Influence of the machined surface roughness on the pitting behavior of 304 stainless steel
Source abstract
Abstract
Abstract The relationship between specimens with different machined surface roughness and pitting resistance was explored using the critical pitting temperature (CPT), critical pitting potential (Ep), and FeCl3 pitting immersion tests. Compared with the arithmetic mean deviation of the surface contour (Ra), the depth–width ratio could characterize the mathematical relationship between the machined surface roughness and pitting parameters more simply. With an increase in the depth–width ratio, the CPT and Ep of 304 stainless steel decreased, the average corrosion rate increased, the number of pits decreased, and the pit sizes increased. A larger depth–width ratio led to a larger effective diffusion length of metal cations in the pits, thus, the critical pitting criteria could be reached easily, which resulted in the reduction of the pitting resistance of 304 stainless steel.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science, State Key Laboratory of Molecular Engineering of Polymers Fudan University Shanghai China
Xichang Satellite Launch Center Xichang China
School of Materials Science and Engineering, State Key Lab of Marine Resource Utilization in South China Sea Hainan University Haikou China
Funding
National Natural Science Foundation of China · Natural Science Foundation of Shanghai
References (34)
Show source-provided references
1. 10.1016/j.mser.2009.03.00110.1016/j.mser.2009.03.001 ↗
2. 10.1016/j.corsci.2021.10933810.1016/j.corsci.2021.109338 ↗
3. 10.3724/SP.J.1037.2012.0061610.3724/SP.J.1037.2012.00616 ↗
4. Yang H. · Acta Metall. Sin. · 2015 · 51 · 333
5. 10.1016/j.corsci.2021.10931110.1016/j.corsci.2021.109311 ↗
6. 10.1088/2053-1591/ac09bc10.1088/2053-1591/ac09bc ↗
7. 10.1002/maco.20181062210.1002/maco.201810622 ↗
8. 10.1149/1945-7111/ab798310.1149/1945-7111/ab7983 ↗
9. 10.1016/j.corsci.2022.11017610.1016/j.corsci.2022.110176 ↗
10. 10.1016/j.corsci.2022.11069210.1016/j.corsci.2022.110692 ↗
11. Lv C. · Acta Metall. Sin. · 2021 · 57
12. 10.1016/j.jpowsour.2014.06.12110.1016/j.jpowsour.2014.06.121 ↗
13. 10.5006/1.358493810.5006/1.3584938 ↗
14. 10.1016/S0010-938X(01)00107-X10.1016/S0010-938X(01)00107-X ↗
15. Han Y. · Tungsten · 2022
16. 10.1007/s42864-021-00099-110.1007/s42864-021-00099-1 ↗
17. 10.1016/j.corcom.2021.09.00210.1016/j.corcom.2021.09.002 ↗
18. 10.5006/1.328054510.5006/1.3280545 ↗
19. 10.1016/S0964-8305(03)00104-510.1016/S0964-8305(03)00104-5 ↗
20. 10.1016/0010-938X(94)90109-010.1016/0010-938X(94)90109-0 ↗
21. 10.5006/1.329360310.5006/1.3293603 ↗
22. 10.1016/S0010-938X(02)00215-910.1016/S0010-938X(02)00215-9 ↗
23. 10.1002/maco.20160889310.1002/maco.201608893 ↗
24. 10.1149/2.1381704jes10.1149/2.1381704jes ↗
25. 10.1149/2.0591809jes10.1149/2.0591809jes ↗
26. 10.1149/2.0251811jes10.1149/2.0251811jes ↗
27. 10.1149/2.0211906jes10.1149/2.0211906jes ↗
28. 10.1149/2.0431911jes10.1149/2.0431911jes ↗
29. 10.1016/j.corsci.2021.10927710.1016/j.corsci.2021.109277 ↗
30. G01 Committee Test Method for Electrochemical Critical Pitting Temperature Testing of Stainless Steels ASTM International West Conshohocken2018.
31. 10.3390/ma1205073810.3390/ma12050738 ↗
32. 10.20964/2019.07.5110.20964/2019.07.51 ↗
33. 10.3389/fchem.2020.0052910.3389/fchem.2020.00529 ↗
34. 10.1002/aic.69032060510.1002/aic.690320605 ↗