Corrosion behavior of austenitic 304L and 316LN stainless steel clad reinforcing bars in cracked concrete
Source abstract
Abstract
Abstract A study has been conducted on the chloride‐induced corrosion behavior of 304L and 316LN stainless steel clad reinforcing bars (rebar) in concrete and in synthetic concrete pore solution. Metallographic examination of the as‐received clad bars confirmed a strong metallurgical bond at the core/clad interface and some grain growth interdiffusion of species at the interface. Both bars showed a wide variation in coating thickness around the rebar circumference, from a minimum of 0.32 and 0.60 mm to a maximum of 1.4 and 2.8 mm in the 304L clad and 316LN clad, respectively. The electrochemical results and visual examination after autopsy showed that active corrosion was yet initiated on either the solid and clad stainless steel or carbon steel rebar in the sound noncracked concrete specimens. In contrast, corrosion had initiated in the bars embedded in cracked concrete at the base of the crack and extended along or around the bars. In the concrete and synthetic pore solution tests, the current densities of both solid and clad stainless steel rebar exposed to ∼21% chloride brine solution for days between 400 and 1,500 were similar. This was also the case for current densities of the straight and bent stainless steel bars tested in the synthetic pore solution test.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Concrete Corrosion and Durability · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical and Mechatronics Engineering University of Waterloo Waterloo Ontario Canada
References (20)
Show source-provided references
1. 10.5006/237010.5006/2370 ↗
2. 10.1007/s10853-015-9387-010.1007/s10853-015-9387-0 ↗
3. D.Darwin J.Browning T.Van Nguyen J. C.Locke FHWA‐South Dakota DOT SD2002‐16‐X 2007.
4. Yunovich M. · Concr. Int. · 2003 · 25 · 52
5. Nuovinox Stelax Industries.http://www.stelaxindustries.com(accessed: August 2019).
6. J. R.Scully M. F.Hurley Investigation of the Corrosion Propagation Characteristics of New Metallic Reinforcing Bars (VTRC 07‐CR9) Virginia Department of Transportation Richmond VA2007.
7. G. H.Koch M. P.Brongers N. G.Thompson Y. P.Virmani J. H.Payer Corrosion Cost and Preventive Strategies in the United States (FHWA‐RD‐01‐156)2002.
8. G.Markeset S.Rostam O.Klinghoffer Nor. Build. Res. Inst. (Nordic Innov. Cent. Proj.—04118) Vol. no. 4052006.
9. F.Cui A.Sagüés Prog. Report Proj. “Corrosion Perform. Stainl. Steel Clad Rebar in Marine Substructure Service.”USF Acc. #21 04 301 LO ID #99P00612 2003.
10. Van Niejenhuis C. B. · ACI Mater. J. · 2018
11. 10.1016/j.cemconres.2010.04.00610.1016/j.cemconres.2010.04.006 ↗
12. ASTM G61‐86 “Standard test method for conducting cyclic polarization measurement for localized corrosion susceptibility of iron‐ nickel‐ or cobalt‐based alloys ” West Conshohocken PA 2009.
13. 10.1016/0010-938X(88)90101-110.1016/0010-938X(88)90101-1 ↗
14. 10.5006/336010.5006/3360 ↗
15. 10.21809/rilemtechlett.2018.7010.21809/rilemtechlett.2018.70 ↗
16. 10.5006/1.327989910.5006/1.3279899 ↗
17. Canadian Standards Association (CSA) “Canadian Highway Bridge Design Code ” Can. Stand. Assoc. CAN/CSA‐S6 2006.
18. OPSS.PROV 920 “Construction Specification for Deck Joint Assemblies Preformed Seals Joint Fillers Joint Seals Joint Sealing Compounds and Waterstops—Structures ” Ontatio Prov. Stand. Specif. 2008.
19. McDonald D. B. · Concr. Int · 1995 · 17 · 65
20. Y. P.Virmani D. B.McDonald D. W.Pfeifer M. R.Sherman FHWA‐RD‐98‐153 1998.