Hydrogen embrittlement of nodular cast iron

Patrik Sahiluoma, Yuriy Yagodzinskyy, Antti Forsström, Hannu Hänninen, Sven Bossuyt

Materials and Corrosion· Volume 72· Issue 1-2

Abstract

Abstract Ferritic nodular cast iron, intended for use as the material for inserts of canisters for long‐term geological disposal of spent nuclear fuel, was studied for hydrogen sensitivity. In the canisters, the insert provides the mechanical strength against external loads. Hydrogen was charged from 0.1 N H2SO4 solution in free‐corrosion tests and under controlled cathodic potential. Hydrogen uptake and trapping were then measured using thermal desorption spectroscopy. The hydrogen desorption rate after hydrogen charging manifests two distinct peaks. Plastic deformation during hydrogen charging increases the hydrogen uptake considerably. Hydrogen reduces the elongation to fracture and time to fracture in slow strain rate testing and constant load testing (CLT), respectively. Especially, the strain rate in CLT is dramatically increased. The appearance of hydrogen‐induced cracking in the ferrite phase changes from ductile dimple fracture to brittle cleavage fracture due to hydrogen charging, which initiates from the interphases of the graphite nodules. The results are discussed in terms of the role of hydrogen and the graphite nodules in hydrogen embrittlement of ductile cast iron.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering Aalto University School of Engineering Aalto Finland

Funding

KYT2022

References (15)

Show source-provided references
1. H.Raiko R.Sandström H.Ryden M.Johansson SKB Report TR‐10‐28 Stockholm Sweden2010.
2. SKB SKB Report TR‐16‐15 Stockholm Sweden2016.
3. M.Jonsson G.Emilsson L.Emilsson Posiva SKB Report 04 Eurajoki Finland2018.
4. 10.1515/corrrev-2019-000710.1515/corrrev-2019-0007 ↗
5. 10.1016/j.jnucmat.2018.06.01210.1016/j.jnucmat.2018.06.012 ↗
6. 10.1111/j.1460-2695.2009.01337.x10.1111/j.1460-2695.2009.01337.x ↗
7. 10.1007/BF0335558410.1007/BF03355584 ↗
8. 10.1016/j.engfracmech.2015.06.04210.1016/j.engfracmech.2015.06.042 ↗
9. 10.1007/s11661-002-0387-810.1007/s11661-002-0387-8 ↗
10. R.Wu J.Ahlström H.Magnusson K.Frisk Å.Martinsson SKB Report R‐13‐45 Stockholm Sweden2015.
11. 10.1007/s11661-013-2109-910.1007/s11661-013-2109-9 ↗
12. 10.1088/1742-6596/843/1/01201210.1088/1742-6596/843/1/012012 ↗
13. 10.1007/BF0264242410.1007/BF02642424 ↗
14. 10.1021/ac60131a04510.1021/ac60131a045 ↗
15. Zapffe C. · Trans. Am. Inst. Min., Metall. Eng. · 1941 · 145 · 225