Experimental study of dynamic DC stray current corrosion of X70 steel
Source abstract
Abstract
Abstract In this paper, an experimental investigation on X70 steel was performed with respect to dynamic DC stray current interference in a soil‐simulated solution and in quartz sand. The results showed that the interference period had a huge impact on the corrosion rate. When the interference period was less than 100 s, corrosion rates in the two testing conditions were less than 12% of that induced by steady DC corrosion with an equivalent current. When the interference period was longer than 100 s, the corrosion rate in the soil‐simulated solution increased more significantly than that in quartz sand. Also, when the interference period was longer than 1 h, the corrosion rate in the soil‐simulated solution was approximately equal to the Faraday theory corrosion rate. However, the corrosion rate in quartz sand was still less than 81% of the Faraday theory corrosion rate, even though the interference period had been increased to 16 h. The difference of the corrosion rates in the two testing conditions was probably because of the different capacities of charge consumption by the capacitance effect of the electric double layer as well as the different charge consumption due to the extra reaction of species other than iron.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Transmission and Distribution Department, Research Institute Beijing Gas Group Co. Ltd. Beijing China
Corrosion and Protection Center, Institute for Advanced Materials and Technology University of Science and Technology Beijing Beijing China
References (39)
Show source-provided references
1. Gao P. · Int. Pet. Econ. · 2019 · 27 · 54
2. Liu Z. · Total Corros. Control · 2016 · 30 · 56
3. Chen Z. G. · Corros. Prot. · 2008 · 29 · 344
4. Xu H. · Gas Technology · 2016 · 3 · 12
5. 10.5006/096310.5006/0963 ↗
6. 10.1109/TVT.2014.230452210.1109/TVT.2014.2304522 ↗
7. 10.1016/j.corsci.2013.03.01410.1016/j.corsci.2013.03.014 ↗
8. 10.1016/j.corsci.2006.05.04810.1016/j.corsci.2006.05.048 ↗
9. 10.1109/TPWRD.2012.221162310.1109/TPWRD.2012.2211623 ↗
10. 10.1016/j.jngse.2015.10.02210.1016/j.jngse.2015.10.022 ↗
11. 10.1016/j.jngse.2015.06.04410.1016/j.jngse.2015.06.044 ↗
12. 10.1007/s00202-015-0333-610.1007/s00202-015-0333-6 ↗
13. 10.1016/S0010-938X(99)00034-710.1016/S0010-938X(99)00034-7 ↗
14. 10.1108/0003559091100031310.1108/00035590911000313 ↗
15. 10.1016/j.jngse.2013.09.00310.1016/j.jngse.2013.09.003 ↗
16. Chen Z. G. · World Sci‐Tech R&D · 2012 · 34 · 740
17. Liu J. · Corros. Prot. · 2016 · 37 · 68
18. Meng Q. S. · Corros. Prot. · 2016 · 37 · 355
19. Dai S. · Chin Water Wastewater · 2016 · 32 · 58
20. 10.1007/s11771-014-2024-210.1007/s11771-014-2024-2 ↗
21. Wang L. W. · Corros. Prot. · 2014 · 35 · 218
22. 10.1016/j.conbuildmat.2017.05.02410.1016/j.conbuildmat.2017.05.024 ↗
23. 10.1108/ACMM-08-2018-199210.1108/ACMM-08-2018-1992 ↗
24. Wang X. H. · Corros. Prot. · 2010 · 31 · 193
25. 10.5006/1.328065010.5006/1.3280650 ↗
26. 10.1179/1743278215Y.000000004410.1179/1743278215Y.0000000044 ↗
27. 10.1016/j.conbuildmat.2021.12264510.1016/j.conbuildmat.2021.122645 ↗
28. 10.18178/ijscer.6.2.93-10010.18178/ijscer.6.2.93-100 ↗
29. 10.1016/j.jmst.2017.11.00410.1016/j.jmst.2017.11.004 ↗
30. 10.1016/j.matdes.2015.12.11210.1016/j.matdes.2015.12.112 ↗
31. 10.1149/1.183780910.1149/1.1837809 ↗
32. 10.1016/j.elecom.2006.07.01510.1016/j.elecom.2006.07.015 ↗
33. 10.1149/1.158082310.1149/1.1580823 ↗
34. 10.1016/S0010-938X(02)00242-110.1016/S0010-938X(02)00242-1 ↗
35. 10.1007/BF0101246710.1007/BF01012467 ↗
36. 10.1016/0010-938X(94)P4303-X10.1016/0010-938X(94)P4303-X ↗
37. M.Yunovich N. G.Thompson presented at Proc. IPC2004 Calgary Canada ASME 2004 IPC2004‐0574.
38. 10.1002/maco.20120669010.1002/maco.201206690 ↗
39. 10.5006/1.331916010.5006/1.3319160 ↗