journal article·1998-05

Protection of high alloy steels against metal dusting by oxide scales

H.J. Grabke, E.M. Müller-Lorenz

Materials and Corrosion· Volume 49· Issue 5
Publisher page

Abstract

The metal dusting resistance of various high alloy steels was tested by exposures of specimens in different surface states at temperatures in the range 500 – 650°C. In addition surface analytical studies (AES) were conducted on the initial stages of oxide formation and the oxide layer after long term exposure under metal dusting conditions. The factors leading to a protective, Cr-rich oxide layer were elucidated and are summarized here.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Material Properties and Applications · High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.