Electromagnetic induction corrosion control technology (EICCT)
Source abstract
Abstract
Over the past several years, a new corrosion control technology has been developed for protecting damaged, painted galvanized, and galvannealed surfaces in contact with ambient aqueous environments. This technology, which we call electromagnetically induced corrosion control technology (EICCT), is an electronic technology that is based upon coupling surface currents into the metal structure to be protected. Electromagnetic induction experiments have demonstrated that the induced current is spread across the surfaces of complex shapes, such as an automobile body, as required by Maxwell's equations, so that induction at a single point is effective in protecting a whole, complex‐shaped surface, that the power consumption is very low, and possibly that the induced signal may be tailored to optimize the efficacy. The observed efficacy is attributed to inhibition of zinc passivation as directly indicated by the coupling current. Efficacy is also indicated by inhibition of rusting at scribes in painted panels. It is important to emphasize that the technique is not a classical, impressed current cathodic protection (ICCP) system.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Non-Destructive Testing Techniques · Concrete Corrosion and Durability · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Nuclear Engineering and Materials Science and Engineering University of California Berkeley California USA
Final Coat Research and Development 1136 West Maple Street Hartville Ohio USA
Canadian Auto Preservation Inc. 321 Cityview Blvd, Unit 1 Vaughan ON L4H 3S7 Canada
Funding
Canadian Auto Preservation, Inc.
References (18)
Show source-provided references
1. D. D.Macdonald M.Lewis J.McLafferty R.Peek presented at215th ECS Meeting San Francisco CA May 24–29 2009 pp.55–74.10.1149/1.3259799 ↗
2. Clement R. · 2001
3. Askea D. · 2004
4. R.Baboian presented atthe 5th Automotive Corrosion and Prevention Conference & Exposition SAE Technical Paper 912270 Dearborn USA October 21–23 1991 pp. 17–24.
5. 10.1002/maco.20120686810.1002/maco.201206868 ↗
6. Young J. · 2004
7. 10.1016/0010-938X(89)90051-610.1016/0010-938X(89)90051-6 ↗
8. 10.1149/1.350027410.1149/1.3500274 ↗
9. 10.5006/0010-9312-6.9.30810.5006/0010-9312-6.9.308 ↗
10. 10.1016/S0010-938X(74)80042-910.1016/S0010-938X(74)80042-9 ↗
11. Kurr G. · Mater. Perform · 1979 · 18 · 34
12. 10.1016/0010-938X(77)90027-010.1016/0010-938X(77)90027-0 ↗
13. 10.1016/0010-938X(85)90066-610.1016/0010-938X(85)90066-6 ↗
14. Szab S. · Corros. Rev · 2011 · 23 · 17110.1515/CORRREV.2005.23.2-3.171 ↗
15. 10.1016/0376-4583(85)90139-610.1016/0376-4583(85)90139-6 ↗
16. 10.5006/0010-9312-5.10.33010.5006/0010-9312-5.10.330 ↗
17. 10.1351/pac19997106095110.1351/pac199971060951 ↗
18. 10.1149/1.183877710.1149/1.1838777 ↗