High‐Temperature Corrosion Behavior of Al 0.3 CoCrFeNi and AlCoCrFeNi High‐Entropy Alloys in Na 2 SO 4 ‐K 2 SO 4 Salt Films
Source abstract
Abstract
ABSTRACT The high‐temperature corrosion behavior of Al 0.3 CoCrFeNi and AlCoCrFeNi high‐entropy alloys is evaluated at 900°C for 100 h in a Na 2 SO 4 ‐25 wt.% K 2 SO 4 molten salt environment. Corrosion kinetics are determined through mass change measurements, and the corrosion products are characterized using X‐ray diffraction, scanning electron microscopy, and energy‐dispersive spectroscopy. Electrochemical impedance spectroscopy is employed to investigate corrosion mechanisms and the role of aluminum content. AlCoCrFeNi exhibits significantly lower mass loss, attributed to the formation of a dense, continuous Al 2 O 3 scale that inhibits internal oxidation and sulfidation. The presence of Warburg impedance in the EIS spectra indicates a diffusion‐controlled process, with Al 2 O 3 dissolution acting as the rate‐limiting step. In contrast, Al 0.3 CoCrFeNi undergoes severe degradation due to oxide layer disruption, driven by molten salt penetration and extensive scale spallation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering Xi'an University of Science and Technology Xi'an China
References (36)
Show source-provided references
1. Hot Corrosion Behavior of AlCoCrFeNiZr High Entropy Alloy (HEA) Coating System Exposed to Na2SO4‐V2O5 Salt
2. 10.1016/j.surfcoat.2025.13228510.1016/j.surfcoat.2025.132285 ↗
3. 10.1016/j.corsci.2015.08.01110.1016/j.corsci.2015.08.011 ↗
4. 10.1002/maco.20191137610.1002/maco.201911376 ↗
5. 10.1080/10408436.2016.124309010.1080/10408436.2016.1243090 ↗
6. 10.1016/j.ijoes.2023.10019210.1016/j.ijoes.2023.100192 ↗
7. 10.3390/ma1809199610.3390/ma18091996 ↗
8. 10.3390/ma1808174910.3390/ma18081749 ↗
9. 10.1002/maco.20231424010.1002/maco.202314240 ↗
10. 10.1002/maco.20221370510.1002/maco.202213705 ↗
11. 10.1007/s13204-021-02077-y10.1007/s13204-021-02077-y ↗
12. 10.1080/09506608.2016.118002010.1080/09506608.2016.1180020 ↗
13. 10.1016/j.matlet.2008.01.01110.1016/j.matlet.2008.01.011 ↗
14. 10.1016/j.actamat.2011.06.04110.1016/j.actamat.2011.06.041 ↗
15. Effect of AlCoCrFeNi High‐Entropy Alloy on Microstructure and Mechanical Properties of Al‐Si‐Cu Alloyand Mechanical Properties of Al‐Si‐Cu Alloy
16. 10.1016/j.matdes.2012.04.04910.1016/j.matdes.2012.04.049 ↗
17. 10.1016/j.matdes.2016.11.02710.1016/j.matdes.2016.11.027 ↗
18. 10.1016/j.jallcom.2015.09.04210.1016/j.jallcom.2015.09.042 ↗
19. 10.1149/2.0821613jes10.1149/2.0821613jes ↗
20. 10.1016/j.apsusc.2016.11.17610.1016/j.apsusc.2016.11.176 ↗
21. 10.1016/j.jnucmat.2017.08.01510.1016/j.jnucmat.2017.08.015 ↗
22. 10.3390/e1802006210.3390/e18020062 ↗
23. 10.1016/j.corsci.2017.02.01910.1016/j.corsci.2017.02.019 ↗
24. 10.1016/j.corsci.2008.04.01110.1016/j.corsci.2008.04.011 ↗
25. 10.1002/maco.20241435110.1002/maco.202414351 ↗
26. 10.1016/j.intermet.2017.09.01210.1016/j.intermet.2017.09.012 ↗
27. 10.1016/j.jmst.2018.02.00310.1016/j.jmst.2018.02.003 ↗
28. 10.1016/j.corsci.2010.07.01110.1016/j.corsci.2010.07.011 ↗
29. 10.1016/j.corsci.2011.10.02110.1016/j.corsci.2011.10.021 ↗
30. 10.1007/s00339-022-05897-z10.1007/s00339-022-05897-z ↗
31. 10.1016/j.scriptamat.2019.04.04110.1016/j.scriptamat.2019.04.041 ↗
32. Dissolution Behavior of Metal Oxides in Molten Na2SO4
33. 10.1007/s11661-020-06068-610.1007/s11661-020-06068-6 ↗
34. 10.1016/j.matchar.2024.11439710.1016/j.matchar.2024.114397 ↗
35. 10.1002/1521-4176(200008)51:8<564::AID-MACO564>3.0.CO;2-410.1002/1521-4176(200008)51:8<564::AID-MACO564>3.0.CO;2-4 ↗
36. 10.1351/pac19906201011310.1351/pac199062010113 ↗