journal article·2015-03

High temperature corrosion investigation in an oxyfuel combustion test rig

M. Montgomery, M. Bjurman, A. Hjørnhede, H. B. Rombrecht, A. Lisk, H. J. Krautz

Materials and Corrosion· Volume 66· Issue 3
Publisher page

Abstract

Oxyfuel firing and subsequent capture of CO2is a way to reduce CO2emissions from coal‐fired boilers. Literature is summarized highlighting results which may contribute to understanding of the corrosion processes in an oxyfuel boiler. Tests were conducted in a 500 kWth oxyfuel test facility constructed by Brandenburg Technical University to gain understanding into oxyfuel firing. Two air‐cooled corrosion probes were exposed in this oxyfuel combustion chamber where the fuel was lignite. Gas composition was measured at the location of testing. Various alloys from aCr steel, austenitic steels to nickel alloys were exposed at set metal temperatures of 570 and 630 °C for 287 h. The specimens were investigated using light optical and scanning electron microscopy and X‐ray diffraction. The deposit on the probe contained predominantly CaSO4and Fe2O3. Oxide thickness and depth of the precipitated (perhaps carburized) zone was used as a measure of corrosion rates. The lowest alloyed steel had the highest corrosion rate, and the other austenitic and nickel alloys had much lower corrosion rates. Precipitates in the alloy adjacent the corrosion front were revealed for both Sanicro 28 and C‐276. However, it was observed that precipitates were present on both the concave and fireside convex tube surfaces, thus oxyfuel conditions cannot be responsible for these precipitations.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Thermochemical Biomass Conversion Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Vattenfall Thermal Engineering Denmark/DTU Mekanik Produktiontorvet, Building 425 2800 Lyngby (Denmark)

Formerly Vattenfall Research and Development AB Alvkarleby (Sweden), now Studsvik Nuclear AB

Formerly Vattenfall Power Consultant AB Goteborg (Sweden), now at Swedish Technical Research Institute Borås

Brandenburgische Technische Universität Cottbus‐Senftenberg Platz der Deutschen Einheit 1 03046 Cottbus (Germany)

References (37)

Show source-provided references
1. M.Montgomery A.Hjørnhede A.Gerhardt ProceedingsEurocorr 2009 Nice France 6–9 September2009 Paper 7979.
2. Rowlands P. C. · Gas Cooled Reactors Today, BNES London · 1983 · 4 · 173
3. P. C.Rowlands M. I.Manning ProceedingsNACE Corrosion 1983 NACE International Houston1983 pp300–309.
4. Rowlands P. C. · Nucl. Energy · 1986 · 25 · 267
5. Kofstad P. · 1988
6. 10.1179/bcj.1967.2.6.23510.1179/bcj.1967.2.6.235 ↗
7. Montgomery M. · VGB Kraftværkstechnik · 1995 · 75 · 258
8. I. G.Wright B. A.Pint Proc.NACE Corrosion 2002 NACE International Houston2002 Paper 02377.
9. S.Fry S.Osgerby M.Wright NPL Report MATC(A)90 September2002.
10. 10.1007/BF0167050710.1007/BF01670507 ↗
11. 10.1016/j.scriptamat.2007.06.05810.1016/j.scriptamat.2007.06.058 ↗
12. R. C.John Proc.NACE Corrosion 2007 NACE International Houston2007 Paper 07465.
13. I. G.Wright B. A.Pint Y.Zhang R. A.Bishop J. C.Farmer A.Jankowski R. B.Rebak ProcNACE Corrosion 2004 NACE International Houston2004 Paper 04531.
14. D.Huenert A.Kranzmann Proc.NACE Corrosion 2008 NACE International Houston2008 Paper 08447.
15. A.Kranzmann D.Huenert H.Rooch I.Urban W.Schulz W.Oesterle Proc.NACE Corrosion 2009 NACE International Houston2009 Paper 09265.
16. W.Schulz D.Huenert H.Nitschke R. S.Neumann A.Kranzmann Proc.NACE Corrosion 2009 NACE International Houston2009 Paper 09264.
17. D.Hünert W.Schulz A.Kranzmann ProceedingsEurocorr 2009 6–9 September2009 Nice France.
18. 10.3184/096034009X43818510.3184/096034009X438185 ↗
19. K.Natesan D. L.Rink Proc.21st Annual Conference on Fossil Energy Materials. Knoxville Tenessee USA 2007.
20. P.Pohjanne S.Yli‐Olli P.Auerkari S.Tuurna P.Jauhiainen E.Turunen T.Varis K.Ruusuvuori M.Makipaa ProceedingsNACE Corrosion 2010 NACE International Houston2010 Paper 10200.
21. 10.1515/HTMP.1989.8.3.14910.1515/HTMP.1989.8.3.149 ↗
22. Lai G. Y. · 1990 · 140
23. 10.1016/j.ijhydene.2006.08.02710.1016/j.ijhydene.2006.08.027 ↗
24. 10.1007/BF0066646910.1007/BF00666469 ↗
25. 10.1007/BF0060383510.1007/BF00603835 ↗
26. W. T.Bakker S. C.Kung Proc.NACE Corrosion 2000 NACE International Houston2000 Paper 00246.
27. 10.1080/09603409.1997.1168954210.1080/09603409.1997.11689542 ↗
28. 10.1023/A:100469802450610.1023/A:1004698024506 ↗
29. 10.1002/(SICI)1521-4176(199907)50:7<405::AID-MACO405>3.0.CO;2-810.1002/(SICI)1521-4176(199907)50:7<405::AID-MACO405>3.0.CO;2-8 ↗
30. 10.1016/j.fuel.2007.07.02310.1016/j.fuel.2007.07.023 ↗
31. Sroda S. · Mater. Corros. · 2006 · 57 · 77610.1002/maco.200503931 ↗
32. B. S.Covino S. A.Matthes S. J.Bullard Proc.NACE Corrosion 2008 NACE International Houston2008 Paper 08456.
33. A.Findeisen M.Klatt H. J.Krautz Chem. Erde – Geochem. Supplement 32010 70 193.10.1016/j.chemer.2010.05.006 ↗
34. Aha U. · VGB PowerTech. · 2010 · 6 · 53
35. 10.1021/ef040016110.1021/ef0400161 ↗
36. 10.4028/www.scientific.net/MSF.595-598.26110.4028/www.scientific.net/MSF.595-598.261 ↗
37. 10.1016/S0921-5093(99)00446-310.1016/S0921-5093(99)00446-3 ↗