Estimating galvanic corrosion rate of copper/steel couple by using remote earth mixed potential
Source abstract
Abstract
Abstract Copper and steel are often electrically connected in industrial devices, which causes galvanic corrosion in environments. To ensure the safety of the devices, it is needed to assess the corrosion rate of galvanic couples. The galvanic current is often used to calculate the galvanic corrosion rate in theory, however, in the actual devices, the copper parts are generally coupled with the steel parts and it is difficult to separate them to measure the galvanic current between them, as well as to determine the galvanic corrosion rates for actual devices. In this paper, the galvanic couple mixed potential distribution and influencing factors including area ratios, polarization characteristics, and medium resistivity are studied by experiments and calculation. The mixed potential becomes stable with a certain distance from the surface of copper/steel couple and acts as remote earth mixed potential. Remote earth mixed potential is positively associated with galvanic corrosion rate. Based on the results of experiments and calculation, a method to estimate the galvanic corrosion rate of steel in copper/steel couple by using the remote earth mixed potential is proposed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Non-Destructive Testing Techniques · Concrete Corrosion and Durability · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Corrosion and Protection Center, Institute of Advanced Materials and Technology University of Science and Technology Beijing Beijing China
China National Petroleum and Natural Gas Pipeline Network Group Co. Ltd. West East Gas Pipeline Branch, Qinhuai District Nanjing City Jiangsu China
References (32)
Show source-provided references
1. 10.1108/ACMM-05-2014-138910.1108/ACMM-05-2014-1389 ↗
2. 10.1080/1478422X.2017.130697210.1080/1478422X.2017.1306972 ↗
3. 10.1016/j.nucengdes.2015.08.01110.1016/j.nucengdes.2015.08.011 ↗
4. 10.1016/j.jece.2014.09.00910.1016/j.jece.2014.09.009 ↗
5. 10.1007/s40195-020-01071-710.1007/s40195-020-01071-7 ↗
6. 10.1016/j.geothermics.2020.10202410.1016/j.geothermics.2020.102024 ↗
7. E. L.Kirkpatrick presented atCORROSION 2011 Houston Texas March 13–17 2011 p. 11184
8. Kirkpatrick E. L. · Mater Perform. · 2003 · 42 · 28
9. Li G. C. · Commission. Oper · 2019 · 38 · 1378
10. Ge A. T. · Nat. Gas Oil · 2010 · 28 · 15
11. Wang B. Q. · J Chin. Soc. Corros. Prot. · 2022 · 42 · 200
12. 10.1016/j.corsci.2021.10940010.1016/j.corsci.2021.109400 ↗
13. 10.1016/j.jhazmat.2020.12293610.1016/j.jhazmat.2020.122936 ↗
14. 10.1016/j.corsci.2017.07.00910.1016/j.corsci.2017.07.009 ↗
15. 10.1002/adem.20060020610.1002/adem.200600206 ↗
16. 10.1016/j.corsci.2020.10869710.1016/j.corsci.2020.108697 ↗
17. L.Dong W.Cui Y.Yang X.Wang F.Gu presented atCORROSION 2017 New Orleans Louisiana USA March 26–30 2017 p. 9254.
18. 10.1016/j.corsci.2021.10956210.1016/j.corsci.2021.109562 ↗
19. 10.1016/j.corsci.2005.08.01310.1016/j.corsci.2005.08.013 ↗
20. 10.5006/074510.5006/0745 ↗
21. 10.1016/j.conbuildmat.2020.11833710.1016/j.conbuildmat.2020.118337 ↗
22. Jiang Z. T. · Corros. Prot. · 2016 · 37 · 1003
23. 10.1016/j.electacta.2020.13694710.1016/j.electacta.2020.136947 ↗
24. 10.1016/j.jmst.2020.10.04410.1016/j.jmst.2020.10.044 ↗
25. 10.1016/j.electacta.2008.04.02910.1016/j.electacta.2008.04.029 ↗
26. 10.1016/j.petrol.2014.09.03610.1016/j.petrol.2014.09.036 ↗
27. 10.1016/j.jhazmat.2022.12916910.1016/j.jhazmat.2022.129169 ↗
28. 10.1149/2.0521911jes10.1149/2.0521911jes ↗
29. 10.1016/j.enganabound.2018.08.01210.1016/j.enganabound.2018.08.012 ↗
30. 10.1016/j.oceaneng.2017.11.02710.1016/j.oceaneng.2017.11.027 ↗
31. 10.1016/j.ijepes.2016.06.00310.1016/j.ijepes.2016.06.003 ↗
32. IEEE Std80‐2000 Guide for Safety in AC Substation Grounding 2000.