journal article·2006-09

The cavitation erosion and erosion‐corrosion behavior of carbon steel in simulating solutions of three rivers of China

H. Yu, Y. G. Zheng, Z. M. Yao

Materials and Corrosion· Volume 57· Issue 9
Publisher page

Abstract

Abstract The corrosion behaviour of the Q235 carbon steel in simulation solution of Yangtze, Yellow and Talimu river of China was investigated by mass loss, electrochemical measurements (polarization curves, linear polarization resistance and electrochemical impedance spectroscopy) and the damaged surfaces were observed by a scanning electron microscope (SEM) under static, cavitation erosion and erosion‐corrosion conditions. It was shown that under static condition, the Ecorr was almost the same in the three solutions but the anodic current density in Talimu river was about one order of magnitude larger than that in Yangtze and Yellow river. Under dynamic conditions including cavitation erosion and erosion‐corrosion, the Ecorr in the three solutions all shifted in positive direction from that under static condition, but the extent of ΔEcorr increased in the order of Yangtze, Yellow and Talimu river. The corrosion rate under dynamic conditions greatly enhanced, especially in Talimu river. It was confirmed that the corrosion played an important role in the synergistic effect under cavitation erosion and erosion‐corrosion conditions. The test results suggested that when the structure materials used in the different rivers were chosen, the difference of corrosiveness of the rivers must be taken into account, especially under dynamic conditions. The materials used in the aggressive rivers such as Talimu river under dynamic conditions must resist the synergistic effects between erosion and corrosion.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgy and Material Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. B. Zhou Disposal Techniques of Industrial Water Beijing: Chemical Industry Press. 1997 1.
2. 10.1016/S0043-1648(97)00072-010.1016/S0043-1648(97)00072-0 ↗
3. 10.5006/1.327759010.5006/1.3277590 ↗
4. 10.1016/S0921-5093(00)00899-610.1016/S0921-5093(00)00899-6 ↗
5. 10.1016/0301-679X(91)90035-810.1016/0301-679X(91)90035-8 ↗
6. 10.1179/09506608679032421210.1179/095066086790324212 ↗
7. 10.1016/0010-938X(90)90239-210.1016/0010-938X(90)90239-2 ↗
8. 10.5006/1.328481910.5006/1.3284819 ↗
9. 10.1016/S0043-1648(03)00566-010.1016/S0043-1648(03)00566-0 ↗
10. 10.1016/0010-938X(90)90001-L10.1016/0010-938X(90)90001-L ↗
11. 10.1016/S0167-577X(00)00255-X10.1016/S0167-577X(00)00255-X ↗
12. ASTM G32‐85 Standard Method of Vibratory Cavition Erosion Test West Conshohocken PA: ASTM International 1985 187.
13. 10.5006/1.327988410.5006/1.3279884 ↗
14. C. N. Cao Electrochemistry Bejing: Chemistry Industry Press 2004 213.
15. Wei. L Ph. Diss. Institude of Metal Research Chinese Academy of Science 2001.
16. 10.1149/1.208559010.1149/1.2085590 ↗
17. 10.1023/B:JACH.0000003855.95788.1210.1023/B:JACH.0000003855.95788.12 ↗
18. 10.5006/0010-9312-36.8.41610.5006/0010-9312-36.8.416 ↗
19. 10.1016/S0010-938X(01)00141-X10.1016/S0010-938X(01)00141-X ↗
20. K. Videm J. Kvarekval Corrosion/96 Paper No.1 NACE International Houston 1996.
21. 10.5006/1.329354810.5006/1.3293548 ↗
22. 10.5006/1.358488810.5006/1.3584888 ↗
23. 10.5006/1.331612710.5006/1.3316127 ↗
24. Z. Yue P. Zhou J Shi in: Proceeding of the Conference on Wear of Materials New York ASTM 1987 763.
25. 10.1016/0043-1648(95)07132-610.1016/0043-1648(95)07132-6 ↗