
Abstract
Long‐term polarisation and immersion for copper corrosion were investigated in chloride‐containing sulphide solutions. Results showed that no active state exists for copper in sulphide‐containing solutions, whereas a typical active‐to‐passive transition exists in the second passivation region, indicating a hydroxyl activation effect on copper. After the sulphide passive film broke down, the pitting area was re‐passivated by hydroxide ions; however, if the chloride and sulphide concentrations were both high, then there was no second passivation and the copper would dissolve rapidly. The corrosion resistance and the film thickness both increased with increasing immersion time and an average corrosion rate of 51.2 µm/year was obtained in aerobic solution, which was much higher than in bentonite or under deoxygenated conditions. Moreover, several local corrosion pits appeared after 1‐year immersion and this would occur at the beginning of storage.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Corrosion and Protection Center Key Laboratory for Corrosion and Protection (MOE) University of Science and Technology Beijing Beijing 111083 P. R. China
Funding
National Natural Science Foundation of China
References (20)
Show source-provided references
1. 10.1016/j.jnucmat.2008.06.00110.1016/j.jnucmat.2008.06.001 ↗
2. 10.1016/S0013-7944(01)00041-810.1016/S0013-7944(01)00041-8 ↗
3. 10.1016/0022-3115(92)90367-T10.1016/0022-3115(92)90367-T ↗
4. SKB Swedish Nuclear Fuel & Waste Management Co. Long‐term safety for KBS‐3 repositories at Forsmark and Laxemar—a first evaluation Main Report of the SR‐Can Project SKB Technical Report TR‐06‐092006.
5. 10.1016/j.electacta.2010.12.03410.1016/j.electacta.2010.12.034 ↗
6. 10.1016/j.electacta.2016.05.13510.1016/j.electacta.2016.05.135 ↗
7. Eriksen T. E. · Corros. Sci · 1989 · 29
8. 10.1016/j.corsci.2015.01.00210.1016/j.corsci.2015.01.002 ↗
9. 10.1007/s10040-008-0416-910.1007/s10040-008-0416-9 ↗
10. Pedersen K. · Cheminform · 2001 · 32 · 110.1002/chin.200129001 ↗
11. 10.1016/j.electacta.2016.01.09810.1016/j.electacta.2016.01.098 ↗
12. 10.1149/1.274564710.1149/1.2745647 ↗
13. 10.1149/1.347857010.1149/1.3478570 ↗
14. 10.1016/j.electacta.2011.04.08610.1016/j.electacta.2011.04.086 ↗
15. 10.1016/j.corsci.2016.10.02410.1016/j.corsci.2016.10.024 ↗
16. 10.1016/j.electacta.2014.07.16010.1016/j.electacta.2014.07.160 ↗
17. 10.1149/2.0401613jes10.1149/2.0401613jes ↗
18. 10.1149/1.349642710.1149/1.3496427 ↗
19. 10.1007/s11665-017-2578-x10.1007/s11665-017-2578-x ↗
20. 10.1016/j.corsci.2016.12.01010.1016/j.corsci.2016.12.010 ↗