Microstructural influence on corrosion properties of aluminium composites reinforced with amorphous iron borides
Source abstract
Abstract
Aluminium composite materials reinforced with amorphous iron borides (Fe/B) have been manufactured following a powder metallurgical (PM) route. Aluminium particles were mixed with 20% (by wt.) Fe/B particles (obtained by mechanical alloying during 36 h from iron and boron powders, 50% by wt. mixture). Mixes were uniaxially pressed and sintered at different temperatures (ranging from 650 to 1100 °C). The effect of sintering temperature on the corrosion resistance of those materials has been studied and related to the formed microstructures. Moreover, those materials were compared to a wrought and a PM plain aluminium. Their behaviour is studied through cyclic anodic polarization curves in chloride media. In the Al + 20%Fe/B composites, low sintering temperatures (650–950 °C) exert a negative effect. However, when the material was sintered at high temperature (1000–110 0°C) its behaviour was very similar to the pure sintered aluminium.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Science and Engineering Department Universidad Carlos III de Madrid Av. Universidad, 30. E‐28911 Leganés (Spain)
References (32)
Show source-provided references
1. 10.1520/JTE11899J10.1520/JTE11899J ↗
2. T. G.Haynes K.Anderson L. E.Oschmann US Patent5 965 829 1999.
3. 10.1016/j.jmatprotec.2006.11.12210.1016/j.jmatprotec.2006.11.122 ↗
4. 10.1016/j.msea.2007.11.15410.1016/j.msea.2007.11.154 ↗
5. 10.1023/A:101862540210310.1023/A:1018625402103 ↗
6. 10.1023/A:101360032859910.1023/A:1013600328599 ↗
7. 10.1016/j.msea.2011.02.02410.1016/j.msea.2011.02.024 ↗
8. 10.1016/j.jallcom.2010.04.20710.1016/j.jallcom.2010.04.207 ↗
9. 10.1016/j.compscitech.2008.04.00610.1016/j.compscitech.2008.04.006 ↗
10. 10.1016/S0924-0136(03)00298-X10.1016/S0924-0136(03)00298-X ↗
11. 10.1016/j.jallcom.2005.11.04210.1016/j.jallcom.2005.11.042 ↗
12. 10.1007/s10853-009-3335-910.1007/s10853-009-3335-9 ↗
13. 10.1016/j.jallcom.2011.04.14510.1016/j.jallcom.2011.04.145 ↗
14. 10.1016/j.jssc.2003.01.00110.1016/j.jssc.2003.01.001 ↗
15. Hihara L. H. · 2010 · 2250
16. 10.1002/maco.20080516410.1002/maco.200805164 ↗
17. 10.1179/00070598579827288510.1179/000705985798272885 ↗
18. 10.1149/1.187087310.1149/1.1870873 ↗
19. 10.1149/1.319052110.1149/1.3190521 ↗
20. 10.1016/j.corsci.2011.04.02310.1016/j.corsci.2011.04.023 ↗
21. 10.5006/1.331597210.5006/1.3315972 ↗
22. 10.1002/maco.20080510610.1002/maco.200805106 ↗
23. Abenojar J. · 2011
24. 10.3989/revmetalm.2006.v42.i2.1110.3989/revmetalm.2006.v42.i2.11 ↗
25. ASTM G‐61: Standard Test Method for Conducting Cyclic Potentiodynamic Polarization Measurements for Localized Corrosion susceptibility of Iron‐ Nickel‐ or Cobalt‐Based Alloys 2009.
26. 10.1179/bcj.1996.31.4.29510.1179/bcj.1996.31.4.295 ↗
27. 10.1016/j.matchar.2006.10.00810.1016/j.matchar.2006.10.008 ↗
28. 10.5006/1.358502010.5006/1.3585020 ↗
29. 10.1016/j.corsci.2009.10.04010.1016/j.corsci.2009.10.040 ↗
30. 10.1007/s11666-010-9574-010.1007/s11666-010-9574-0 ↗
31. 10.1016/j.jssc.2005.12.03710.1016/j.jssc.2005.12.037 ↗
32. 10.1016/S0921-5093(03)00469-610.1016/S0921-5093(03)00469-6 ↗