journal article·2021-08

Localized corrosion of (lean) duplex stainless steels in immersion units of urban wastewater treatment plants

Nicolas Larché, Benoit Emo, Audrey Allion, Elisabeth Johansson, Dominique Thierry

Materials and Corrosion· Volume 72· Issue 8
Publisher page

Abstract

Abstract With lower alloying cost and higher mechanical properties, lean duplex stainless steels can be an alternative to the more commonly used austenitic stainless steels. However, these alloys are still not the preferred choice, probably due to a lack of field experience. A study was thus initiated in view of defining the limits of use of selected (lean) duplexes for urban wastewater treatment units. The present paper shows the localized corrosion performance of selected lean duplexes in chloride contaminated solutions. The results are compared with austenitic S30403 and S31603 and with the more standard duplexes S82441 and S32205. The effect of welding was also investigated. Exposures in field municipal wastewater plants were conducted for 1 year in low and high chloride content units. The results show that lean duplexes S32101 and S32202 can be used as alternatives to S30403 and S31603 in low chloride electrolytes. At 500 ppm of chloride content, duplex stainless steel S32304 showed better corrosion resistance than S30403 and S31603. For higher chloride contents (1000 ppm and above) the standard duplexes S82441 and S32205 shall be preferred.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Offshore & Onshore Infrastructure Department French Corrosion Institute Brest France

Business Support & Performance Department Véolia Water Aubervilliers France

Solutions Department Aperam Global Research Isbergues France

Avesta Research Centre Outokumpu Stainless AB Avesta Sweden

Funding

Research Fund for Coal and Steel

References (39)

Show source-provided references
1. Rovel J.‐M. · 2007
2. Stainless Steel in Sewage Treatment Plants: A Clean Solution for Pure Water International Stainless Steel Forum Brussel Belgium 2010.
3. Tuthill A. H. · 1998
4. 10.1016/S0026-0576(10)80033-910.1016/S0026-0576(10)80033-9 ↗
5. Combrade P. · 2002 · 358
6. Outokumpu Corrosion Handbook 11th ed. Outokumpu Oyj Espoo Finland2015.
7. 10.1016/B978-008044495-6/50024-010.1016/B978-008044495-6/50024-0 ↗
8. 10.1016/0921-3449(95)00052-610.1016/0921-3449(95)00052-6 ↗
9. Iversen A. · Corros. Degrad. Eng. Mater. · 2010 · 3 · 1870
10. Assessment of ServiceConditions in Municipal Waste Water Plants a survey from Veolia Waste Water Plants Deliv. D05 DuplexWASTE Proj. Research Fund Coal Steel Grant Agreement Number 749632 2018.
11. Heubner U. · 2010
12. Corrosion of Stainless Steels in Supply (Drinking) and Waste (Sewage) Water Systems Br. Stainless Steel Assoc. Stainless Steel Advis. Serv.2001.
13. Kahar S. D. · Int. J. Eng. Res. Appl. · 2017 · 7 · 27
14. Charles J. · 2010 · 29
15. 10.1016/j.proeng.2014.03.03610.1016/j.proeng.2014.03.036 ↗
16. ASTM G48‐03 American Society for Testing and Materials2003.
17. E.‐M.Westin Doctorate Thesis Royal Institute of Technology (Stockholm Sweden)2010.
18. L.Peguet A.Gaugain Revue de Métallurgie2011 108 231.10.1051/metal/2011062 ↗
19. 10.1007/BF0332131610.1007/BF03321316 ↗
20. P.Boillot D.Rückle V.Baudu J.Peultier Lean duplex UNS S32202: a new stainless steel for drinking water applications CeoCor Conf. Vienna Austria May 2009.
21. 10.1002/maco.1982033060310.1002/maco.19820330603 ↗
22. Nilsson J.‐O. · Duplex Stainl. Steel Conf. Beaune, France · 2010
23. 10.1016/0011-9164(85)80075-810.1016/0011-9164(85)80075-8 ↗
24. ISO 18070:2015 Corrosion of metals and alloys—Crevice corrosion formers with disc springs for flat specimens or tubes of stainless steels in corrosive solutions 2015.
25. B.Espelid Development of a new crevice corrosion qualification test for stainless steels. KCI Publishing Maastricht2003 pp. 457 462.
26. Torres C. · Corros. Sci. · 2020 · 178
27. 10.1007/s10853-015-9501-310.1007/s10853-015-9501-3 ↗
28. 10.1016/j.electacta.2009.04.02310.1016/j.electacta.2009.04.023 ↗
29. 10.1016/j.corsci.2013.06.03910.1016/j.corsci.2013.06.039 ↗
30. 10.5006/1.331911510.5006/1.3319115 ↗
31. 10.1051/metal/201108010.1051/metal/2011080 ↗
32. N.Larché D.Thierry P.Boillot T.Cassagne J.Blanc P.Dézerville E.Johansson J. M.Lardon presented at Corrosion 2016 (paper 7196) NACE Houston TX March 2016.
33. 10.1016/j.corsci.2004.11.01710.1016/j.corsci.2004.11.017 ↗
34. 10.1108/0003559041053315610.1108/00035590410533156 ↗
35. Örnek C. · Science · 2015 · 99 · 164
36. 10.1149/1.291260110.1149/1.2912601 ↗
37. R.Francis presented at Corrosion 2007 (paper 07262) NACE Houston TX March 2007.
38. Powell C. · 2005
39. MTI manual No. 3—appendix B “Method MTI‐2 for laboratory testing of wrought iron and nickel‐base alloys for relative resistance to crevice corrosion in a standard ferric chloride solution” Materials Technology Institute of the Chemical Process Industries.