journal article·2013-10

Impedance spectroscopy studies of electroless Ni–P matrix, Ni–W–P, Ni–P–ZrO2, and Ni–W–P–ZrO2 coatings exposed to 3.5% NaCl solution

A. Stankiewicz, J. Masalski, B. Szczygieł

Materials and Corrosion· Volume 64· Issue 10
Publisher page

Abstract

Abstract Ni–P matrix, ternary Ni–W–P and Ni–P–ZrO2 coatings, and quaternary Ni–W–P–ZrO2 coatings were deposited using electroless method from a glycine bath. Their corrosion resistance was evaluated by electrochemical impedance spectroscopy (EIS) for various immersion times in a 3.5% NaCl solution. From among the investigated coatings, the ternary Ni–W–P coatings show the highest resistance to corrosion in the first hour of exposure to the 3.5% NaCl medium. An addition of ZrO2 adversely affects the performance of both the Ni–P coatings and the Ni–W–P coatings. For all the coatings, including the ones containing tungsten, a marked decrease in pore resistance (Rpor) over time is observed. This means that their corrosion resistance and capacity to protect the substrate decline. On the other hand, after 24 h immersion in the 3.5% NaCl solution the Ni–W–P coating shows the highest low‐frequency impedance modulus (|Z|f = 0.01 Hz). As regards corrosion resistance, the Ni–P coatings and the Ni–W–P coatings perform best.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. 10.1016/j.surfcoat.2007.05.03010.1016/j.surfcoat.2007.05.030 ↗
2. 10.1002/maco.20060403310.1002/maco.200604033 ↗
3. 10.1007/s10008000015910.1007/s100080000159 ↗
4. 10.1016/j.matdes.2009.04.02010.1016/j.matdes.2009.04.020 ↗
5. 10.1016/S0169-4332(00)00114-810.1016/S0169-4332(00)00114-8 ↗
6. Mamenzadeh M. · Mater. Corros. · 2012 · 63 · 61410.1002/maco.201005985 ↗
7. 10.1002/maco.20080517010.1002/maco.200805170 ↗
8. 10.1016/j.surfcoat.2009.05.02510.1016/j.surfcoat.2009.05.025 ↗
9. 10.1016/j.msea.2006.10.03610.1016/j.msea.2006.10.036 ↗
10. 10.1016/j.surfcoat.2006.01.00510.1016/j.surfcoat.2006.01.005 ↗
11. 10.1016/j.surfcoat.2007.10.01510.1016/j.surfcoat.2007.10.015 ↗
12. 10.1016/j.electacta.2006.07.00110.1016/j.electacta.2006.07.001 ↗
13. 10.1179/002029605X6165810.1179/002029605X61658 ↗
14. 10.1016/j.electacta.2005.01.04010.1016/j.electacta.2005.01.040 ↗
15. 10.1016/j.electacta.2007.11.07110.1016/j.electacta.2007.11.071 ↗
16. 10.1016/j.apsusc.2003.12.03110.1016/j.apsusc.2003.12.031 ↗
17. 10.1016/j.apsusc.2004.12.04810.1016/j.apsusc.2004.12.048 ↗
18. 10.1016/j.surfcoat.2004.07.06810.1016/j.surfcoat.2004.07.068 ↗
19. 10.1016/S1044-5803(96)00089-710.1016/S1044-5803(96)00089-7 ↗
20. 10.1016/j.electacta.2004.01.03510.1016/j.electacta.2004.01.035 ↗
21. 10.1016/j.surfcoat.2007.09.02310.1016/j.surfcoat.2007.09.023 ↗
22. 10.1007/s10800-008-9673-510.1007/s10800-008-9673-5 ↗
23. 10.1007/s10800-009-0066-110.1007/s10800-009-0066-1 ↗
24. 10.1007/s10800-010-0203-x10.1007/s10800-010-0203-x ↗
25. 10.1016/j.electacta.2010.05.04610.1016/j.electacta.2010.05.046 ↗
26. 10.1016/j.corsci.2006.08.02510.1016/j.corsci.2006.08.025 ↗
27. 10.1007/s11802-007-0349-210.1007/s11802-007-0349-2 ↗
28. 10.1016/j.surfcoat.2011.12.01310.1016/j.surfcoat.2011.12.013 ↗
29. 10.1016/j.surfcoat.2012.01.04910.1016/j.surfcoat.2012.01.049 ↗
30. 10.1016/j.surfcoat.2007.08.01610.1016/j.surfcoat.2007.08.016 ↗
31. 10.1016/j.apsusc.2008.05.34210.1016/j.apsusc.2008.05.342 ↗
32. 10.1002/maco.20090557510.1002/maco.200905575 ↗
33. 10.1016/j.matdes.2010.02.02710.1016/j.matdes.2010.02.027 ↗
34. ZPlot for Windows Electrochemical Impedance Software. Scribner Associates Southern Pines 2001.
35. 10.1016/S0010-938X(97)00168-610.1016/S0010-938X(97)00168-6 ↗
36. 10.1088/0508-3443/18/6/30510.1088/0508-3443/18/6/305 ↗
37. Funke W. · 1993